Abstract:
A process for the production of sodium perborate monohydrate having an increased resistance to abrasion wherein sodium perborate tetrahydrate is treated with hot air having a relative humidity between 40 and 80%. The temperature of the moist air discharged from the dryer is maintained between 60* and 90*C.