公开(公告)号:US11232901B2
公开(公告)日:2022-01-25
申请号:US15738710
申请日:2016-07-01
IPC分类号: H01F41/02 , C21D6/00 , C21D9/52 , C21D1/26 , H01F27/25 , H01F3/04 , H01F1/153 , C22C45/02 , H01F1/147 , H01F27/245
摘要: A method for producing a magnetic core includes a processing step of giving a desired shape to a strip made of an alloy composition, a heat-treating step of forming bcc-Fe crystals, and then a stacking step of obtaining a magnetic core having a shape. Here, the alloy composition is Fe—B—Si—P—Cu—C and has an amorphous phase as a primary phase. In the heat-treating step, the strip is heated up to a temperature higher than a crystallization temperature of the alloy composition at a high heating rate.
-
公开(公告)号:US10388444B2
公开(公告)日:2019-08-20
申请号:US15327143
申请日:2015-07-17
IPC分类号: C22C33/02 , C22C38/00 , C22C38/02 , C22C38/10 , C22C38/16 , C22C45/02 , B22F1/00 , H01F1/147 , H01F1/20 , H01F1/153
摘要: Alloy powder of a composition formula Fe100-a-b-c-d-e-fCoaBbSicPdCueCf having an amorphous phase as a main phase is provided. Parameters satisfy the following conditions: 3.5≤a≤4.5 at %, 6≤b≤15 at %, 2≤c≤11 at %, 3≤d≤5 at %, 0.5≤e≤1.1 at %, and 0≤f≤2 at %. With this composition, the alloy powder has good magnetic characteristics even when it has a large particle diameter such as 90 μm. Therefore, yield thereof is improved.
-