公开(公告)号:US11898216B2
公开(公告)日:2024-02-13
申请号:US16981435
申请日:2019-03-26
发明人: Hiroki Kamitani , Takanori Tanaka , Atsushi Soma , Keiichi Kondo , Hideki Mitsunari , Seiya Okada , Takuya Matsumoto , Shinji Yoshida , Yuji Arai
摘要: A seamless steel pipe heat-treatment-finishing-treatment continuous facility includes: a heat treatment apparatus; a steel pipe inspection apparatus which performs a test for a surface defect and/or an inner defect of the seamless steel pipe, the steel pipe inspection apparatus being disposed downstream of the heat treatment apparatus; a main transfer mechanism which forms a main transfer path MT for transferring the seamless steel pipe, discharged from the heat treatment apparatus, to the steel pipe inspection apparatus disposed downstream of the heat treatment apparatus; and a first forced steel pipe-temperature reduction apparatus which forcibly reduces a temperature of the seamless steel pipe on the main transfer path MT, the first forced steel pipe-temperature reduction apparatus being disposed on the main transfer path MT at a position downstream of the heat treatment apparatus and upstream of the steel pipe inspection apparatus.
-
公开(公告)号:US11078558B2
公开(公告)日:2021-08-03
申请号:US16339577
申请日:2017-10-06
发明人: Yuji Arai , Shinji Yoshida , Atsushi Soma , Hiroki Kamitani
IPC分类号: C22C38/42 , C21D7/13 , C21D9/08 , C22C38/00 , C22C38/02 , C22C38/04 , C22C38/06 , C22C38/44 , C22C38/46 , C22C38/48 , C22C38/50 , C22C38/52 , C22C38/54 , C21D1/18
摘要: The steel material according to the present invention contains a chemical composition consisting of, in mass %, C: 0.25 to 0.50%, Si: 0.05 to 0.50%, Mn: 0.05 to 1.00%, P: 0.025% or less, S: 0.0100% or less, Al: 0.005 to 0.100%, Cr: 0.30 to 1.50%, Mo: 0.25 to 1.50%, Ti: 0.002 to 0.050%, B: 0.0001 to 0.0050%, N: 0.002 to 0.010% and O: 0.0100% or less, with the balance being Fe and impurities. The steel material also contains an amount of dissolved C within a range of 0.010 to 0.050 mass%. The steel material also contains an yield strength is in a range of 862 to less than 965 MPa, and an yield ratio is 90% or more.
-
公开(公告)号:US11492688B2
公开(公告)日:2022-11-08
申请号:US17253229
申请日:2019-09-26
发明人: Shinji Yoshida , Yuji Arai
IPC分类号: C22C38/32 , C22C38/00 , C22C38/02 , C22C38/04 , C22C38/06 , C22C38/22 , C22C38/28 , C21D8/10
摘要: The steel material according to the present disclosure has a chemical composition consisting of, in mass %, C: 0.20 to 0.35%, Si: 0.05 to 1.00%, Mn: 0.01 to 1.00%, P: 0.025% or less, S: 0.0100% or less, Al: 0.005 to 0.100%, Cr 0.25 to 0.80%, Mo: 0.20 to 2.00%, Ti: 0.002 to 0.050%, B: 0.0001 to 0.0050%, N: 0.0020 to 0.0100% and O: 0.0100% or less, with the balance being Fe and impurities, and satisfying Formula (1). A number density of precipitates having an equivalent circular diameter of 400 nm or more is 0.150 particles/μm2 or less. The yield strength is within a range of 655 to 965 MPa. A dislocation density ρ is 7.0×1014 m−2 or less. 5×Cr—Mo-2×(V+Ti)≤3.00 (1)
-
公开(公告)号:US11434554B2
公开(公告)日:2022-09-06
申请号:US17044616
申请日:2019-03-22
发明人: Hiroki Kamitani , Atsushi Soma , Keiichi Kondo , Shinji Yoshida , Yuji Arai
摘要: The steel material according to the present disclosure contains a chemical composition consisting of, in mass %, C: 0.20 to 0.50%, Si: 0.05 to 0.50%, Mn: 0.05 to 1.00%, P: 0.030% or less, S: less than 0.0050%, Al: 0.005 to 0.050%, Cr: 0.10 to 1.50%, Mo: 0.25 to 1.80%, Ti: 0.002 to 0.050%, Nb: 0.002 to 0.100%, B: 0.0001 to 0.0050%, N: 0.0070% or less and O: less than 0.0050% with the balance being Fe and impurities. A yield strength is within a range of 655 to 1069 MPa, and a yield ratio is 85% or more. A proportion of KAM values of 1° or less is 30 area % or more.
-
公开(公告)号:US11174539B2
公开(公告)日:2021-11-16
申请号:US16980671
申请日:2019-03-25
发明人: Hiroki Kamitani , Atsushi Soma , Shinji Yoshida , Yuji Arai , Seiya Okada
IPC分类号: C22C38/00 , C22C38/54 , C22C38/02 , C22C38/04 , C22C38/06 , C22C38/22 , C22C38/42 , C22C38/46 , C22C38/48 , C22C38/50 , C22C38/52
摘要: The steel material according to the present disclosure contains a chemical composition consisting of, in mass %, C: 0.20 to 0.50%, Si: 0.05 to 0.50%, Mn: 0.05 to 1.00%, P: 0.030% or less, S: 0.0100% or less, Al: 0.005 to 0.100%, Cr: 0.10 to 1.50%, Mo: 0.25 to 1.50%, Ti: 0.002 to 0.050%, N: 0.0100% or less and O: 0.0100% or less, with the balance being Fe and impurities. The steel material contains an amount of dissolved C within a range of 0.010 to 0.050 mass %. The steel material also has a yield strength within a range of 655 to less than 862 MPa, and a yield ratio of the steel material is 85% or more.
-
公开(公告)号:US11473177B2
公开(公告)日:2022-10-18
申请号:US16975318
申请日:2019-02-26
发明人: Shinji Yoshida , Yuji Arai
IPC分类号: C22C38/14 , C22C38/02 , C22C38/04 , C22C38/20 , C22C38/32 , C22C38/28 , C22C38/24 , C21D9/08
摘要: The steel material according to the present disclosure has a chemical composition consisting of, in mass %, C: 0.10 to 0.60%, Si: 0.05 to 1.00%, Mn: 0.05 to 1.00%, P: 0.025% or less, S: 0.0100% or less, Al: 0.005 to 0.100%, Cr: 0.20 to 1.50%, Mo: 0.25 to 1.50%, V: 0.01 to 0.60%, Ti: 0.002 to 0.050%, B: 0.0001 to 0.0050%, N: 0.0020 to 0.0100%, and O: 0.0100% or less, with the balance being Fe and impurities. A dislocation density ρ is 3.5×1015 m−2 or less. Among fine precipitates, the numerical proportion of precipitates for which a ratio of the Mo content is not more than 50% is 15% or more. The yield strength is in a range of 655 to 1172 MPa.
-
公开(公告)号:US11332813B2
公开(公告)日:2022-05-17
申请号:US17043096
申请日:2019-03-22
发明人: Shinji Yoshida , Yuji Arai , Atsushi Soma , Hiroki Kamitani
IPC分类号: C22C38/02 , C22C38/04 , C22C38/06 , C22C38/22 , C22C38/32 , C21D1/18 , C21D6/00 , C21D8/02 , C21D9/46 , C22C38/00 , C22C38/20 , C22C38/24 , C22C38/26 , C22C38/28 , C22C38/30
摘要: The steel material according to the present disclosure contains a chemical composition consisting of, in mass %, C: more than 0.50 to 0.80%, Si: 0.05 to 1.00%, Mn: 0.05 to 1.00%, P: 0.025% or less, S: 0.0100% or less, Al: 0.005 to 0.100%, Cr: 0.20 to 1.50%, Mo: 0.25 to 1.50%, Ti: 0.002 to 0.050%, B: 0.0001 to 0.0050%, N: 0.0100% or less and O: 0.0100% or less, with the balance being Fe and impurities. The steel material contains an amount of dissolved C within a range of 0.010 to 0.060 mass %. The steel material also has a yield strength within a range of 862 to less than 965 MPa, and a yield ratio of the steel material is 90% or more.
-
公开(公告)号:US12054798B2
公开(公告)日:2024-08-06
申请号:US17265614
申请日:2019-10-16
发明人: Yuji Arai , Shinji Yoshida , Hiroki Kamitani , Yohei Otome
CPC分类号: C21D8/105 , C21D6/004 , C21D6/005 , C21D6/007 , C21D6/008 , C21D9/085 , C22C38/001 , C22C38/44 , C22C38/46 , C22C38/54
摘要: The steel material according to the present disclosure has a chemical composition consisting of, in mass %, C: 0.15 to 0.45%, Si: 0.05 to 1.00%, Mn: 0.01 to 1.00%, P: 0.030% or less, S: 0.0050% or less, Al: 0.005 to 0.100%, Cr 0.60 to 1.80%, Mo: 0.80 to 2.30%, Ti: 0.002 to 0.020%, V: 0.05 to 0.30%, Nb: 0.002 to 0.100%, B: 0.0005 to 0.0040%, Cu: 0.01 to 0.50%, Ni: 0.01 to 0.50%, N: 0.0020 to 0.0100% and O: 0.0020% or less, with the balance being Fe and impurities. The number density of BN in the steel material is 10 to 100 particles/100 μm2. The yield strength of the steel material is 758 MPa or more.
-
公开(公告)号:US11905580B2
公开(公告)日:2024-02-20
申请号:US17259651
申请日:2019-09-26
发明人: Hiroki Kamitani , Nobuaki Komatsubara , Seiya Okada , Atsushi Soma , Yuji Arai , Shinji Yoshida
IPC分类号: C22C38/32 , C21D9/08 , C22C38/00 , C22C38/02 , C22C38/04 , C22C38/06 , C22C38/26 , C22C38/28
CPC分类号: C22C38/32 , C21D9/085 , C22C38/002 , C22C38/02 , C22C38/04 , C22C38/06 , C22C38/26 , C22C38/28
摘要: The seamless steel pipe according to the present disclosure has a chemical composition consisting of, in mass %, C: 0.15 to 0.45%, Si: 0.05 to 1.00%, Mn: 0.01 to 1.00%, P: 0.030% or less, S: 0.0050% or less, Al: 0.005 to 0.070%, Cr: 0.30 to 1.50%, Mo: 0.25 to 2.00%, Ti: 0.002 to 0.020%, Nb: 0.002 to 0.100%, B: 0.0005 to 0.0040%, rare earth metal: 0.0001 to 0.0015%, Ca: 0.0001 to 0.0100%, N: 0.0100% or less and O: 0.0020% or less, with the balance being Fe and impurities, and satisfying Formula (1) described in the description. A predicted maximum major axis of inclusions is 150 μm or less, the predicted maximum major axis being predicted by means of extreme value statistical processing. The yield strength is within a range of 758 to 862 MPa.
-
公开(公告)号:US11773460B2
公开(公告)日:2023-10-03
申请号:US17044601
申请日:2019-03-22
发明人: Yuji Arai , Shinji Yoshida , Atsushi Soma , Hiroki Kamitani
IPC分类号: C21D9/00 , C21D6/04 , C21D6/00 , C22C38/00 , C21D9/08 , C21D8/10 , C22C38/02 , C22C38/04 , C22C38/06 , C22C38/30 , C22C38/42 , C22C38/44 , C22C38/46 , C22C38/48 , C22C38/50 , C22C38/54
CPC分类号: C21D9/085 , C21D6/004 , C21D6/005 , C21D6/007 , C21D6/008 , C21D8/105 , C22C38/001 , C22C38/002 , C22C38/02 , C22C38/04 , C22C38/06 , C22C38/30 , C22C38/42 , C22C38/44 , C22C38/46 , C22C38/48 , C22C38/50 , C22C38/54
摘要: The steel pipe according to the present disclosure contains a chemical composition consisting of, in mass %, C: 0.25 to 0.50%, Si: 0.05 to 0.50%, Mn: 0.05 to 1.00%, P: 0.025% or less, S: 0.0050% or less, Al: 0.005 to 0.100%, Cr: 0.30 to 1.50%, Mo: 0.25 to 3.00%, Ti: 0.002 to 0.050%, N: 0.0010 to 0.0100% and O: 0.0030% or less, with the balance being Fe and impurities. The steel pipe contains an amount of dissolved C within a range of 0.010 to 0.050 mass %. The tensile yield strength in the axial direction and the circumferential direction is 862 to 965 MPa, and the yield ratio in the axial direction is 90% or more. The tensile yield strength in the circumferential direction is 30 to 80 MPa higher than the compressive yield strength in the circumferential direction.
-
-
-
-
-
-
-
-
-