Resin composition and molded article thereof

    公开(公告)号:US10119024B2

    公开(公告)日:2018-11-06

    申请号:US15673953

    申请日:2017-08-10

    摘要: Disclosed is a resin composition including at least a polyamide (A) and a polyrotaxane (B) whose cyclic molecule is modified with a graft chain, which are mixed together, wherein 80 parts by weight or more and 99.9 parts by weight or less of the polyamide (A) and 0.1 part by weight or more and 20 parts by weight or less of the polyrotaxane (B) are mixed together relative to 100 parts by weight of the total amount of the polyamide (A) and the polyrotaxane (B). To provide a resin composition capable of affording a molded article having excellent balance between rigidity and toughness.

    Method of producing polyamide fine particles, and polyamide fine particles

    公开(公告)号:US11685813B2

    公开(公告)日:2023-06-27

    申请号:US17288959

    申请日:2019-10-24

    IPC分类号: C08J3/14 C08G69/08

    摘要: A method produces polyamide fine particles by polymerizing a polyamide monomer (A) in the presence of a polymer (B) at a temperature equal to or higher than the crystallization temperature of a polyamide to be obtained, wherein the polyamide monomer (A) and the polymer (B) are homogeneously dissolved at the start of polymerization, and polyamide fine particles are precipitated after the polymerization. Polyamide fine particles have a number average particle size of 0.1 to 100 μm, a sphericity of 90 or more, a particle size distribution index of 3.0 or less, a linseed oil absorption of 100 mL/100 g or less, and a crystallization temperature of 150° C. or more.

    METHOD OF PRODUCING POLYAMIDE FINE PARTICLES, AND POLYAMIDE FINE PARTICLES

    公开(公告)号:US20210403651A1

    公开(公告)日:2021-12-30

    申请号:US17288959

    申请日:2019-10-24

    IPC分类号: C08J3/14 C08G69/08

    摘要: A method produces polyamide fine particles by polymerizing a polyamide monomer (A) in the presence of a polymer (B) at a temperature equal to or higher than the crystallization temperature of a polyamide to be obtained, wherein the polyamide monomer (A) and the polymer (B) are homogeneously dissolved at the start of polymerization, and polyamide fine particles are precipitated after the polymerization. Polyamide fine particles have a number average particle size of 0.1 to 100 μm, a sphericity of 90 or more, a particle size distribution index of 3.0 or less, a linseed oil absorption of 100 mL/100 g or less, and a crystallization temperature of 150° C. or more.

    FIBER-REINFORCED POLYAMIDE RESIN COMPOSITION MOLDED ARTICLE

    公开(公告)号:US20230272216A1

    公开(公告)日:2023-08-31

    申请号:US18016884

    申请日:2021-08-18

    摘要: A fiber-reinforced polyamide resin composition molded article is characterized by 5 to 50 parts by weight of reinforcing fibers, 40 to 94.9 parts by weight of a polyamide resin composition, and 0.1 to 10 parts by weight of an ammonium salt composed of ammonia and an aliphatic dicarboxylic acid having 6 to 12 carbon atoms, and which is also characterized in that: a weight average fiber length of the reinforcing fibers is 0.4 to 7 mm; the polyamide resin composition comprises a polyamide resin, a second resin having a reactive functional group, and a compound produced by a reaction of the resin and the second resin; and the second resin is dispersed in a form of particles with a number average particle diameter of 10 to 1,000 nm.