1.
公开(公告)号:US20240375336A1
公开(公告)日:2024-11-14
申请号:US18580699
申请日:2022-07-20
Applicant: NITTO DENKO CORPORATION
Inventor: Tatsuya Araki , Kenichiro Nishiwaki , Sho Irie , Yasuharu Imamura
IPC: B29C48/21 , B29C48/05 , B29C48/285 , B29L11/00
Abstract: A method is disclosed for manufacturing a plastic optical fiber composed of a plurality of layers including a core and a cladding, which includes forming at least one layer formed of the plurality of layers by melt extrusion molding of a material resin using a melt extrusion unit including an extrusion screw, wherein a pellet of the material resin is fed to the melt extrusion unit, and a relation expressed by the following inequality (I) is satisfied by a flight height Hf (mm) of the extrusion screw in a feed zone Lf of the melt extrusion unit and a maximum dimension Lmax (mm) of the pellet to be fed: 0≤Hf−Lmax≤3 (I); and a volume V (mm3) of the pellet satisfies the following inequality (II): 4
-
2.
公开(公告)号:US20230226737A1
公开(公告)日:2023-07-20
申请号:US17928507
申请日:2021-05-28
Applicant: NITTO DENKO CORPORATION
Inventor: Kenjiro Saomoto , Shinsuke Sugiura , Yasuaki Okada , Sho Irie
CPC classification number: B29C48/29 , B29C43/32 , B29C43/36 , B29C48/022 , B29C2043/3205 , B29C2043/3233 , B29K2096/00
Abstract: An optical resin formed body manufacturing method includes: (i) depressurizing an inside of a container holding a molten optical resin; (ii) pressurizing the inside of the container holding the molten optical resin; and (iii) shaping the optical resin taken out of the container into a given shape. The steps (i) and (ii) are sequentially performed once each or are alternately performed two or more times each. In the step (i), a duration t1 [min] of the depressurization of the inside of the container is set such that the duration t1 and a viscosity µ1 [Pa•s] of the molten optical resin satisfy a relation µ1/t1
-