Sequential and selective flotation of sulfide ores containing copper and
molybdenum
    1.
    发明授权
    Sequential and selective flotation of sulfide ores containing copper and molybdenum 失效
    含铜和钼的硫化矿石的顺序和选择性浮选

    公开(公告)号:US5078860A

    公开(公告)日:1992-01-07

    申请号:US651315

    申请日:1991-02-06

    CPC classification number: B03D1/06 B03D1/014 B03D1/018 B03D2201/02 B03D2203/02

    Abstract: A sequential flotation process for the separation of components of an ore containing sulfides of copper and molybdenum involves initially effecting selective flotation of the copper component directly from the ore by conditioning the ore with a combination of a source of bisulfite ion and causticized starch to produce a conditioned ore having a pH between approximately 5.2 and 6.2, and thereafter treating the conditioned ore with a collector selected from the group consisting of dialkyl dithiophosphates and alkyl dithiophosphinates.

    Abstract translation: 用于分离含有铜和钼的硫化物的矿石的组分的顺序浮选方法包括首先通过用亚硫酸氢盐源和苛性淀粉源的组合调节矿石来直接从矿石中进行铜成分的选择性浮选,以产生 pH在约5.2和6.2之间的调节矿石,然后用选自二烷基二硫代磷酸酯和二烷基二硫代磷酸烷基酯的收集器处理调节矿石。

    Sequential and selective flotation of sulfide ores
    2.
    发明授权
    Sequential and selective flotation of sulfide ores 失效
    硫化矿石的顺序和选择性浮选

    公开(公告)号:US5074994A

    公开(公告)日:1991-12-24

    申请号:US599620

    申请日:1990-10-18

    Abstract: A sequential flotation process for the separation of components of a sulfide ore selected from the group consisting of copper and lead sulfide containing ores and copper, zinc and lead sulfide containing ores in which the copper component is initially selectively floated directly from said ore by conditioning the ore with a combination of a source of bisulfite ion and causticized starch to produce a conditioned ore having a pH between approximately 5.7 and 6.5, and thereafter treating the conditioned ore with a collector selected from the group consisting of dialkyl dithiophosphates and alkyl dithiophosphinates.

    Abstract translation: 用于分离选自包含铜和硫化铅的矿石和铜,锌和含硫化铅的矿石的组分的顺序浮选方法,其中铜组分最初选择性地通过调节所述矿石选择性地浮选 矿石与亚硫酸氢盐源和苛性淀粉源的组合,以产生pH在约5.7和6.5之间的调节矿石,然后用选自二烷基二硫代磷酸盐和烷基二硫代磷酸盐的收集器处理调节矿石。