Abstract:
Provided is a slurry composition for a non-aqueous secondary battery positive electrode that has excellent stability and enables formation of a positive electrode mixed material layer that causes a non-aqueous secondary battery to display excellent output characteristics. The slurry composition contains a positive electrode active material and a copolymer. The proportion constituted by nickel among transition metal in the positive electrode active material is at least 30.0 mol % and not more than 100.0 mol %. The copolymer includes a nitrile group-containing monomer unit in a proportion of at least 70.0 mass % and not more than 96.0 mass % and a basic group-containing monomer unit in a proportion of at least 0.1 mass % and not more than 5.0 mass %.
Abstract:
Composite particles for electrochemical device electrode comprising a first particle-shaped binder with a glass transition temperature of 5° C. or less, a second particle-shaped binder with a glass transition temperature of 10 to 80° C. and with a gel content of 70 wt % or more, and an electrode active material, wherein a ratio of content of said second particle-shaped binder is 30 to 95 wt % in the total binder which is contained in said composite particles for electrochemical device electrode, are provided.
Abstract:
A nozzle part dropping a slurry and a rotary disk centrifugally spraying the slurry to be dropped from the nozzle part are included. The rotary disk includes a plurality of grooves stretching in a radiation direction at least in a periphery part of a surface on which the slurry is sprayed.
Abstract:
A disclosed binder composition comprises a copolymer which comprises a nitrile group-containing monomer unit, an acidic group-containing monomer unit and a basic group-containing monomer unit, wherein the proportion of the nitrile group-containing monomer unit in the copolymer is 70.0 mol % or more and 99.0 mol % or less, and wherein the total proportion of the acidic group-containing monomer unit and the basic group-containing monomer unit in the copolymer is 0.8 mol % or more and 10.0 mol % or less.