公开(公告)号:US08574518B2
公开(公告)日:2013-11-05
申请号:US13203337
申请日:2010-02-19
申请人: Gunnar Buehler , Kilian Schwarz
发明人: Gunnar Buehler , Kilian Schwarz
CPC分类号: C01B25/375 , B82Y30/00 , C01P2004/62 , C01P2004/64 , C01P2006/10 , C01P2006/80 , H01M4/5825
摘要: A process for the production of iron (III) orthophosphate of the general formula FePO4×nH2O (n≦2.5) comprising: a) producing an aqueous solution containing Fe2+ ions by introducing, iron (II), iron (III) or mixed iron (II, III) compounds selected from hydroxides, oxides, oxide hydroxides, oxide hydrates, carbonates and hydroxide carbonates, together with elementary iron, into a phosphoric acid-bearing aqueous medium, to dissolve Fe2+ ions and to react Fe3+ with elementary Fe in a comproportionation reaction to give Fe2+; b) separating solids from the phosphoric-acid aqueous Fe2+ solution, and c) adding an oxidation agent to the phosphoric-acid aqueous Fe2+ solution to oxidize iron (II) in the solution to precipitate iron (III) orthophosphate of the general formula FePO4×nH2O. The invention includes the product of the process and its use to make LiFePO4 for batteries.
摘要翻译: 一种制备通式FePO4×nH2O(n@2.5)的正磷酸铁(III)的方法,包括:a)通过引入铁(II),铁(III)或混合铁(),制备含有Fe 2+离子的水溶液 II,III)选自氢氧化物,氧化物,氧化物氢氧化物,氧化物水合物,碳酸盐和氢氧化物碳酸盐的化合物与元素铁一起转化成含磷酸的水性介质,以溶解Fe 2+离子并使Fe 3+与基本的Fe反应在比例 反应得到Fe2 +; b)从磷酸Fe2 +水溶液中分离固体,和c)向磷酸水溶液中加入氧化剂以氧化溶液中的铁(II),以沉淀出通式FePO4的正磷酸铁(Ⅲ)× nH2O。 本发明包括该方法的产物及其制备用于电池的LiFePO 4的用途。
-
公开(公告)号:US08609056B2
公开(公告)日:2013-12-17
申请号:US12680366
申请日:2008-10-06
CPC分类号: H01M4/5825 , C01B25/375 , C01B25/45 , C01P2002/30 , C01P2002/72 , C01P2004/03 , C01P2004/20 , C01P2004/62 , C01P2006/11 , C01P2006/80 , H01M10/0525 , Y10T428/2982
摘要: Iron(III) orthophosphate of the general formula FePO4×nH2O (n≦2.5), prepared by a process in which iron(II)-, iron(III)- or mixed iron(II, III) compounds selected from among hydroxides, oxides, oxidehydroxides, oxide hydrates, carbonates and hydroxidecarbonates are reacted with phosphoric acid having a concentration in the range from 5% to 50%, any iron(II) present after the reaction is converted into iron(III) by addition of an oxidant and solid iron(III) orthophosphate is separated off from the reaction mixture.
摘要翻译: 通过选自氢氧化物中的铁(II) - ,铁(III)或混合铁(II,III)化合物,氧化物的方法制备的通式为FePO 4×nH 2 O(n 2+)的正磷酸铁(III) ,氧化物氢氧化物,氧化物水合物,碳酸盐和羟基碳酸盐与浓度为5%至50%的磷酸反应,通过加入氧化剂和固体将反应中的任何铁(II)转化成铁(III) 从反应混合物中分离正磷酸铁(III)。
-
公开(公告)号:US20110117003A1
公开(公告)日:2011-05-19
申请号:US12680366
申请日:2008-10-06
CPC分类号: H01M4/5825 , C01B25/375 , C01B25/45 , C01P2002/30 , C01P2002/72 , C01P2004/03 , C01P2004/20 , C01P2004/62 , C01P2006/11 , C01P2006/80 , H01M10/0525 , Y10T428/2982
摘要: Iron(III) orthophosphate of the general formula FePO4×nH2O (n≦2.5), prepared by a process in which iron(II)-, iron(III)- or mixed iron(II, III) compounds selected from among hydroxides, oxides, oxidehydroxides, oxide hydrates, carbonates and hydroxidecarbonates are reacted with phosphoric acid having a concentration in the range from 5% to 50%, any iron(II) present after the reaction is converted into iron(III) by addition of an oxidant and solid iron(III) orthophosphate is separated off from the reaction mixture.
摘要翻译: 通过选自氢氧化物中的铁(II) - ,铁(III)或混合铁(II,III)化合物的方法制备的通式为FePO 4·nH 2 O(n≦̸ 2.5)的正磷酸铁(III) ,氧化物氢氧化物,氧化物水合物,碳酸盐和羟基碳酸盐与浓度为5%至50%的磷酸反应,通过加入氧化剂和固体将反应中的任何铁(II)转化成铁(III) 从反应混合物中分离正磷酸铁(III)。
-
公开(公告)号:US20100140571A1
公开(公告)日:2010-06-10
申请号:US12310087
申请日:2007-07-23
申请人: Gerhard Scheuer , Joachim Markmann , Gunnar Buehler , Hans-Dieter Naegerl , Thomas Futterer , Ruediger Wissemborski
发明人: Gerhard Scheuer , Joachim Markmann , Gunnar Buehler , Hans-Dieter Naegerl , Thomas Futterer , Ruediger Wissemborski
IPC分类号: G02B5/23
CPC分类号: B41M5/267 , C08K5/0041 , C08L83/04
摘要: There is provided a laser-writable molding material containing A) at least one polymer material or at least one precursor compound which can be polymerised to give a polymer material, and B) a particulate salt-like compound or a mixture of particulate salt-like compounds, which under the influence of laser light changes its color or leads to a color change in the component A). In order to enlarge the range of matrix materials hitherto available for laser writing and to overcome the disadvantages of the previously used writing procedures for such matrix materials, the laser-writable molding material according to the invention is characterised in that the at least one polymer material of the component A) is selected from polymer compounds having siloxane crosslinking units.
摘要翻译: 提供了一种激光可写成型材料,其包含A)至少一种聚合物材料或至少一种可聚合以得到聚合物材料的前体化合物,和B)颗粒状盐状化合物或颗粒状盐状混合物 化合物,其在激光的影响下改变其颜色或导致组分A)中的颜色变化。 为了扩大迄今为止可用于激光写入的基质材料的范围,并克服了以前用于这种基质材料的书写过程的缺点,根据本发明的激光可写成型材料的特征在于,至少一种聚合物材料 的组分A)选自具有硅氧烷交联单元的聚合物化合物。
-
公开(公告)号:US09437868B2
公开(公告)日:2016-09-06
申请号:US13981369
申请日:2012-01-23
IPC分类号: H01M4/36 , B82Y30/00 , C01B25/37 , H01M4/131 , H01M4/1391 , H01M4/58 , H01M4/62 , H01M10/0525 , C01B25/45
CPC分类号: H01M4/364 , B82Y30/00 , C01B25/375 , C01B25/45 , C01P2002/72 , C01P2002/85 , C01P2004/03 , C01P2004/62 , C01P2004/64 , C01P2006/12 , C01P2006/40 , H01M4/131 , H01M4/1391 , H01M4/5825 , H01M4/625 , H01M10/0525 , Y02E60/122 , Y02P70/54
摘要: A method for producing an iron(III)orthophosphate-carbon composite which contains iron(III)orthophosphate of the general formula FePO4×nH2O (n≦2.5), a carbon source being dispersed in a phosphoric aqueous Fe2+ ion-containing solution and orthophosphate-carbon composite being precipitated and removed from the aqueous solution when an oxidant is added to the dispersion.
摘要翻译: 一种含有FePO 4·nH 2 O(n≤2.5)的正磷酸铁(Ⅲ)的正磷酸铁 - 铁复合物的制造方法,将碳源分散在含磷酸的含Fe 2+离子的溶液中, 当向分散体中加入氧化剂时,碳水化合物被沉淀并从水溶液中除去。
-
公开(公告)号:US20140145120A1
公开(公告)日:2014-05-29
申请号:US13981369
申请日:2012-01-23
IPC分类号: H01M4/36
CPC分类号: H01M4/364 , B82Y30/00 , C01B25/375 , C01B25/45 , C01P2002/72 , C01P2002/85 , C01P2004/03 , C01P2004/62 , C01P2004/64 , C01P2006/12 , C01P2006/40 , H01M4/131 , H01M4/1391 , H01M4/5825 , H01M4/625 , H01M10/0525 , Y02E60/122 , Y02P70/54
摘要: A method for producing an iron(III)orthophosphate-carbon composite which contains iron(III)orthophosphate of the general formula FePO4×nH2O (n≦2.5), a carbon source being dispersed in a phosphoric aqueous Fe2+ ion-containing solution and orthophosphate-carbon composite being precipitated and removed from the aqueous solution when an oxidant is added to the dispersion.
摘要翻译: 一种含有通式FePO 4·nH 2 O(n≦̸ 2.5)的正磷酸铁(Ⅲ)的正磷酸铁 - 铁复合物的制造方法,将碳源分散在含磷酸的含Fe 2+离子的溶液中, 当向分散体中加入氧化剂时,碳水化合物被沉淀并从水溶液中除去。
-
公开(公告)号:US08293147B2
公开(公告)日:2012-10-23
申请号:US12310087
申请日:2007-07-23
申请人: Gerhard Scheuer , Joachim Markmann , Gunnar Buehler , Hans-Dieter Naegerl , Thomas Futterer , Ruediger Wissemborski
发明人: Gerhard Scheuer , Joachim Markmann , Gunnar Buehler , Hans-Dieter Naegerl , Thomas Futterer , Ruediger Wissemborski
CPC分类号: B41M5/267 , C08K5/0041 , C08L83/04
摘要: A laser-writable molding material containing A) at least one polymer material or at least one precursor compound which can be polymerised to give a polymer material, and B) a particulate salt-like compound or a mixture of particulate salt-like compounds, which under the influence of laser light changes its color or leads to a color change in the component A). In order to enlarge the range of matrix materials hitherto available for laser writing and to overcome the disadvantages of the previously used writing procedures for such matrix materials, the laser-writable molding material according to the invention is characterised in that the at least one polymer material of the component A) is selected from polymer compounds having siloxane crosslinking units.