INFRARED SHIELDING FILM
    2.
    发明申请
    INFRARED SHIELDING FILM 审中-公开
    红外屏蔽膜

    公开(公告)号:US20150177433A1

    公开(公告)日:2015-06-25

    申请号:US14413359

    申请日:2013-07-08

    IPC分类号: G02B5/28 G02B1/14

    摘要: [Problem] To provide a an infrared shielding film which realizes a balance between the hard coating properties of the cured resin layer and the suppression of peeling or cracking of the film, while having heat shielding characteristics of an infrared shielding film.[Solution] An infrared shielding film including a substrate; an infrared reflecting layer having at least one or more low refractive index layers and at least one or more high refractive index layers laminated therein; and a cured resin layer formed at the outermost surface, laminated together, the cured resin layer containing inorganic nanoparticles, in which the hardness obtainable by the pencil hardness test described in JIS K5600-5-4:1999 is from 2B to 3H; the number of scratches obtainable by a steel wool test (load 500 g/cm2, 10 reciprocations) is 15 or less; and the mandrel diameter at which the hard coated surface begins to crack in the bending test described in JIS K5600-5-1:1999 (cylindrical mandrel method) is 15 mm or less.

    摘要翻译: [问题]提供一种红外线屏蔽膜,其实现了固化树脂层的硬涂层性能与抑制膜的剥离或破裂之间的平衡,同时具有红外屏蔽膜的隔热特性。 [解决方案]一种包括基板的红外屏蔽膜; 具有至少一个或多个低折射率层和层压在其中的至少一个或多个高折射率层的红外反射层; 和在最外层形成的固化树脂层,层叠在一起,含有无机纳米粒子的固化树脂层,其中通过JIS K5600-5-4:1999中所述的铅笔硬度试验得到的硬度为2B〜3H; 通过钢丝绒试验(载荷500g / cm 2,10次往复运动)可获得的划痕数为15个以下; 在JIS K5600-5-1:1999(圆筒型心轴法)所示的弯曲试验中硬质表面开始裂纹的心轴直径为15mm以下。

    FUNCTIONAL FILM AND METHOD OF MANUFACTURING FUNCTIONAL FILM
    3.
    发明申请
    FUNCTIONAL FILM AND METHOD OF MANUFACTURING FUNCTIONAL FILM 审中-公开
    功能膜和制造功能膜的方法

    公开(公告)号:US20150124314A1

    公开(公告)日:2015-05-07

    申请号:US14404934

    申请日:2013-05-30

    IPC分类号: G02B1/14 G02B5/20 G02B5/08

    摘要: In a case where a functional film that includes an acrylic layer 7, an intermediate layer 8, and a protection layer 9 adjacent to one another on a resin substrate 3, and has the protection layer 9 on its outermost surface is manufactured, the protection layer 9 contains at least a polysiloxane compound, and the intermediate layer 8 contains at least one of the following materials: polyvinyl alcohol resin, polyvinyl acetate, cellulose, and water glass. With this structure, interlayer coupling between the acrylic layer 7 and the intermediate layer 8, and interlayer coupling between the intermediate layer 8 and the protection layer 9 can be strengthened, and detachment of each of the acrylic layer 7, the intermediate layer 8, and the protection layer 9 can be reduced. Accordingly, a functional film that is highly resistant to damage can be obtained.

    摘要翻译: 在树脂基板3上包含丙烯酸酯层7,中间层8和保护层9相邻并在其最外面具有保护层9的功能膜的情况下,制作保护层 9含有至少一种聚硅氧烷化合物,并且中间层8含有以下材料中的至少一种:聚乙烯醇树脂,聚乙酸乙烯酯,纤维素和水玻璃。 通过这种结构,可以加强丙烯酸层7和中间层8之间的层间耦合以及中间层8和保护层9之间的层间结合,并且可以使丙烯酸层7,中间层8和 可以减小保护层9。 因此,可以获得高度耐损伤的功能膜。