公开(公告)号:US4497668A
公开(公告)日:1985-02-05
申请号:US554879
申请日:1983-11-25
申请人: Raschad Mady , Winand Hanelt , Roland Morlock , Dieter Geruhn , Lutz Leyhe , Jobst H. Meyer zu Bexten , Franz Ricke
发明人: Raschad Mady , Winand Hanelt , Roland Morlock , Dieter Geruhn , Lutz Leyhe , Jobst H. Meyer zu Bexten , Franz Ricke
摘要: A process for phosphating zinc-plated metal articles, particularly electrolytically zinc-plated steel sheets, by treatment thereof for a short period with an acidic phosphating solution which, in addition to zinc and phosphate ions, can contain other metal cations and/or anions of oxygen-containing acids having an accelerating effect, wherein the phosphating solution has a content of Zn.sup.2+ -cations of between about 1 and 2.5 g/l, a free acid content in the range from 0.8 to 3 points, and the acid ratio of total acid to free acid in the range from 5 to 10. The phosphating treatment is carried out for a period of time not in excess of about 5 seconds.
摘要翻译: 一种通过用酸性磷酸盐溶液处理短时间的镀锌金属制品,特别是电解镀锌钢板的方法,除了锌和磷酸根离子之外,还可以含有其它金属阳离子和/或阴离子 具有促进作用的含氧酸,其中磷酸盐化合物的Zn 2+离子含量在约1至2.5g / l之间,游离酸含量在0.8至3个点之间,而酸的酸的比例 游离酸在5至10的范围内。磷化处理进行不超过约5秒的时间。
-
公开(公告)号:US5516372A
公开(公告)日:1996-05-14
申请号:US387931
申请日:1995-04-27
申请人: Joerg Riesop , Raschad Mady , Dieter Geruhn , Frank Panter , Franz Ricke , Hubertus Peters , Juergen Verheien , Manfred Wessel
发明人: Joerg Riesop , Raschad Mady , Dieter Geruhn , Frank Panter , Franz Ricke , Hubertus Peters , Juergen Verheien , Manfred Wessel
CPC分类号: C23C22/362 , C23C22/12 , C23C22/184
摘要: A process for phosphating a galvanized surface of a steel strip electrolytically galvanized on one side by contacting the galvanized surface of the steel strip with a phosphating solution containing 1.0 to 6 g/l zinc, 0.5 to 5.0 g/l nickel and 14 to 25 g/l phosphate at a temperature of 40.degree. to 70.degree. C. for from 2 to 20 seconds. The ungalvanized surface remains metal bright.
摘要翻译: PCT No.PCT / EP93 / 02205 Sec。 371日期:1995年04月27日 102(e)日期1995年4月27日PCT 1993年8月18日PCT公布。 出版物WO94 / 05826 日期:1994年3月17日。一种通过使钢带的镀锌表面与含有1.0〜6g / l的锌,0.5〜5.0g / l的磷酸盐化溶液接触的方式使一面电解镀锌钢带的镀锌表面磷化, l镍和14至25g / l磷酸盐,温度为40至70℃,持续2至20秒。 未镀锌的表面保持金属光亮。
-