1.
公开(公告)号:US4398980A
公开(公告)日:1983-08-16
申请号:US286422
申请日:1981-07-24
CPC分类号: C04B37/021 , B23K35/38 , G01N27/07 , C04B2235/656 , C04B2235/6567 , C04B2235/6582 , C04B2237/32 , C04B2237/34 , C04B2237/341 , C04B2237/403 , C04B2237/405 , C04B2237/525 , C04B2237/54 , Y10S228/903
摘要: A method of fabricating a seal between a ceramic and an alloy comprising the steps of prefiring the alloy in an atmosphere with a very low partial pressure of oxygen, firing the assembled alloy and ceramic in air, and gradually cooling the fired assembly to avoid the formation of thermal stress in the ceramic. The method forms a bond between the alloy and the ceramic capable of withstanding the environment of a pressurized water reactor and suitable for use in an electrical conductivity sensitive liquid level transducer.
摘要翻译: 一种在陶瓷和合金之间制造密封的方法,包括以下步骤:在具有非常低的氧分压的气氛中预烧合金,在空气中烧结组合的合金和陶瓷,并逐渐冷却烧制的组件以避免形成 的陶瓷中的热应力。 该方法在合金和能够耐受压水反应器的环境的陶瓷之间形成粘结,并适用于导电敏感液位传感器。