Abstract:
In some embodiments are an article including a woven fabric having warp yarns and weft yarns. Either warp yarn or weft yarn or both warp and weft yarns have two separate systems of yarns. The systems of yarns include a hard yarn forming the main body of fabric and a composite covered elastic yarn with an elastic fiber core; wherein the fabric has an outer face side, a back side, and the fabric includes at least one of: (a) a weaving pattern where the composite yarn and at least one adjacent hard yarn pass over the same pick when the composite yarn is on the outer surface; (b) the ratio of hard yarn denier to composite yarn denier is at least 1:1; and (c) the composite yarn floats over no more than 5 picks on the outer face side.
Abstract:
The invention provides a polyester bicomponent core spun yarn comprising a sheath of at least one hard fiber and having an English cotton count of from about 5 to about 60 and a core of bicomponent polyester filament. The invention further includes a fabric substantially free of grin-through of the bicomponent polyester filament.
Abstract:
Composite yarns, comprising one or more elastomeric fibers and hard yarns, are formed by adhering the elastomeric fibers and hard yarns together using a size material. The size-covered composite yarn can be used in weaving and knitting to make stretch fabrics with desired garment characteristics. The size material may be removed by subsequent wet fabric processing.
Abstract:
Included is a woven fabric having warp yarns and weft yarns. Either warp yarn or weft yarn or both warp and weft yarns have two separate systems of yarns. The systems of yarns include a hard yarn forming the main body of fabric and a composite covered elastic yarn with an elastic fiber core; wherein the fabric has an outer face side, a back side, and the fabric includes at least one of: (a) a weaving pattern where the composite yarn and at least one adjacent hard yarn pass over the same pick when the composite yarn is on the outer surface; (b) the ratio of hard yarn denier to composite yarn denier is at least 1:1; and (c) the composite yarn floats over no more than 5 picks on the outer face side.
Abstract:
Stretch woven fabrics including plain, twill and satin constructions are disclosed. The fabrics include weft yarns and warp yarns. Polyester bicomponent continuous filaments including poly(ethylene terephthalate) and poly(trimethylene terephthalate) having an after-heat-set crimp contraction value from about 20% to about 80% contribute to the stretch recovery properties.
Abstract:
The invention provides a polyester bicomponent core spun yarn comprising a sheath of at least one hard fiber and having an English cotton count of from about 5 to about 60 and a core of bicomponent polyester filament. The invention further includes a fabric substantially free of grin-through of the bicomponent polyester filament.
Abstract:
Warp stretch woven fabrics including plain, twill and satin constructions are disclosed. The fabrics include weft yarns and warp yarns. About 15 weight percent to about 55 weight percent of the warp yarns are polyester bicomponent continuous filaments comprising poly(ethylene terephthalate) and poly(trimethylene terephthalate) having an after-heat-set crimp contraction value from about 20% to about 80%.
Abstract:
The invention provides a polyester bicomponent core spun yarn comprising a sheath of at least one hard fiber and having an English cotton count of from about 5 to about 60 and a core of bicomponent polyester filament. The invention further includes a fabric substantially free of grin-through of the bicomponent polyester filament.
Abstract:
Methods for making stretch fabric having stretch between 10% to 45% in the weft and/or warp direction are disclosed. A corespun composite elastomeric yarn is produced either (a) by low draft (2.7× or below) core-spinning of the elastomeric yarn, or (b) by pretreating the corespun composite yarn in steam or heated water at temperatures of at least 110° C. to reduce yarn power before dyeing or weaving. The fabric with such corespun composite elastomeric yarn in the weft meets end-use specifications without heat-setting.
Abstract:
Methods for making stretch shirting fabric having fabric weight less than 175 g/m2 and fabric stretch between 15% to 45% in the weft direction are disclosed. A corespun composite elastomeric yarn is produced either (a) by low draft (2.7× or below) core-spinning of the elastomeric yarn, or (b) by pretreating the corespun composite yarn in steam or heated water at temperatures of at least 110° C. to reduce yarn power before dyeing or weaving. The shirting fabric with such corespun composite elastomeric yarn in the weft meets end-use specifications without heat-setting.
Abstract translation:公布了织物重量小于175g / m 2的拉伸衬衫织物在纬向方向拉伸15%至45%之间的方法。 (a)通过低速(2.7×或更低)的弹性纱线的芯纱纺丝,或(b)通过在至少110°的温度下在蒸汽或加热的水中预处理复合纱线 C.在染色或编织之前减少纱线力。 在纬纱中使用这种芯绒复合弹性纱线的衬衫织物满足最终用途规格而不进行热定型。