公开(公告)号:USD1061074S1
公开(公告)日:2025-02-11
申请号:US29971594
申请日:2024-11-05
Applicant: Weidong Xue
Designer: Weidong Xue
-
公开(公告)号:US08076959B2
公开(公告)日:2011-12-13
申请号:US12607279
申请日:2009-10-28
Applicant: Xiaohu Tang , Weidong Xue , Yan Li
Inventor: Xiaohu Tang , Weidong Xue , Yan Li
IPC: H03K5/153
CPC classification number: G01R19/16538 , G01R19/16566 , G06F1/28
Abstract: A circuit for detecting an input voltage includes a voltage-to-current converter and a current comparator. The voltage-to-current converter is operable for generating a monitoring current that varies in accordance with the input voltage. The current comparator coupled to the voltage-to-current converter is operable for comparing the monitoring current to a threshold current proportional to the temperature of the circuit, and for generating a detection signal indicating a condition of the input voltage based on a result of the comparison.
Abstract translation: 用于检测输入电压的电路包括电压 - 电流转换器和电流比较器。 电压 - 电流转换器可用于产生根据输入电压而变化的监控电流。 耦合到电压 - 电流转换器的电流比较器可操作用于将监测电流与电路温度成比例的阈值电流进行比较,并且用于基于所述电压转换器的结果产生指示输入电压的条件的检测信号 比较。
-
公开(公告)号:US09303297B2
公开(公告)日:2016-04-05
申请号:US12741556
申请日:2008-10-30
Applicant: Weidong Xue
Inventor: Weidong Xue
IPC: C21D1/42 , C21D9/00 , B62D55/21 , C21D1/06 , C21D1/10 , C21D1/18 , C21D9/08 , C22C38/02 , C22C38/04 , C22C38/22 , C21D1/00
CPC classification number: C21D9/0068 , B62D55/211 , C21D1/06 , C21D1/10 , C21D1/18 , C21D1/25 , C21D1/42 , C21D1/78 , C21D9/0075 , C21D9/0093 , C21D9/08 , C21D2211/008 , C21D2221/10 , C22C38/02 , C22C38/04 , C22C38/22 , Y02P10/253
Abstract: The present invention relates to a method for heat treatment of a columnar work. In order to provide the method for heat treatment of a columnar work being able to attain a high productivity, a reduction of cost, and an improvement of quality, as compared with the prior art, the method for heat treatment of a columnar work of the present invention includes a quench-hardening step (S1) and a tempering step (S2) being carried out after the quench-hardening step (S1), the quench-hardening step (S1) includes a first quench-hardening step (S11) and a second quench-hardening step (S12) being carried out after the first quench-hardening step (S11), the entire region of the columnar work (3) from an outer circumferential surface (31f) to a core thereof (32), or a partial region thereof, is heated up to a temperature not lower than a transformation temperature Ac3, and then, the work is quench-hardened.
Abstract translation: 本发明涉及柱状工件的热处理方法。 为了提供能够实现高生产率,降低成本和提高质量的柱状工件的热处理方法,与现有技术相比,本发明的热处理方法 本发明包括淬火硬化步骤(S1)和在淬火硬化步骤(S1)之后进行的回火步骤(S2),淬火硬化步骤(S1)包括第一淬火步骤(S11)和 在第一淬火硬化步骤(S11)之后,将圆柱形工件(3)的整个区域从外周表面(31f)到其芯(32)进行的第二淬火硬化步骤(S12),或 将其部分区域加热到不低于转变温度Ac3的温度,然后将工件淬火硬化。
-
公开(公告)号:US20100252150A1
公开(公告)日:2010-10-07
申请号:US12741556
申请日:2008-10-30
Applicant: Weidong Xue
Inventor: Weidong Xue
CPC classification number: C21D9/0068 , B62D55/211 , C21D1/06 , C21D1/10 , C21D1/18 , C21D1/25 , C21D1/42 , C21D1/78 , C21D9/0075 , C21D9/0093 , C21D9/08 , C21D2211/008 , C21D2221/10 , C22C38/02 , C22C38/04 , C22C38/22 , Y02P10/253
Abstract: The present invention relates to a method for heat treatment of a columnar work. In order to provide the method for heat treatment of a columnar work being able to attain a high productivity, a reduction of cost, and an improvement of quality, as compared with the prior art, the method for heat treatment of a columnar work of the present invention includes a quench-hardening step (S1) and a tempering step (S2) being carried out after the quench-hardening step (S1), the quench-hardening step (S1) includes a first quench-hardening step (S11) and a second quench-hardening step (S12) being carried out after the first quench-hardening step (S11), the entire region of the columnar work (3) from an outer circumferential surface (31f) to a core thereof (32), or a partial region thereof, is heated up to a temperature not lower than a transformation temperature Ac3, and then, the work is quench-hardened.
Abstract translation: 本发明涉及柱状工件的热处理方法。 为了提供能够实现高生产率,降低成本和提高质量的柱状工件的热处理方法,与现有技术相比,本发明的热处理方法 本发明包括淬火硬化步骤(S1)和在淬火硬化步骤(S1)之后进行的回火步骤(S2),淬火硬化步骤(S1)包括第一淬火步骤(S11)和 在第一淬火硬化步骤(S11)之后,将圆柱形工件(3)的整个区域从外周表面(31f)到其芯(32)进行的第二淬火硬化步骤(S12),或 将其部分区域加热到不低于转变温度Ac3的温度,然后将工件淬火硬化。
-
-
-