A method for forming mesophase pitch can include applying a stimulus to a first amount of coal tar to form a first amount of mesophase pitch. The stimulus can include one or more of an electromagnetic field (“EMF”) or a magnetic field. The method can further include evaluating a characteristic of the first amount of mesophase pitch, changing a parameter of the stimulus in response to evaluating the characteristic of the first amount of mesophase pitch, and applying the stimulus exhibiting the changed parameters to a second amount of coal tar to form mesophase pitch.
摘要:
A method for forming mesophase pitch can include applying a stimulus to a first amount of coal tar to form a first amount of mesophase pitch. The stimulus can include one or more of an electromagnetic field (“EMF”) or a magnetic field. The method can further include evaluating a characteristic of the first amount of mesophase pitch, changing a parameter of the stimulus in response to evaluating the characteristic of the first amount of mesophase pitch, and applying the stimulus exhibiting the changed parameters to a second amount of coal tar to form mesophase pitch.
摘要:
A method of producing low CTE graphite electrodes from needle coke formed from a coal tar distillate material having a relatively high initial boiling point.
摘要:
Mechanical visbreaking and pyrolysis between counter-rotating coaxial centrifugal impellers in a continuous radial counterflow process minimizes wastewater discharges. In an embodiment, a cataclastic shear retort comminutes, shear thins, and shear heats an axial feed, such as tar sand, oil shale, coal tailings, distillation bottoms, or lignite. Pyrolyzing the feedstock in this shear retort yields a product stream of gases, naphthas, and oils which first mixes with the feedstock and then is axially extracted, while spent solids are simultaneously extruded from the periphery as coked devolatilized residue, such as char sand for upgrading soil to terra preta. Recirculation of shear-heated solids in long residence time within the shear retort brings heat from the spent solids at the periphery to the feedstock without an external heated sand loop. CO2 emissions from combustion to heat water for oil extraction are eliminated.
摘要:
Embodiments of a method are described for modifying pitches, oils, tars, and binders by using these materials as solvents to extract organic chemicals from coal.
摘要:
A method of making a carbon/graphite product using a coal tar pitch having a softening point in the range of about 150° C. to 250° C. Also, a carbon/graphite product having a softening point in the range of about 150° C. to 250° C. A method of making mesophase pitch is formed from quinoline insoluble free coal tar pitch distillate from a high efficiency evaporative distillation process.
摘要:
Described are methods that utilize high efficiency evaporative distillation to make a high softening point coal tar pitch, a quinoline insoluble-free and ash-free coal tar pitch having a desired softening point, and a mesophase coal tar pitch. Each of the methods uses a feed coal tar pitch having a softening point in the range of 70° C. to 160° C. The methods may be carried out using appropriate conventional distillation equipment, a wiped film evaporator, or a thin film evaporator.
摘要:
An isotropic coal tar pitch having a low content of carcinogenic compounds is prepared by distilling a coal tar pitch in an evaporator having a specific evaporator surface of from 330 to 10,000 m.sup.2 /m.sup.3, at a temperature in the range of from 300.degree. to 380.degree. C., under a pressure not exceeding 1 mbar, whereby the average stay period is from 2 to 10 minutes. The isotropic pitch thus obtained contains less that 50 ppm of benzo[a]pyrene and is suitable, optionally after adding an oil, resin or other modifying agents having a low benzo[a]pyrene content, for use as binding and impregnating agent and also as protecting agent in construction materials or as varnish (painting agent).
摘要翻译:具有低含量致癌化合物的各向同性煤焦油沥青通过在具有330至10,000m 2 / m 3的特定蒸发器表面的蒸发器中蒸馏煤焦油沥青而制备,温度范围为300-380℃ C.在不超过1毫巴的压力下,平均逗留时间为2至10分钟。 由此获得的各向同性沥青包含少于50ppm的苯并[a]芘,并且任选地在加入具有低苯并[a]芘含量的油,树脂或其它改性剂之后,适合用作结合和浸渍剂,并且还 作为建筑材料中的保护剂或清漆(涂漆剂)。