Abstract:
The invention relates to a catalyst composition comprising (a) a metal M selected from the group consisting of platinum (Pt), palladium (Pd), rhodium (Rh), rhenium (Re), ruthenium (Ru) and iridium (Ir), (b) tin (Sn), (c) zinc (Zn), (d) alkaline earth metal and (e) a porous metal oxide catalyst support, wherein the amount of each of elements (a), (b) and (d) is independently chosen in the range of from 0.1 to 5 wt. % based on the porous metal oxide catalyst support and wherein the amount of element (c) is chosen in the range of from 0.1 to 2 wt. % based on the porous metal oxide catalyst support. Furthermore, the invention also relates to a process for the preparation of said catalyst composition and its use in non-oxidative dehydrogenation of an alkane, preferably propane.
Abstract:
The invention relates to a catalyst composition comprising: (i) a porous metal oxide catalyst support, (ii) a precious metal comprises at least one of platinum (Pt), palladium (Pd), rhodium (Rh), rhenium (Re), ruthenium (Ru) and iridium (Ir), and (iii) tin (Sn), and (iv) zinc (Zn), and/or (v) an alkaline earth metal, wherein the catalyst composition is obtained or obtainable by a process comprising (a) depositing the precious metal, Sn, Zn and/or the alkaline earth metal on the porous metal oxide catalyst support to obtain a catalyst precursor and (b) subjecting the catalyst precursor to calcination in an environment comprising oxygen to obtain a catalyst, wherein step (a) comprises the step of (a1) contacting the porous metal oxide catalyst support with a solution comprising a salt of the precious metal and a salt of tin (Sn) and a salt of zinc (Zn) and/or a salt of the alkaline earth metal.
Abstract:
The invention relates to a catalyst composition comprising (a) a metal M selected from the group consisting of platinum (Pt), palladium (Pd), rhodium (Rh), rhenium (Re), ruthenium (Ru) and iridium (Ir), (b) tin (Sn), (c) zinc (Zn), (d) alkaline earth metal and (e) a porous metal oxide catalyst support, wherein the amount of each of elements (a), (b) and (d) is independently chosen in the range of from 0.1 to 5 wt. % based on the porous metal oxide catalyst support and wherein the amount of element (c) is chosen in the range of from 0.1 to 2 wt. % based on the porous metal oxide catalyst support. Furthermore, the invention also relates to a process for the preparation of said catalyst composition and its use in non-oxidative dehydrogenation of an alkane, preferably propane.