摘要:
A method of making a refractory article is provided. The method includes: a) mixing a binder system, a refractory charge, and a second colloidal binder to form an aqueous slurry; b) casting the aqueous slurry into a mold; c) subjecting the mold containing the aqueous slurry to a temperature that is lower than a slurry casting temperature for a time sufficient to form a green strength article; and d) firing the green strength article at a temperature of at least 450° C. for a time sufficient to achieve thermal homogeneity, thereby forming a refractory article. Refractory articles made in accordance with the method have a unique combination of pore structure and mechanical properties.
摘要:
A preparation method and use of a green fluorescent transparent ceramic are disclosed. The preparation method includes: weighing, according to a stoichiometric ratio, elements present in Ca3-x-yCexAySc2-xBzSi3-mCmO12, in forms of oxides, carbonates or nitrates as raw materials; mixing the raw materials, annealing, melting at a high temperature, cooling and annealing at a low temperature; putting the glass into a high-temperature furnace, holding, raising the temperature, and performing crystallization and densification sintering; finally cutting, reducing and surface-polishing, where A is at least one from the group consisting of Lu, Y, Gd, La and Na; B is at least one from the group consisting of Zr, Hf and Mg; C is at least one from the group consisting of Al and P; x, y, z and m satisfy 0.001≤x≤0.06, 0≤y≤0.06, 0≤z≤0.06 and 0≤m≤0.3, respectively.
摘要:
Various embodiments of the present invention relate to reactive media including calcium. A reactive media includes a vitrified calcium silicate comprising reactive calcium. Various embodiments of the reactive media described herein are useful for removal of anionic impurities such as phosphate from water.
摘要:
The invention provides novel paving stones and construction block composite materials and methods for preparation thereof. The paving stones and construction block composite materials can be readily produced from widely available, low cost precursor materials by a production process that involves compacting in a mold that is suitable for large-scale production. The precursor materials include calcium silicate, for example, wollastonite, and particulate filler materials which can comprise silicon dioxide-rich materials. Additives can include calcium carbonate-rich and magnesium carbonate-rich materials. Various additives can be used to fine-tune the physical appearance and mechanical properties of the composite material, such as colorants such as particles of colored materials, such as, and pigments (e.g., black iron oxide, cobalt oxide and chromium oxide). These paving stones and construction block composite materials exhibit visual patterns similar to stone as well as display compressive strength and water absorption equal to or better than that of stone.
摘要:
Process for the moderately refractory assembly of at least two articles made of silicon carbide-based materials by non-reactive brazing in an oxidizing atmosphere, in which the articles are placed in contact with a non-reactive brazing composition and the assembly formed by the articles and the brazing composition is heated in an oxidizing atmosphere at a brazing temperature sufficient to melt the brazing composition so as to form a moderately refractory joint, wherein the non-reactive brazing composition is a composition A composed of silica (SiO2), alumina (Al2O3) and calcium oxide (CaO), or alternatively a composition B composed of alumina (Al2O3), calcium oxide (Cao) and magnesium oxide (MgO).Brazing suspension, paste comprising a powder of said brazing composition and an organic binder.Refractory joint and assembly.
摘要:
The invention provides novel aerated composite materials that possess excellent physical and performance characteristics of aerated concretes, and methods of production and uses thereof. These composite materials can be readily produced from widely available, low cost raw materials by a process suitable for large-scale production with improved energy consumption, desirable carbon footprint and minimal environmental impact.
摘要:
A method of preparing and rapidly curing a composite material having a thin cross section. The composite material includes a mixture of solid particles, at least some of which are a material that reacts with CO2, such as a silicate, for example Wollastonite. The green material is prepared by mixing the solid components with a liquid such as water to form a slurry, and forming green bodies by placing the slurry in forms. The green bodies are reacted with CO2 to form cured composite materials having thin sections, in the range of 10 to 15 mm. Curing in periods of 6 hours has been demonstrated.
摘要:
An inorganic fibrous shaped refractory article having a high bio-solubility which is capable of exhibiting a desired heat resistance without containing expensive ceramic fibers, alumina powder and silica powder can be provided at a low production cost and with a low product price.An inorganic fibrous shaped refractory article includes 2 to 95 mass % of rock wool, 2 to 95 mass % of inorganic powder having a needle-like crystal structure and 3 to 32 mass % of a binder. Preferably, in the an inorganic fibrous shaped refractory article, the inorganic powder having a needle-like crystal structure has an average length of 1 to 3000 μm and an aspect ratio of 1 to 1000, and more preferably the inorganic powder having a needle-like crystal structure is wollostonite powder or sepiolite powder.
摘要:
An inorganic fibrous shaped body including partially-crystallized bio-soluble inorganic fibers and an inorganic binder, wherein the bio-soluble inorganic fibers are SiO2/MgO fibers or SiO2/CaO fibers having the following composition: [SiO2/MgO fibers] SiO2 66 to 82 wt % CaO 1 to 9 wt % MgO 10 to 30 wt % Al2O3 3 wt % or less [SiO2/CaO fibers] SiO2 66 to 82 wt % CaO 10 to 34 wt % MgO 3 wt % or less Al2O3 5 wt % or less.
摘要:
The present invention relates to a biocompatible ceramic material comprising Sr, Mg or Ba doped Hardystonite (Ca2ZnSi2O7), and a method for its synthetic preparation. The present invention also relates to an implantable medical device comprising biocompatible doped Hardystonite, and a method for its production. The present invention further relates to a method for improving the long term stability of an implantable medical device and an implantable drug delivery device comprising doped Hardystonite. Further, the present invention relates to the use of comprising biocompatible doped Hardystonite in the regeneration or resurfacing of tissue.