CATALYTIC COMPOSITION FOR THE ELECTROCHEMICAL REDUCTION OF CARBON DIOXIDE
    8.
    发明申请
    CATALYTIC COMPOSITION FOR THE ELECTROCHEMICAL REDUCTION OF CARBON DIOXIDE 审中-公开
    用于二氧化碳电化学还原的催化组合物

    公开(公告)号:US20140174916A1

    公开(公告)日:2014-06-26

    申请号:US13727515

    申请日:2012-12-26

    Abstract: The catalytic composition for the electrochemical reduction of carbon dioxide is a metal oxide supported by multi-walled carbon nanotubes. The metal oxide may be nickel oxide (NiO) or tin dioxide (SnO2). The metal oxides form 20 wt % of the catalyst. In order to make the catalysts, a metal oxide precursor is first dissolved in deionized water to form a metal oxide precursor solution. The metal oxide precursor solution is then sonicated and the solution is impregnated in a support material composed of multi-walled carbon nanotubes to form a slurry. The slurry is then sonicated to form a homogeneous solid solution. Solids are removed from the homogeneous solid solution and dried in an oven for about 24 hours at a temperature of about 110° C. Drying is then followed by calcination in a tubular furnace under an argon atmosphere for about three hours at a temperature of 450° C.

    Abstract translation: 用于二氧化碳的电化学还原的催化组合物是由多壁碳纳米管支撑的金属氧化物。 金属氧化物可以是氧化镍(NiO)或二氧化锡(SnO 2)。 金属氧化物形成20重量%的催化剂。 为了制备催化剂,首先将金属氧化物前体溶解在去离子水中以形成金属氧化物前体溶液。 然后将金属氧化物前体溶液超声处理,并将溶液浸渍在由多壁碳纳米管组成的载体材料中以形成浆料。 然后将浆液超声处理以形成均匀的固溶体。 将固体从均匀的固溶体中除去,并在烘箱中在约110℃的温度下干燥约24小时。然后在管式炉中在氩气气氛下在450℃的温度下煅烧约3小时 C。

Patent Agency Ranking