Abstract: A method of maintaining an article, e.g. an engine and its components in a potentially explosive environment at a surface temperature above that allowed by safety regulations, e.g. above 200° C. This is achieved by applying a composition comprising: about 9 to about 90% of one or more silicone rubber about 9 to about 90% of one or more fluorosilicone rubber about 0.05 to about 1% of one or more vulcanisation catalyst and about 0 to about 20% of one or more additive to the surface of the article and curing the composition, and maintaining the article in a potentially explosive environment such that the surface temperature of the article is above that allowed by safety regulations but the surface temperature of the coating does not exceed that allowed by safety regulations.
Abstract translation: 一种维持物品的方法,例如, 发动机及其部件处于潜在爆炸性环境中,表面温度高于安全规定允许的表面温度,例如。 这通过施用组合物来实现,所述组合物包含:约9至约90%的一种或多种硅橡胶约9至约90%的一种或多种氟硅橡胶约0.05至约1%的一种或多种硫化催化剂 和约0至约20%的一种或多种添加剂加入到制品的表面并固化组合物,并将制品保持在潜在的爆炸性环境中,使得制品的表面温度高于安全规定允许的表面温度,但表面 涂层的温度不超过安全规定允许的温度。