11.
公开(公告)号:US20170217774A1
公开(公告)日:2017-08-03
申请号:US15500990
申请日:2015-08-11
Applicant: Nippon Electric Glass Co., Ltd.
Inventor: Junichi IKEJIRI , Hideo YAMAUCHI , Fumio SATO
IPC: C01B25/45 , H01M4/58 , H01M4/62 , H01M10/054
CPC classification number: C01B25/45 , H01M4/58 , H01M4/5825 , H01M4/62 , H01M10/054
Abstract: Provided are a positive electrode active material for a sodium ion secondary battery excellent in quick charge-discharge characteristics by preventing fusion between particles of powder during firing, and a method of producing the same. A positive electrode active material for a sodium ion secondary battery of the present invention includes inorganic powder that contains at least one kind of transition metal element selected from the group consisting of Cr, Fe, Mn, Co, and Ni, Na, P, and O, and has a BET specific surface area of from 3 m2/g to 50 m2/g.
-
公开(公告)号:US20140045675A1
公开(公告)日:2014-02-13
申请号:US14055929
申请日:2013-10-17
Applicant: NIPPON ELECTRIC GLASS CO., LTD.
Inventor: Takahiro MATANO , Fumio SATO , Yoko USUI
Abstract: The invention provides an optical glass for press molding which can satisfy all of the following requirements: (1) it contains no environmentally undesirable components; (2) it can easily achieve a low glass transition point; (3) it has a high refractive index and high dispersion; (4) it can easily provide a glass having an excellent visible light transmittance; and (5) it has excellent resistance to devitrification during preparation of a preform. The optical glass for press molding has a refractive index nd of 1.925 or more, an Abbe's number νd of 10 to 30, and a glass composition, in % by mass, of 20 to 80% Bi2O3, 10 to 30% B2O3, and 0 to 5.5% GeO2 and is substantially free of lead component, arsenic component, and F component.
Abstract translation: 本发明提供了一种用于压制成型的光学玻璃,其可以满足以下所有要求:(1)其不含环境不理想的组分; (2)可以轻松实现玻璃化转变点低; (3)折射率高,色散高; (4)可以容易地提供具有优异的可见光透射率的玻璃; 和(5)在制备预成型件时具有优异的耐失透性。 压模成形用光学玻璃的折射率nd为1.925以上,阿贝数nud为10〜30,玻璃组合物的质量%为20〜80%的Bi2O3,10〜30%的B2O3,0 至5.5%的GeO 2,并且基本上不含铅成分,砷成分和F成分。
-
公开(公告)号:US20240288672A1
公开(公告)日:2024-08-29
申请号:US18571383
申请日:2022-07-08
Applicant: Nippon Electric Glass Co., Ltd.
Inventor: Yoshimasa MATSUSHITA , Fumio SATO , Nobuo HORI
Abstract: Provided is a telephoto lens which is excellent in resolution. An infrared imaging lens (1) includes a first lens (L1), a second lens (L2), and a third lens (L3) each of which is made of chalcogenide glass having a refractive index of 2.5 to 4.0 measured at a wavelength of 10 μm, the infrared imaging lens (1) having a total system focal length not less than two times larger than a diameter of an image circle of the infrared imaging lens (1).
-
公开(公告)号:US20210053866A1
公开(公告)日:2021-02-25
申请号:US16961738
申请日:2019-01-18
Applicant: NIPPON ELECTRIC GLASS CO., LTD.
Inventor: Yoshimasa MATSUSHITA , Fumio SATO
Abstract: Provided is a glass having an excellent infrared transmittance and suitable for use in infrared sensors. An infrared transmitting glass containing, in terms of % by mole, over 0 to 50% Ge, over 0 to 50% Ga, over 0 to 50% Si, 20 to 90% Te, 0 to 40% Ag+Al+Ti+Cu+In+Sn+Bi+Cr+Sb+Zn+Mn, and 0 to 40% F+Cl+Br+I.
-
公开(公告)号:US20190202725A1
公开(公告)日:2019-07-04
申请号:US16297771
申请日:2019-03-11
Applicant: NIPPON ELECTRIC GLASS CO., LTD.
Inventor: Tomoko YAMADA , Fumio SATO
CPC classification number: C03B5/235 , C03B19/063 , C03B19/1005 , C03B23/00 , C03B40/04
Abstract: Provided is a method that can manufacture a glass material having excellent homogeneity by containerless levitation. With a block (12) of glass raw material held levitated above a forming surface (10a) of a forming die (10) by jetting gas through a gas jet hole (10b) opening on the forming surface (10a), the block (12) of glass raw material is heated and melted by irradiation with laser beam, thus obtaining a molten glass, and the molten glass is then cooled to obtain a glass material. Control gas is jetted to the block (12) of glass raw material along a direction different from a direction of jetting of the levitation gas for use in levitating the block (12) of glass raw material or the molten glass.
-
公开(公告)号:US20180127301A1
公开(公告)日:2018-05-10
申请号:US15565471
申请日:2015-06-10
Applicant: NIPPON ELECTRIC GLASS CO., LTD. , The University of Tokyo
Inventor: Fumio SATO , Tomoko YAMADA , Hiroyuki INOUE , Atsunobu MASUNO
CPC classification number: C03B40/04 , C03B5/235 , C03B19/063 , C03B19/1005
Abstract: The development of cracks or breakage in a glass material during production of the glass material by a containerless levitation technique is reduced. A glass material is obtained by heating a levitated block 12 of glass raw material to melting by irradiation of the block 12 of glass raw material with laser light to thus obtain a molten glass and then cooling the molten glass. A first irradiation step and a second irradiation step are performed. In the first irradiation step, the levitated block 12 of glass raw material is heated to melting by irradiating the block 12 of glass raw material with the laser light. In the second irradiation step, an intensity of the laser light being applied to the molten glass is reduced and irradiation with the laser light is then stopped.
-
公开(公告)号:US20170158549A1
公开(公告)日:2017-06-08
申请号:US15316590
申请日:2015-05-29
Applicant: NIPPON ELECTRIC GLASS CO., LTD.
Inventor: Tomoko YAMADA , Fumio SATO
IPC: C03B32/00
Abstract: Provided is a method that can manufacture a glass material having excellent homogeneity by containerless levitation. A block (12) of glass raw material is heated and melted by irradiation with a plurality of laser beams with the block (12) of glass raw material held levitated, thus obtaining a molten glass, and the molten glass is then cooled to obtain a glass material. The plurality of laser beams include a first laser beam (13A) and a second laser beam (13B). A size (θ) of an angle formed between the first laser beam (13A) and the second laser beam (13B) is 0° or more but less than 180°. A center (C1) of a spot (S1) of the first laser beam (13A) on the surface of the block (12) of glass raw material and a center (C2) of a spot (S2) of the second laser beam (13B) on the surface of the block 12 of glass raw material are different from each other.
-
公开(公告)号:US20170153141A1
公开(公告)日:2017-06-01
申请号:US15319403
申请日:2015-08-04
Applicant: NIPPON ELECTRIC GLASS CO., LTD.
Inventor: Fumio SATO , Yoshimasa MATSUSHITA
Abstract: Provided is a novel infrared-transmitting glass that can be vitrified without containing any environmentally harmful compound and has high light transmissivity from visible range to a mid-infrared range of wavelengths of about 4 to about 8 μm. An infrared-transmitting glass containing, in % by mole, 50% or more TeO2, 0 to 45% (exclusive of 0%) ZnO, and 0 to 50% (exclusive of 0% and 50%) RO (where R is at least one selected from the group consisting of Ca, Sr, and Ba).
-
公开(公告)号:US20160311719A1
公开(公告)日:2016-10-27
申请号:US15103436
申请日:2014-12-16
Applicant: NIPPON ELECTRIC GLASS CO., LTD.
Inventor: Tomoko YAMADA , Fumio SATO
CPC classification number: C03C4/10 , C03C3/321 , C03C2204/00 , G01J1/0437 , G01J1/42 , G02B5/208
Abstract: Provided is a thermally stable and inexpensive infrared transmitting glass. An infrared transmitting glass containing, in % by mole, 0 to 20% Ge (exclusive of 0% and 20%), 0 to 40% Sb (exclusive of 0%), 0 to 20% Bi (exclusive of 0%), and 50 to 80% S+Se+Te.
Abstract translation: 提供了一种热稳定且廉价的红外透射玻璃。 一种红外透射玻璃,其含有0〜20%的Ge(不含0%和20%),0〜40%Sb(不含0%),0〜20%Bi(不含0%), 和50〜80%的S + Se + Te。
-
20.
公开(公告)号:US20160221863A1
公开(公告)日:2016-08-04
申请号:US15021288
申请日:2014-09-26
Applicant: Nippon Electric Glass Co., Ltd.
Inventor: Takashi MURATA , Fumio SATO
CPC classification number: C03C3/093 , C03C3/085 , C03C3/087 , C03C3/091 , C03C21/002 , G06F1/1626 , H04M1/0202 , H04M1/0266 , H04M1/03
Abstract: Provided is a tempered glass which is suitable for protection of a display or the like and allows transmission of an infrared ray having a wavelength of from 5 μm to 20 μm. The tempered glass has a compressive stress layer on its surface and has formed therein a through hole penetrating through the tempered glass so as to pass through the surface.
Abstract translation: 本发明提供一种适用于保护显示器等并且允许透射波长为5μm至20μm的红外线的钢化玻璃。 钢化玻璃在其表面上具有压应力层,并且在其中形成有穿过钢化玻璃的通孔,以穿过表面。
-
-
-
-
-
-
-
-
-