Abstract:
A composition for forming film having wrinkle structure and a method of forming the film are disclosed. The composition includes photo-curable agent and photoinitiator dissolved in the photo-curable agent. The cut off wavelength of light transmittance of the photo-curable agent is greater than the cut off wavelength of light absorbance of the photoinitiator. Photo-cured thin film is formed at the upper portion of composition layer at an initial time period of irradiation. By subsequent contraction, the photo-cured thin film forms wrinkles. The wrinkle structure is controlled by the relation of the cut off wavelength of light transmittance of the photo-curable agent and the cut off wavelength of light absorbance of the photoinitiator, the photo-curing rate of the composition and the thickness of the composition layer, and the photoinitiator concentration, etc., before photo-curing. The film may increase the emission efficiency of LED and OLED and the sensing effect of sensor.
Abstract:
Provided is a method for manufacturing an electronic device including a transparent conductive structure, the method including preparing a transparent electrode in which, among a first region and a second region, the first region is selectively surface-modified, preparing a mixed composition including a first composition and a second composition having a different polarity from the first composition, and applying the mixed composition onto the transparent electrode, wherein the applied mixed composition is disposed in the surface modified first region, and the mixed composition disposed in the first region is phase-separated into a first composition layer and a second composition layer disposed on the first composition layer.
Abstract:
The inventive concept provides light emitting devices and methods of manufacturing a light emitting device. The light emitting device may include a transparent substrate including a first region and a second region, a first transparent electrode disposed on a first surface of the transparent substrate, a second transparent electrode facing and spaced apart from the first transparent electrode, an organic light emitting layer disposed between the first and second transparent electrodes, an assistant electrode disposed between the first and second transparent electrodes and selectively masking the second region, and a light path changing structure disposed on a second surface of the transparent substrate and selectively masking the second region.
Abstract:
Provided is a method of fabricating an organic scattering layer. The method may include providing a deposition apparatus with a reaction chamber and a source chamber, loading a substrate in the reaction chamber, supplying carrier gas into the source chamber that may be configured to supply an evaporated organic source material into the reaction chamber, a temperature of the carrier gas ranging from 25° C. to 50° C., and spraying the carrier gas and the evaporated organic source material into the reaction chamber through a showerhead to deposit an organic scattering layer on the substrate, the organic scattering layer including organic particles, which may be provided in a molecularized form of the evaporated organic source material, and thereby having an uneven surface.
Abstract:
Provided is a dual-mode display including a substrate, and a plurality of sub pixels on the substrate. Each of the sub pixels may include an emissive device, a reflective optical filter provided on a surface of the emissive device, and an optical shutter provided on other surface of the emissive device.
Abstract:
Provided is a light source apparatus which include a light emitting unit including a light emitting area of unit of surface, an antenna disposed along the outer periphery so as not to encroach on a light emitting area and a driving unit, and a driving unit processing wireless power received from the antenna and supplying the processed wireless power to the light emitting unit. According to the light source apparatus, miniaturization may be accomplished and a shielding phenomenon of an antenna reception signal caused by the light emitting area may be suppressed.
Abstract:
Disclosed are an organic light emitting diode device and a method of fabricating the organic light emitting diode device capable of achieving high light extraction efficiency even without a high-cost and complicated process. The organic light emitting diode device according to an exemplary embodiment of the present disclosure includes a substrate; a phase change thin film layer formed on the substrate and formed of a phase change material changeable from an amorphous state to a crystalline state or from a crystalline state to an amorphous state; and an anode electrode layer, an organic light emitting layer and a cathode electrode layer which are sequentially formed on the phase change thin film layer.