发明人: Xuzhen Zhang , Wenxing Chen , Yanlin Sun , Xiuhua Wang , Shaobo Liu , Xueyan Lin , Shunli Xiao
IPC分类号: D01D5/088 , B29B13/06 , D01D5/092 , D01D5/096 , D01D5/12 , D01D5/22 , D01D5/32 , D01D7/00 , D01D10/02 , D01D10/04 , D01D10/06 , D01F8/14 , D02G1/00 , D02J1/22 , D02J13/00 , B29B9/16
CPC分类号: D01D5/22 , B29B13/065 , D01D5/32 , D01D10/02 , D01D10/0409 , D01D10/06 , D01F8/14 , D02G1/004 , D02J1/228 , D02J13/003 , D02J13/005 , B29B2009/165 , D10B2331/04
摘要: The present invention discloses a method for preparing a PET/PTT parallel complex filament with high self-crimpiness, wherein PET and PTT are sliced, dried and crystallized, and then fused separately and subjected to extrusion molding through a parallel-type spinneret plate; oil is applied after cooling; then level 1-3 drafting and heat setting treatment are adopted; and during drafting, a total drafting rate is controlled to be 3 to 3.5, wherein the level-1 drafting rate is 2.8 to 3.0 at a temperature controlled to be 75 to 80° C., according to the method for preparing the PET/PTT parallel complex filament with high self-crimpiness, methods like multi-level drafting for increasing the drafting rate are adopted, and the effects of improving the fiber strength, moderately lowering the breaking elongation, and greatly improving the self-crimpiness are achieved.