公开(公告)号:US20170247833A1
公开(公告)日:2017-08-31
申请号:US15067760
申请日:2016-03-11
Applicant: WEYERHAEUSER NR COMPANY
Inventor: Mengkui Lou
CPC classification number: D21C9/005 , C08B15/10 , C08H8/00 , D21C9/1063 , D21C9/147 , D21C9/18 , D21H13/04
Abstract: A pulp in accordance with a particular embodiment includes crosslinked cellulose fibers. The pulp can have high brightness, reactivity, and intrinsic viscosity. The pulp, therefore, can be well suited for use as a precursor in the production of low-color, high-viscosity cellulose derivatives. A method in accordance with a particular embodiment of the present technology includes forming a pulp from a cellulosic feedstock, bleaching the pulp, crosslinking cellulose fibers within the pulp while the pulp has a high consistency, and drying the pulp. The bleaching process can reduce a lignin content of the pulp to less than or equal to 0.09% by oven-dried weight of the crosslinked cellulose fibers. Crosslinking the cellulose fibers can include exposing the cellulose fibers to a glycidyl ether crosslinker having two or more glycidyl groups and a molecular weight per epoxide within a range from 140 to 175.
-
公开(公告)号:US20170247839A1
公开(公告)日:2017-08-31
申请号:US15067749
申请日:2016-03-11
Applicant: WEYERHAEUSER NR COMPANY
Inventor: Mengkui Lou
IPC: D21H13/04
CPC classification number: D21C9/005 , C08B15/10 , C08H8/00 , D21C9/1063 , D21C9/147 , D21C9/18 , D21H13/04
Abstract: A pulp in accordance with a particular embodiment includes crosslinked cellulose fibers. The pulp can have high brightness, reactivity, and intrinsic viscosity. The pulp, therefore, can be well suited for use as a precursor in the production of low-color, high-viscosity cellulose derivatives. A method in accordance with a particular embodiment of the present technology includes forming a pulp from a cellulosic feedstock, bleaching the pulp, crosslinking cellulose fibers within the pulp while the pulp has a high consistency, and drying the pulp. The bleaching process can reduce a lignin content of the pulp to less than or equal to 0.09% by oven-dried weight of the crosslinked cellulose fibers. Crosslinking the cellulose fibers can include exposing the cellulose fibers to a glycidyl ether crosslinker having two or more glycidyl groups and a molecular weight per epoxide within a range from 140 to 175.
-