摘要:
Disclosed are a non-normalized steel composition which includes carbon (C), silicon (Si), manganese (Mn), sulfur (S), vanadium (V), titanium (Ti), nitrogen (N), and iron (Fe), and a method of manufacturing the connecting rod for improving yield strength, fatigue strength, and the like of the connecting rod. The non-normalized steel composition includes carbon (C) in an amount of about 0.30 to 0.55 weight %, silicon (Si) in an amount of about 0.80 to 1.20 weight %, manganese (Mn) in an amount of about 0.80 to 1.20 weight %, sulfur (S) in an amount of about 0.06 to 0.10 weight %, vanadium (V) in an amount of about 0.20 to 0.35 weight %, titanium (Ti) in an amount of about 0.01 to 0.20 weight %, nitrogen (N) in an amount of about 0.005 to 0.02 weight %, and the remainder of iron (Fe), and inevitable impurities, based on a total weight of the composition.
摘要:
Processes and apparatuses for micro-treating iron-based alloys to transform and/or shape them and the resulting materials obtained by treating low, medium, and high carbon steel and other iron-based alloys to form at least a mixed microstructure that may contain martensite, bainite and un-dissolved carbides, and may also contain complex steel microstructures including portions of bainite, coalesced bainite, acicular ferrite, retained austenite and/or martensite along with combinations thereof by micro-treating said iron based alloy.
摘要:
The invention relates to a method for producing a friction element (3) comprising the steps: providing a metal main body (10), hardening the main body (10) on at least part of its surface (11, 12) in a salt bath, wherein the salt bath hardening is the final method step, and no further processing of the hardened surface (11, 12) is performed. Furthermore, the invention relates to a friction element produced according to this method and a friction component comprising the latter.
摘要:
A method continuously creates a bainite structure in a carbon steel, especially a strip steel by austenitizing the carbon steel; introducing the austenitized carbon steel into a bath containing a quenching agent; adjusting the carbon steel to the transformation temperature for bainite and maintaining the transformation temperature for a certain period of time; and then cooling the carbon steel. The carbon steel stays in the bath until a defined percentage of the bainite structure relative to the total structure of the carbon steel has formed. Residues of the quenching agent are removed from the surface of the carbon steel by blowing the same off when the carbon steel is discharged from the bath, and the remaining structure components of the carbon steel are then transformed into bainite in an isothermal tempering station without deflecting the carbon steel at all.
摘要:
The present invention is directed to a method of extending the life of thin walled tubing by austempering the tubing in a controlled continuous run process involving heating, quenching, and cooling the tubing pursuant to predetermined process parameters. The invention is also directed to a process for austempering tubing having a welded seam and for relieving residual stress in the weld. The invention is further directed to the product of the above processes as well as an austempered weld stress relieved thin walled tubing and such tubing in combination with other apparatus with which it is suitable for use in the production of hydrocarbons.
摘要:
Ferritic nitrocarburized surface treatment of cast iron brake rotors providing oxidation resistance, good braking performance and absence of distortion. Machined brake rotors are pre-heated, then immersed into a high temperature molten nitrocarburizing salt bath for a first predetermined dwell time. After removing the brake rotors from the nitrocarburizing salt bath, the brake rotors are directly immersed into an oxidizing salt bath at a lower temperature than the nitrocarburizing salt bath so that the brake rotors are thermally quenched. After a predetermined second dwell time in the oxidizing salt bath, the brake rotors are removed therefrom and further cooled to room temperature, either by water application thermal quenching or slow cooling in air. A fixture provides stable holding the brake rotors with a minimum of contact during placement in the salt baths.
摘要:
The method comprises effecting the solidification of the metal in a continuous casting ingot mould constituted by two cooled rolls (2) rotating in opposite directions and disposed in confronting relation so as to define a casting space therebetween, continuously extracting from the ingot mould a solidified steel strip (3), and, below the ingot mould, subjecting the strip to a quenching medium (6) so as to cool it sufficiently rapidly to prevent formation of austenite. This medium may be formed by a quenching bath placed in a container (4) disposed under the rolls (2) and having a bottom provided with an opening (5) for the passage of the solidified strip (3). The quenching medium may also be formed by an inert gas in the liquid state blown onto the product by nozzles. The steel strips obtained are easier to shear and coiled at the output end of the casting line owing to the absence of martensite in the ferritic matrix.
摘要:
Iron and steel construction parts which have been treated in a high cyanate, low cyanide or cyanide free nitriding salt bath or in other cyanide containing salt baths are tempered in a bath comprising an alkali metal hydroxide. There also can be present in the cooling bath 2 to 20 weight % of an alkali nitrate.
摘要:
A cold rolled and hardened martensitic austenitic stainless steel strip for flapper valves in compressors is made from steel combining, in weight %(wt. %), the following elements: C: 0.3-0.5, Si: 0.2-0.8, Mn: 0.2-1.0, Cr: 12.0-15.0, Mo: 0.50-2.00, N: 0.02-0.15, and V: 0.01-0.20. The steel strip has a matrix consisting of tempered martensite and between 5 and 15 volume % austenite and a tensile strength (Rm) of 1970-2300 MPa. The steel strip has a thickness of 0.07-3 mm and a width of ≦500 mm.
摘要:
The invention relates to a method for producing a friction element (3) comprising the steps: providing a metal main body (10), hardening the main body (10) on at least part of its surface (11, 12) in a salt bath, wherein the salt bath hardening is the final method step, and no further processing of the hardened surface (11, 12) is performed. Furthermore, the invention relates to a friction element produced according to this method and a friction component comprising the latter.