公开(公告)号:US12258495B2
公开(公告)日:2025-03-25
申请号:US16720149
申请日:2019-12-19
Inventor: Nicky Chan , Olivia Gady , Choung-Houng Lai , Yubo Cui , James N. Gordon
IPC: C09J151/00 , C08F2/50 , C08F220/06 , C08F220/18 , C08F236/20 , C08F236/22 , C08K5/00 , C08K5/01 , C08K5/132 , C08K5/37 , C08K7/28 , C09J7/38 , C09J133/08 , C09J133/10 , G01R23/00 , G01R31/00 , G01R31/30 , G01R31/317 , H04L9/08 , H04L9/32
Abstract: An adhesive may include an adhesive structure and an adhesive composition. The adhesive structure may include a graft copolymer. The adhesive composition may include at least about 1 wt. % and not greater than 40 wt. % of a macromonomer component for a total weight of the adhesive composition, at least about 50 wt. % and not greater than about 98 wt. % of a (meth)acrylic based polymeric component A for a total weight of the adhesive composition, and at least about 0.1 wt. % and not greater than about 30 wt. % of a tackifier component for a total weight of the adhesive composition. The macromonomer component may have a weight-average molecular weight of at least 1000 g/mol and a glass transition temperature (Tg) of at least about 40° C. The (meth)acrylic based polymeric component A may have a glass transition temperature (Tg) of not greater than about 20° C.
-
公开(公告)号:US20200208025A1
公开(公告)日:2020-07-02
申请号:US16720158
申请日:2019-12-19
Inventor: Yubo CUI , Thomas L. Adams , David A. Elliott , James N. Gordon
IPC: C09J133/08 , C09J7/38 , C08K5/01
Abstract: An adhesive composition may include at least about 2 wt. % and not greater than 49 wt. % of a (meth)acrylic based polymeric component A for a total weight of the adhesive composition, at least about 51 wt. % of a (meth)acrylic based polymeric component B for a total weight of the adhesive composition, and at least about 0.1 wt. % and not greater than about 30 wt. % of a tackifier component for a total weight of the adhesive composition. The (meth)acrylic based polymeric component A may have a glass transition temperature (Tg) of at least about 40° C. The (meth)acrylic based polymeric component B may have a glass transition temperature (Tg) of not greater than about 20° C. Further, the (meth)acrylic based polymeric component B may be acid-free.
-
公开(公告)号:US09272499B2
公开(公告)日:2016-03-01
申请号:US14455643
申请日:2014-08-08
Inventor: Thomas A. Veilleux , James N. Gordon , Stewart B. Dittmeier
IPC: E06B3/54 , B32B37/12 , C03C27/04 , C09J7/02 , E06B3/56 , B32B37/02 , B32B37/14 , B32B37/22 , B32B38/00 , B32B5/18 , B32B7/12
CPC classification number: B32B37/1284 , B32B5/18 , B32B7/12 , B32B37/02 , B32B37/144 , B32B37/223 , B32B38/00 , B32B38/0008 , B32B38/0036 , B32B2038/0056 , B32B2305/022 , B32B2305/77 , B32B2307/748 , B32B2310/0409 , B32B2310/0831 , B32B2311/00 , B32B2315/08 , B32B2327/18 , B32B2375/00 , B32B2383/00 , B32B2398/00 , B32B2419/00 , C03C27/048 , C09J7/26 , C09J7/40 , E06B3/5427 , E06B3/56 , Y10T428/249983
Abstract: A method of preparing a window module includes providing a metal frame having a first major surface, applying a structural glazing tape to the first major surface of the metal frame, and positioning a glass panel overtop the structural glazing tape. The structural glazing tape includes a polymer foam tape having first and second major surfaces, an adhesive layer overlying the first major surface for bonding the structural glazing tape to the structural frame, and a release layer overlying the second major surface. The method further includes filling a channel defined by the glass panel, the metal frame, and the structural glazing tape with a curable sealant, and curing the sealant to bond the glass panel and the metal frame together.
Abstract translation: 一种制备窗户模块的方法包括提供具有第一主表面的金属框架,将金属框架的第一主表面施加结构玻璃带,并将玻璃面板定位在结构上光带上方。 结构玻璃带包括具有第一和第二主表面的聚合物泡沫带,覆盖在第一主表面上用于将结构玻璃胶带粘结到结构框架上的粘合剂层和覆盖在第二主表面上的剥离层。 该方法还包括用可固化密封剂填充由玻璃面板,金属框架和结构玻璃胶带限定的通道,并固化密封剂以将玻璃面板和金属框架结合在一起。
-
公开(公告)号:US11512229B2
公开(公告)日:2022-11-29
申请号:US16712286
申请日:2019-12-12
Inventor: Qing Diao , Yue Dong , Russell S. Cook , James N. Gordon
IPC: C09J7/26 , C08G18/08 , C08G18/42 , C09J7/25 , C09J7/30 , C08J9/00 , B32B5/18 , B32B27/06 , C08G18/76 , C08K7/22 , C08K3/26
Abstract: A polyurethane foam may include an isocyanate polymer component and a polyol component. The polyol component may include a polyol having a molecular weight of at least about 500 kg/mol and not greater than about 6000 kg/mol. The polyurethane foam may have an elongation of at least about 500%. The polyurethane foam may further have a density of at least about 250 g/L and a tensile strength of not greater than about 1000 kPa.
-
公开(公告)号:US20140345782A1
公开(公告)日:2014-11-27
申请号:US14455643
申请日:2014-08-08
Inventor: Thomas A. Veilleux , James N. Gordon , Stewart B. Dittmeier
CPC classification number: B32B37/1284 , B32B5/18 , B32B7/12 , B32B37/02 , B32B37/144 , B32B37/223 , B32B38/00 , B32B38/0008 , B32B38/0036 , B32B2038/0056 , B32B2305/022 , B32B2305/77 , B32B2307/748 , B32B2310/0409 , B32B2310/0831 , B32B2311/00 , B32B2315/08 , B32B2327/18 , B32B2375/00 , B32B2383/00 , B32B2398/00 , B32B2419/00 , C03C27/048 , C09J7/26 , C09J7/40 , E06B3/5427 , E06B3/56 , Y10T428/249983
Abstract: A method of preparing a window module includes providing a metal frame having a first major surface, applying a structural glazing tape to the first major surface of the metal frame, and positioning a glass panel overtop the structural glazing tape. The structural glazing tape includes a polymer foam tape having first and second major surfaces, an adhesive layer overlying the first major surface for bonding the structural glazing tape to the structural frame, and a release layer overlying the second major surface. The method further includes filling a channel defined by the glass panel, the metal frame, and the structural glazing tape with a curable sealant, and curing the sealant to bond the glass panel and the metal frame together.
Abstract translation: 一种制备窗户模块的方法包括提供具有第一主表面的金属框架,将金属框架的第一主表面施加结构玻璃带,并将玻璃面板定位在结构上光带上方。 结构玻璃带包括具有第一和第二主表面的聚合物泡沫带,覆盖在第一主表面上用于将结构玻璃胶带粘结到结构框架上的粘合剂层和覆盖在第二主表面上的剥离层。 该方法还包括用可固化密封剂填充由玻璃面板,金属框架和结构玻璃胶带限定的通道,并固化密封剂以将玻璃面板和金属框架结合在一起。
-
-
-
-