Abstract:
Provided is a method of preparing cellulose fiber and carbon fiber by recycling industrial wood waste, wherein the carbon fiber is prepared by preparing high purity cellulose pulp by using, as a raw material, wood waste generated by manufacturers of pulp, furniture and other industrial products from wood and by eliminating resin and lignin impregnated in the wood waste through pulping and bleaching of the raw material, by preparing cellulose fiber by directly dissolving the prepared pulp in a cellulose solvent, and then by performing stabilizing and carbonizing with the cellulose fiber as a precursor.
Abstract:
The present invention relates to a method for manufacturing carbon composite fibers and carbon nanofibers, and more particularly, to a method for manufacturing carbon composite fiber with greatly improved specific tensile strength, specific modulus, electrical conductivity, and thermal conductivity.
Abstract:
Disclosed are a spinning dope for an aramid and carbon-nanotube composite fiber and a method of manufacturing an aramid and carbon-nanotube composite fiber using the same.
Abstract:
The present disclosure relates to a carbon nanotube fiber having improved physical properties and a method for manufacturing the same. The method according to the present disclosure comprises the steps of: spinning carbon nanotubes with a purity of 90% by weight or more to obtain a first carbon nanotube fiber; and heat-treating the first carbon nanotube fiber at 500 to 3,000° C. under an inert gas atmosphere to obtain a second carbon nanotube fiber, wherein the second carbon nanotube fiber has a density of 1.0 to 2.5 g/cm3.