Abstract:
A flame retardant with which fire retardancy is improved and the fire retardancy is able to be secured stably for a long time is provided. An internal layer 11 containing a polymer and a flame retardant factor layer 12 that is formed outside of the internal layer 11 and that contains a polymer to which at least one of a sulfonate group and a sulfonate base is bonded are included. Thereby, compared to a case that the flame retardant factor layer 12 is not included, moisture is hardly absorbed, and respective particles of the flame retardant are inhibited from being adhered to each other. Accordingly, blocking is inhibited.
Abstract:
To provide a halogen-free type polycarbonate resin composition and a resin molded object having good flame retardant properties and physical properties that make them suitable for the use as manufactured products.A resin composition of the present disclosure includes a component A, a component B, a component C and a component D. The component A is a polycarbonate resin. The component B is talc having an average median diameter of 4.6 μm or more and 6.0 μm or less, whose content is 5% or more and 20% or less by weight. The component C is an organic sulfonic acid or an organic sulfonic acid metal salt, whose content is 0.05% or more and 2.0% or less by weight. The component D is a drip inhibitor, whose content is 0.05% or more and 1.0% or less by weight.
Abstract:
A flame retardant resin composition in which an acrylonitrile-styrene based polymer, into which sulfonic acid groups and/or sulfonate groups have been introduced by sulfonating processing with a sulfonating agent containing less than 3 wt % of moisture, is contained in a resin to be made flame retardant, so that flame retardant properties will be conferred on the resin flame resistant.
Abstract:
A flame retardant with which fire retardancy is improved and the fire retardancy is able to be secured stably for a long time is provided. An internal layer 11 containing a polymer and a flame retardant factor layer 12 that is formed outside of the internal layer 11 and that contains a polymer to which at least one of a sulfonate group and a sulfonate base is bonded are included. Thereby, compared to a case that the flame retardant factor layer 12 is not included, moisture is hardly absorbed, and respective particles of the flame retardant are inhibited from being adhered to each other. Accordingly, blocking is inhibited.
Abstract:
A flame retardant resin composition in which an acrylonitrile-styrene based polymer, into which sulfonic acid groups and/or sulfonate groups have been introduced by sulfonating processing with a sulfonating agent containing less than 3 wt % of moisture, is contained in a resin to be made flame retardant, so that flame retardant properties will be conferred on the resin flame resistant.
Abstract:
To provide a transparent resin composition having excellent optical characteristics, particularly, excellent optical characteristics under high temperature and high humidity. There is provided a transparent resin composition, including: an aromatic polycarbonate resin; and a water-insoluble organic sulfonic acid and/or a metal salt thereof, in which a content of the water-insoluble organic sulfonic acid and/or the metal salt thereof is 0.01 to 3.0 pts·mass to 100 pts·mass of the aromatic polycarbonate resin, and a dissolved amount of the water-insoluble organic sulfonic acid and/or the metal salt thereof is not more than 0.5 g to 100 g of pure water.
Abstract:
A flame retardant with which fire retardancy is improved and the fire retardancy is able to be secured stably for a long time is provided. An internal layer 11 containing a polymer and a flame retardant factor layer 12 that is formed outside of the internal layer 11 and that contains a polymer to which at least one of a sulfonate group and a sulfonate base is bonded are included. Thereby, compared to a case that the flame retardant factor layer 12 is not included, moisture is hardly absorbed, and respective particles of the flame retardant are inhibited from being adhered to each other. Accordingly, blocking is inhibited.
Abstract:
A flame retardant with which fire retardancy is improved and the fire retardancy is able to be secured stably for a long time is provided. An internal layer 11 containing a polymer and a flame retardant factor layer 12 that is formed outside of the internal layer 11 and that contains a polymer to which at least one of a sulfonate group and a sulfonate base is bonded are included. Thereby, compared to a case that the flame retardant factor layer 12 is not included, moisture is hardly absorbed, and respective particles of the flame retardant are inhibited from being adhered to each other. Accordingly, blocking is inhibited.
Abstract:
To provide a transparent resin composition having excellent optical characteristics, particularly, excellent optical characteristics under high temperature and high humidity.There is provided a transparent resin composition, including: an aromatic polycarbonate resin; and a water-insoluble organic sulfonic acid and/or a metal salt thereof, in which a content of the water-insoluble organic sulfonic acid and/or the metal salt thereof is 0.01 to 3.0 pts·mass to 100 pts·mass of the aromatic polycarbonate resin, and a dissolved amount of the water-insoluble organic sulfonic acid and/or the metal salt thereof is not more than 0.5 g to 100 g of pure water.
Abstract:
A halogen-free type polycarbonate resin composition and a resin molded object having good flame retardant properties and physical properties that make them suitable for the use as manufactured products. The resin component includes a component A which is a polycarbonate resin, a component B including organic sulfonic acid or organic sulfonic acid metal salt, whose content is 0.05% or more and 2.0% or less by weight, a component C which is a drip inhibitor, whose content is 0.05% or more and 1.0% or less by weight, and a component D which is a silicone compound, whose content is 0.1% or more and 2.0% or less by weight. Among hydrogen atoms in the silicone compound and the proportion of hydrogen atoms in phenyl groups is 51% or more.