METHOD OF SYNTHESIZING SILVER NANOPARTICLES
    1.
    发明申请
    METHOD OF SYNTHESIZING SILVER NANOPARTICLES 有权
    合成银纳米粒子的方法

    公开(公告)号:US20160121401A1

    公开(公告)日:2016-05-05

    申请号:US14563494

    申请日:2014-12-08

    CPC classification number: B22F9/24 B22F1/0018 B22F2301/255 C22B11/04 C22C5/06

    Abstract: Provided is a method of synthesizing silver nanoparticles including: a) a nucleation step of reacting a composition containing a silver precursor, a heterogeneous metal precursor, and an amine-based compound at 30 to 120° C. to form a nucleus; and b) a growth step of reacting the composition containing the nucleus formed therein at 155 to 350° C. to grow the nucleus. According to the present invention, significantly uniform and fine silver nanoparticles may be synthesized with high reproducibility on a large scale.

    Abstract translation: 提供一种合成银纳米颗粒的方法,其包括:a)在30〜120℃下使含有银前体,异质金属前体和胺系化合物的组合物反应以形成核的成核步骤; 和b)生长步骤,使含有其中形成的细胞核的组合物在155-350℃下反应以生长细胞核。 根据本发明,可以大规模地以高再现性合成显着均匀且细小的银纳米颗粒。

    PREPARING METHOD OF AG NANO-PARTICLE AND HYDROPHOBIC SPHERICAL AG NANO-PARTICLE PREPARED USING THE SAME
    2.
    发明申请
    PREPARING METHOD OF AG NANO-PARTICLE AND HYDROPHOBIC SPHERICAL AG NANO-PARTICLE PREPARED USING THE SAME 有权
    使用其制备的AG纳米颗粒和疏水性球形AG纳米颗粒的制备方法

    公开(公告)号:US20150132595A1

    公开(公告)日:2015-05-14

    申请号:US14176357

    申请日:2014-02-10

    CPC classification number: C07F1/10 B22F1/0044 B22F1/0048 B22F9/24 Y10T428/12

    Abstract: Provided is a preparing method of an Ag nano-particle for mass-producing Ag nano-particles, the method including: performing a first reaction of a reaction solution containing an Ag precursor and oleylamine at a set first temperature T1; performing a second reaction of the reaction solution at a second temperature T2 set so as to be higher than the first temperature; and obtaining a reactant from the reaction solution, wherein at least one of the first and second reactions is performed in a state in which the reaction solution is not stirred.

    Abstract translation: 本发明提供一种用于大量生产Ag纳米颗粒的Ag纳米颗粒的制备方法,该方法包括:在设定的第一温度T1下进行含有Ag前体和油胺的反应溶液的第一次反应; 在设定为高于第一温度的第二温度T2下进行反应溶液的第二反应; 从所述反应溶液中获得反应物,其中所述第一反应和所述第二反应中的至少一个在所述反应溶液不被搅拌的状态下进行。