Cubic boron nitride sintered material

    公开(公告)号:US11591266B2

    公开(公告)日:2023-02-28

    申请号:US17625750

    申请日:2020-07-17

    IPC分类号: C04B35/5831

    摘要: A cubic boron nitride sintered material includes: more than or equal to 50 volume % and less than 80 volume % of cubic boron nitride grains; and more than 20 volume % and less than or equal to 50 volume % of a binder phase, and when an oxygen content is measured in a direction perpendicular to an interface between cubic boron nitride grains using TEM-EDX, a first region having an oxygen content larger than an average value of an oxygen content of a cubic boron nitride grain exists, the interface exists in the first region, and a length of the first region along the direction perpendicular to the interface is more than or equal to 0.1 nm and less than or equal to 10 nm.

    Cubic boron nitride sintered material

    公开(公告)号:US11542203B2

    公开(公告)日:2023-01-03

    申请号:US17626064

    申请日:2020-07-17

    IPC分类号: C04B35/5831

    摘要: A cubic boron nitride sintered material includes: 20 to 80 volume % of cBN grains; and 20 to 80 volume % of a binder phase, wherein the binder phase includes first binder grains and second binder grains, in each of the first binder grains, a ratio of the number of atoms of the first metal element to a total of the number of atoms of the titanium and the number of atoms of the first metal element is more than or equal to 0.01% and less than 10%, in each of the second binder grains, this ratio is more than or equal to 10% and less than or equal to 80%, and in an X-ray diffraction spectrum of the cubic boron nitride sintered material, one or both of conditions 1 and 2 are satisfied.

    CUBIC BORON NITRIDE SINTERED MATERIAL

    公开(公告)号:US20220204412A1

    公开(公告)日:2022-06-30

    申请号:US17626051

    申请日:2020-07-17

    IPC分类号: C04B35/5831 C04B35/645

    摘要: A cubic boron nitride sintered material includes: 20 to 80 volume % of cBN grains; and 20 to 80 volume % of a binder phase, wherein the binder phase includes first binder grains and second binder grains, in each of the first binder grains, a ratio of the number of atoms of the first metal element to a total of the number of atoms of the titanium and the first metal element is more than or equal to 0.01% and less than 10%, in each of the second binder grains, the ratio is more than or equal to 10% and less than or equal to 80%, and an average grain size of the second binder grains is more than or equal to 0.2 μm and less than or equal to 1 μm.

    SINTERED POLYCRYSTALLINE CUBIC BORON NITRIDE MATERIAL

    公开(公告)号:US20210403385A1

    公开(公告)日:2021-12-30

    申请号:US16490152

    申请日:2018-03-13

    摘要: A method of making a polycrystalline cubic boron nitride (PCBN), material is provided. The matrix precursor powder comprises an aluminium compound. The method comprises mixing matrix precursor powder comprising particles having an average particle size no greater than 250 nm, with between 30 and 40 volume percent of cubic boron nitride (cBN) particles having an average particle size of at least 4 μm, and then spark plasma sintering the mixed particles. The spark plasma sintering occurs at a pressure of at least 500 MPa, a temperature of no less than 1050° C. and no more than 1500° C. and a time of no less than 1 minute and no more than 3 minutes.