公开(公告)号:US11765846B2
公开(公告)日:2023-09-19
申请号:US17170147
申请日:2021-02-08
Applicant: CORNING INCORPORATED
Inventor: Jaymin Amin , Joshua Michael Jacobs , Jonathan David Pesansky , Kevin Barry Reiman , Ananthanarayanan Subramanian
CPC classification number: H05K5/03 , B32B7/12 , B32B17/06 , B32B17/10036 , B32B17/1077 , B32B17/10091 , B32B17/10119 , B32B17/10137 , B32B17/10743 , B32B17/10761 , B32B17/10788 , B32B17/10798 , C03C3/093 , C03C21/002 , C03C21/005 , C03C23/007 , H05K5/0017 , B32B2307/584 , B32B2457/20
Abstract: Disclosed are device display screen protectors comprising a first strengthened substrate sized to cover a display screen of an electronic device, the first strengthened substrate having a central tension value in the range greater than 0 MPa and less than 20 MPa, a surface having a Knoop lateral cracking scratch threshold of at least 3 N.
-
公开(公告)号:US20220194844A1
公开(公告)日:2022-06-23
申请号:US16129091
申请日:2018-09-12
Applicant: CORNING INCORPORATED
Inventor: Jaymin Amin , Robert Randall Hancock, JR. , Raymond Chih Chung Hsiao , Yuhui Jin , Aize Li
Abstract: An article that includes: a glass-based substrate comprising a thickness, a primary surface and a compressive stress region that extends from the primary surface to a selected depth; and a textured region defined by the primary surface. The textured region comprises a surface roughness (Ra) of at least 10 nm. The article can also comprise a Knoop Scratch Threshold of at least 9 Newtons (N).
-
公开(公告)号:US20210355027A1
公开(公告)日:2021-11-18
申请号:US17391269
申请日:2021-08-02
Applicant: CORNING INCORPORATED
Inventor: Jaymin Amin , Benedict Osobomen Egboiyi , Jonathan David Pesansky , Kevin Barry Reiman , Rostislav Vatchev Roussev , Brian Paul Strines
Abstract: Chemically strengthened glass articles having at least one deep compressive layer extending from a surface of the article to a depth of compression DOC of at least about 125 μm within the glass article. The compressive stress profile includes a single linear segment or portion extending from the surface to the depth of compression DOC. Alternatively, the compressive stress profile may include an additional portion extending from the surface to a relatively shallow depth and the linear portion extending from the shallow depth to the depth of compression.
-
公开(公告)号:US20210070652A1
公开(公告)日:2021-03-11
申请号:US17015668
申请日:2020-09-09
Applicant: Corning Incorporated
Inventor: Jaymin Amin , Yuhui Jin , Karl William Koch, III , Aize Li , David Lee Weidman
Abstract: A glass article is provided that includes: a glass substrate comprising a thickness and a primary surface; and a textured region defined by the primary surface. The textured region comprises a low spatial frequency region and a high spatial frequency region substantially superimposed within the low spatial frequency region. Further, the low spatial frequency region comprises an average lateral feature size that exceeds an average lateral feature size of the high spatial frequency region. In addition, the textured region comprises a surface roughness (Ra) from about 10 nm to about 1000 nm.
-
公开(公告)号:US10917989B2
公开(公告)日:2021-02-09
申请号:US16363208
申请日:2019-03-25
Applicant: CORNING INCORPORATED
Inventor: Jaymin Amin , Joshua Michael Jacobs , Jonathan David Pesansky , Kevin Barry Reiman , Ananthanarayanan Subramanian
Abstract: Disclosed are device display screen protectors comprising a first strengthened substrate sized to cover a display screen of an electronic device, the first strengthened substrate having a central tension value in the range greater than 0 MPa and less than 20 MPa, a surface having a Knoop lateral cracking scratch threshold of at least 3 N.
-
公开(公告)号:US20200325064A1
公开(公告)日:2020-10-15
申请号:US16843377
申请日:2020-04-08
Applicant: Corning Incorporated
Inventor: Jaymin Amin , Robert Randall Hancock, JR. , Raymond Chih Chung Hsiao , Yuhui Jin , Aize Li , Jared Hilliard Seaman
Abstract: A glass substrate comprises: a first surface with surface features having an average width, an average height, a ratio of the average width to the average height of from about 0.04 to about 0.24, and the first surface has a haze value of 3% to 40%. The glass substrate can be transparent to electromagnetic radiation in the visible spectrum. The glass substrate can have a composition of: 61-75 mol. % SiO2; 7-15 mol. % Al2O3; 0-12 mol. % B2O3; 9-21 mol. % Na2O; 0-4 mol. % K2O; 0-7 mol. % MgO; and 0-3 mol. % CaO. The first surface can have an average surface roughness Ra of from 10 nm to 1,000 nm. The first surface can have an average characteristic largest feature size of from 200 nm to 50 μm. The ratio of the average width to the average height can be from 0.06 to about 0.08.
-
公开(公告)号:US20200223749A1
公开(公告)日:2020-07-16
申请号:US16830889
申请日:2020-03-26
Applicant: CORNING INCORPORATED
Inventor: Jaymin Amin , Benedict Osobomen Egboiyi , Jonathan David Pesansky , Kevin Barry Reiman , Rostislav Vatchev Roussev , Brian Paul Strines
Abstract: Chemically strengthened glass articles having at least one deep compressive layer extending from a surface of the article to a depth of compression DOC of at least about 125 μm within the glass article. The compressive stress profile includes a single linear segment or portion extending from the surface to the depth of compression DOC. Alternatively, the compressive stress profile may include an additional portion extending from the surface to a relatively shallow depth and the linear portion extending from the shallow depth to the depth of compression.
-
公开(公告)号:US20190330105A1
公开(公告)日:2019-10-31
申请号:US16506116
申请日:2019-07-09
Applicant: CORNING INCORPORATED
Inventor: Jaymin Amin , Yuhui Jin , Kristy Lynn Smith
Abstract: Methods for reducing a defective area in a strengthened substrate to produce a non-defective substrate are provided. The methods include contacting a strengthened defective substrate with a heated salt bath containing at least one monovalent salt, and removing the strengthened substrate from the bath. The strengthened substrate, before being contacted with the salt bath, is a defective substrate having at least one defective area and one or more non-defective area. Upon removal from the salt bath, at least one defective area has been reduced or substantially removed to produce a non-defective substrate.
-
公开(公告)号:US09902648B2
公开(公告)日:2018-02-27
申请号:US15158230
申请日:2016-05-18
Applicant: CORNING INCORPORATED
Inventor: Jaymin Amin , Benedict Osobomen Egboiyi , Jonathan David Pesansky , Kevin Barry Reiman , Rostislav Vatchev Roussev , Brian Paul Strines
IPC: C03C4/18 , C03C21/00 , C03C3/097 , C03C3/091 , C03C3/093 , C03C3/095 , C03C3/087 , C03C3/04 , C03C3/085 , G06F1/16 , H04B1/3827
CPC classification number: C03C21/002 , C03C3/04 , C03C3/085 , C03C3/087 , C03C3/091 , C03C3/093 , C03C3/095 , C03C3/097 , C03C4/18 , C03C21/00 , C03C2204/00 , G06F1/1637 , G06F2200/1634 , H04B1/3827 , Y10T428/315
Abstract: Chemically strengthened glass articles having at least one deep compressive layer extending from a surface of the article to a depth of at least about 45 μm within the article are provided. In one embodiment, the compressive stress profile includes a single linear segment extending from the surface to the depth of compression DOC. Alternatively, the compressive stress profile includes two linear portions: the first portion extending from the surface to a relatively shallow depth and having a steep slope; and a second portion extending from the shallow depth to the depth of compression. The strengthened glass has a 60% survival rate when dropped from a height of 80 cm in an inverted ball drop test and an equibiaxial flexural strength of at least 10 kgf as determined by abraded ring-on-ring testing. Methods of achieving such stress profiles are also described.
-
公开(公告)号:US20180044231A1
公开(公告)日:2018-02-15
申请号:US15672567
申请日:2017-08-09
Applicant: CORNING INCORPORATED
Inventor: Jaymin Amin , Yuhui Jin , Kristy Lynn Smith
CPC classification number: C03C21/002 , C03C3/093 , C03C3/097 , C03C4/18 , C03C21/005 , C03C2204/00
Abstract: Methods for reducing a defective area in a strengthened substrate to produce a non-defective substrate are provided. The methods include contacting a strengthened defective substrate with a heated salt bath containing at least one monovalent salt, and removing the strengthened substrate from the bath. The strengthened substrate, before being contacted with the salt bath, is a defective substrate having at least one defective area and one or more non-defective area. Upon removal from the salt bath, at least one defective area has been reduced or substantially removed to produce a non-defective substrate.
-
-
-
-
-
-
-
-
-