Abstract:
A method of producing a roll of a continuous web of an optical film laminate, usable in a process of laminating an optical film sheet including a polarizing film and formed to a size corresponding to that an optical panel to a surface of the optical panel being fed to a lamination position, is disclosed. The polarizing film is prepared by subjecting a laminate including a thermoplastic resin substrate and a PVA type resin layer formed on the substrate, to uniaxial 2-stage stretching to reduce a thickness of the PVA type resin layer to 10 μm or less, and causing a dichroic material to be absorbed in the PVA type resin layer. A carrier film is releasably attached to the continuous web of optical film laminate including the polarizing film, through an adhesive layer. A defect inspection is performed for the optical film laminate and the adhesive layer.
Abstract:
A method of producing a roll of an optical film laminate strip including a polarizing film includes the steps of: forming a continuous web of optical film laminate including a polarizing film which consists of a polyvinyl alcohol type resin layer and has a thickness of 10 μm or less, wherein the polarizing film is formed by performing an stretching sub-step of subjecting a laminate comprising a continuous web of thermoplastic resin substrate and a polyvinyl alcohol type resin layer formed on the substrate, to a uniaxial stretching in a lengthwise direction of the laminate based on 2-stage stretching consisting of preliminary in-air stretching and in-boric-acid-solution stretching; cutting the continuous web of optical film laminate along a direction parallel to the length direction to form at least one continuous web of laminate strip having a given width; and winding the continuous web of laminate strip having the given width into a roll.
Abstract:
Disclosed is a method of producing a roll of an optical film laminate strip including a polarizing film which has a thickness of 10 μm or less. The method comprises the steps of: forming a continuous web of optical film laminate including a polarizing film which consists of a polyvinyl alcohol type resin layer and has a thickness of 10 μm or less, wherein the polarizing film is formed by performing an stretching sub-step of subjecting a laminate comprising a continuous web of thermoplastic resin substrate and a polyvinyl alcohol type resin layer formed on the substrate, to a uniaxial stretching in a lengthwise direction of the laminate based on 2-stage stretching consisting of preliminary in-air stretching and in-boric-acid-solution stretching, to attain a stretching ratio of 5 to 8.5 to thereby reduce a thickness of the polyvinyl alcohol type resin layer to 10 μm or less, and an absorption sub-step of causing a dichroic material to be absorbed in the polyvinyl alcohol type resin layer; cutting the continuous web of optical film laminate along a direction parallel to the length direction to form at least one continuous web of laminate strip having a given width; and winding the continuous web of laminate strip having the given width into a roll.
Abstract:
A method of producing an optical panel assembly including the polarizing film in a continuous manner by laminating a polarizing film to a surface of a rectangular-shaped optical panel, is disclosed. The polarizing film is formed by performing a step of subjecting a laminate including a continuous web of a thermoplastic resin substrate and a PVA type resin layer formed on the substrate, to a 2-stage stretching consisting of a preliminary in-air stretching and an in-boric-acid-solution stretching, to reduce a thickness of the PVA type resin layer to 10 μm or less, and a step of causing a dichroic material to be absorbed in the PVA type resin layer.
Abstract:
Provided is an optical display device using a polarizing film which has a thickness of 10 μm or less and exhibits high optical characteristics. The optical display device comprises a continuous web of polarizing film which is made of a polyvinyl alcohol type resin having a molecularly oriented dichroic material, and formed through stretching to have a thickness of 10 μm or less and satisfy conditions expressed by the following formulas: P>−(100.929T-42.4−1)×100 (where T