公开(公告)号:US12157292B2
公开(公告)日:2024-12-03
申请号:US17664516
申请日:2022-05-23
Inventor: David A. Rich , Gerard T. Buss , James M. McMartin , Timothy P. Pollock
Abstract: The present disclosure relates to a composite article that may include a structural substrate, a multilayer fluoropolymer film that can include a high-melt fluoropolymer layer and a low-melt fluoropolymer adhesion layer that may contact the structural substrate and the fluoropolymer film. The high-melt fluoropolymer layer may have a melting temperature A1 and the low-melt fluoropolymer adhesive layer may have a melting temperature A2. The melting temperature A2 may be less than the melting temperature A1.
-
公开(公告)号:US10751973B2
公开(公告)日:2020-08-25
申请号:US15464909
申请日:2017-03-21
Inventor: Joseph G. Sargent , Michael P. Cushman , Michael J. Lussier , James M. McMartin
IPC: B32B5/26 , B32B5/02 , B32B7/04 , B32B25/10 , B32B25/20 , B32B27/12 , B32B27/18 , B32B27/28 , B32B27/30 , B32B27/32 , B32B37/24 , E04D5/02 , E04D5/10
Abstract: A composite fabric laminate can include an open mesh fabric, a first continuous film comprising a fluoropolymer, and a second continuous film comprising a fluoropolymer. The fluoropolymer of the first continuous film and the fluoropolymer of the second continuous films can be in direct contact with one another. A method of forming a composite fabric laminate that includes disposing an open mesh fabric between a first continuous film and a second continuous film, each comprising an at least partially unsintered fluoropolymer film, to form a composite; laminating the composite at a pressure of at least 100 psig and a temperature of no greater than 350° C.; and sintering the laminated composite to form the composite fabric laminate.
-
公开(公告)号:US10471680B2
公开(公告)日:2019-11-12
申请号:US15464909
申请日:2017-03-21
Inventor: Joseph G. Sargent , Michael P. Cushman , Michael J. Lussier , James M. McMartin
IPC: B32B5/26 , B32B5/02 , B32B27/32 , E04D5/10 , B32B37/24 , E04D5/02 , B32B7/04 , B32B25/10 , B32B25/20 , B32B27/12 , B32B27/18 , B32B27/28 , B32B27/30
Abstract: A composite fabric laminate can include an open mesh fabric, a first continuous film comprising a fluoropolymer, and a second continuous film comprising a fluoropolymer. The fluoropolymer of the first continuous film and the fluoropolymer of the second continuous films can be in direct contact with one another. A method of forming a composite fabric laminate that includes disposing an open mesh fabric between a first continuous film and a second continuous film, each comprising an at least partially unsintered fluoropolymer film, to form a composite; laminating the composite at a pressure of at least 100 psig and a temperature of no greater than 350° C.; and sintering the laminated composite to form the composite fabric laminate.
-
公开(公告)号:US20170266914A1
公开(公告)日:2017-09-21
申请号:US15464909
申请日:2017-03-21
Inventor: Joseph G. SARGENT , Michael P. Cushman , Michael J. Lussier , James M. McMartin
Abstract: A composite fabric laminate can include an open mesh fabric, a first continuous film comprising a fluoropolymer, and a second continuous film comprising a fluoropolymer. The fluoropolymer of the first continuous film and the fluoropolymer of the second continuous films can be in direct contact with one another. A method of forming a composite fabric laminate that includes disposing an open mesh fabric between a first continuous film and a second continuous film, each comprising an at least partially unsintered fluoropolymer film, to form a composite; laminating the composite at a pressure of at least 100 psig and a temperature of no greater than 350° C.; and sintering the laminated composite to form the composite fabric laminate.
-
-
-