公开(公告)号:US06391274B1
公开(公告)日:2002-05-21
申请号:US09389465
申请日:1999-09-03
申请人: Conny Vogler , Frank Forster , Karl Vogel , Burkhard Freund
发明人: Conny Vogler , Frank Forster , Karl Vogel , Burkhard Freund
IPC分类号: C09C148
CPC分类号: B60C1/00 , C01P2006/12 , C01P2006/19 , C09C1/50 , C09C1/56
摘要: Carbon black characterized by a STSA surface of between 20 and 180 m2/g, a 24M4-DBP absorption of between 40 and 140 ml/100 g, a specific BET surface of between 20 and 250 m2/g, a content of 0.01 to 20 wt. % of silicon, referred to its overall weight, and a tan &dgr;0/tan &dgr;60 ratio greater than 3.37−0.0068 STSA is produced by mixing silicon-containing compounds with the carbon black raw materials in the oxidative pyrolysis of the carbon black raw materials and optionally using carbon black oil as fuel. The carbon black can be used as a filler in rubber mixtures, preferably for tires.
摘要翻译: 炭黑的特征在于STSA表面为20〜180m 2 / g,24M4-DBP吸收为40〜140ml / 100g,比BET表面积为20〜250m2 / g,含量为0.01〜20 重量 通过将含硅化合物与炭黑原料在炭黑原料的氧化热解中混合并任选地产生通过将硅的%称为其总重量,并且大于3.37-0.0068 STSA的tanδ0/tanδ60比率 使用炭黑油作为燃料。 炭黑可用作橡胶混合物中的填料,优选用于轮胎。
-
公开(公告)号:US06251983B1
公开(公告)日:2001-06-26
申请号:US09329313
申请日:1999-06-10
申请人: Conny Vogler , Karl Vogel , Werner Niedermeier , Burkhard Freund , Paul Messer
发明人: Conny Vogler , Karl Vogel , Werner Niedermeier , Burkhard Freund , Paul Messer
IPC分类号: C08K303
CPC分类号: C09C1/50 , B60C1/00 , C01P2006/19 , C01P2006/60 , C08K3/04 , Y02T10/862 , C08L21/00
摘要: Inversion carbon blacks and a method for their manufacture are disclosed. The inversion carbon blacks have a lower rolling resistance with identical or improved wet skid behavior. The particle size distribution contains a smaller proportion of particles with large diameters. This leads to an improved abrasion behavior of rubber compounds which were prepared using these carbon blacks. The inversion carbon blacks can be manufactured in conventional carbon black reactors by controlling the combustion in the combustion chamber in such a manner that carbon black nuclei form, which are immediately brought into contact with the carbon black raw material. The carbon blacks present a lower proportion of larger particles if the additions of combustion air and carbon black raw material are increased in an appropriate manner.
摘要翻译: 公开了反相炭黑及其制造方法。 反转炭黑具有较低的滚动阻力,具有相同或改善的湿滑行为。 粒度分布包含较小比例的具有较大直径的颗粒。 这导致使用这些炭黑制备的橡胶化合物的改进的磨损行为。 在常规的炭黑反应器中可以通过控制燃烧室中的燃烧以立即与炭黑原料接触的形成炭黑核的方式制造反转炭黑。 如果以适当的方式增加燃烧空气和炭黑原料的添加量,则炭黑呈现较小比例的较大颗粒。
-
公开(公告)号:US6056933A
公开(公告)日:2000-05-02
申请号:US160143
申请日:1998-09-25
申请人: Conny Vogler , Karl Vogel , Werner Niedermeier , Burkhard Freund , Paul Messer
发明人: Conny Vogler , Karl Vogel , Werner Niedermeier , Burkhard Freund , Paul Messer
CPC分类号: B60C1/0016 , B82Y30/00 , C08K3/04 , C09C1/50 , C01P2004/62 , C01P2004/64 , C01P2006/12 , C01P2006/19
摘要: Inversion carbon blacks and a method for their manufacture and disclosed. The inversion carbon blacks have a smaller rolling resistance with identical or improved wet sliding behavior. The particle size distribution contains a smaller proportion of particles with large diameters. This leads to an improved abrasion behavior of rubber compounds which were prepared using these carbon blacks. The inversion carbon blacks can be manufactured in conventional carbon black reactors by controlling the combustion in the combustion chamber in such a manner that carbon black nuclei form, which are immediately brought into contact with the carbon black raw material. The carbon blacks present a lower proportion of larger particles if the additions of combustion air and carbon black raw material are increased in an appropriate manner.
摘要翻译: 反转炭黑及其制造方法及披露。 反转炭黑具有较小的滚动阻力,具有相同或改善的湿滑动特性。 粒度分布包含较小比例的具有较大直径的颗粒。 这导致使用这些炭黑制备的橡胶化合物的改进的磨损行为。 在常规的炭黑反应器中可以通过控制燃烧室中的燃烧以立即与炭黑原料接触的形成炭黑核的方式制造反转炭黑。 如果以适当的方式增加燃烧空气和炭黑原料的添加量,则炭黑呈现较小比例的较大颗粒。
-
公开(公告)号:US08735488B2
公开(公告)日:2014-05-27
申请号:US12680453
申请日:2008-09-04
CPC分类号: C09C1/50 , B82Y30/00 , C01P2004/51 , C01P2004/64 , C01P2006/12 , C01P2006/16 , C01P2006/19 , C01P2006/60 , C08K3/04 , C09C1/48 , C08L21/00
摘要: The invention relates to black having a CTAB surface area of 100 to 160 m?/g, a quartile ratio of more than 1.60, and an FP index of >0. Said black is produced in a furnace reactor. Sixty to 90 percent by weight of the raw black material are injected into the reactor in the first third of the reaction zone, while the remaining amount of the raw black material is injected into the reactor upstream at least in one other point. In addition, the combustible is conducted such that 90 to 100 percent by weight of the combustible are evaporated when first hitting the raw black material and 80 to 99 percent by weight of the combustible are evaporated 5 ms before hitting the raw black material. Said blacks can be used in rubber mixtures.
摘要翻译: 本发明涉及CTAB表面积为100〜160mΩ/ g,四分位数大于1.60,FP指数> 0的黑色。 所述黑色在炉式反应器中生产。 原料黑料的重量百分之六十至九十重量百分比在反应区的第一个三分之一被注入反应器中,而至少在另一个点上将原料黑色材料的剩余量注入反应器的上游。 此外,可燃物的进行使得当首次击中生黑色材料时,90〜100重量%的可燃物蒸发,80〜99重量%的可燃物在打黑原料之前蒸发5秒钟。 所述黑色可用于橡胶混合物。
-
公开(公告)号:US20110034611A1
公开(公告)日:2011-02-10
申请号:US12680453
申请日:2008-09-04
CPC分类号: C09C1/50 , B82Y30/00 , C01P2004/51 , C01P2004/64 , C01P2006/12 , C01P2006/16 , C01P2006/19 , C01P2006/60 , C08K3/04 , C09C1/48 , C08L21/00
摘要: The invention relates to black having a CTAB surface area of 100 to 160 m?/g, a quartile ratio of more than 1.60, and an FP index of >0. Said black is produced in a furnace reactor. Sixty to 90 percent by weight of the raw black material are injected into the reactor in the first third of the reaction zone, while the remaining amount of the raw black material is injected into the reactor upstream at least in one other point. In addition, the combustible is conducted such that 90 to 100 percent by weight of the combustible are evaporated when first hitting the raw black material and 80 to 99 percent by weight of the combustible are evaporated 5ms before hitting the raw black material. Said blacks can be used in rubber mixtures.
摘要翻译: 本发明涉及CTAB表面积为100〜160mΩ/ g,四分位数大于1.60,FP指数> 0的黑色。 所述黑色在炉式反应器中生产。 原料黑料的重量百分之六十至九十重量百分比在反应区的第一个三分之一被注入反应器中,而至少在另一个点上将原料黑色材料的剩余量注入反应器的上游。 此外,可燃物的进行使得当首次击中原料黑色物质时,90〜100重量%的可燃物蒸发,80〜99重量%的可燃物在打黑原料之前被蒸发5ms。 所述黑色可用于橡胶混合物。
-
公开(公告)号:US06689505B1
公开(公告)日:2004-02-10
申请号:US09648343
申请日:2000-08-25
申请人: Peter Albers , Emmanuel Auer , Walther Behl , Karl Vogel , Conny Vogler
发明人: Peter Albers , Emmanuel Auer , Walther Behl , Karl Vogel , Conny Vogler
IPC分类号: H01M496
CPC分类号: H01M4/926 , B01J21/18 , B01J23/42 , B01J37/031 , H01M4/921 , H01M8/1004 , H01M2300/0082 , Y02P70/56
摘要: Electrocatalyst which are formed of a carbon support, which is a carbon black with an H content of >4000 ppm and, as the catalytically active component, platinum or bi- or multi-metallically doped or alloyed platinum. The electrocatalysts are prepared by deposition of noble metals on the carbon black surface. They can be used for the production of fuel cells.
摘要翻译: 由碳载体形成的电催化剂,其为H含量> 4000ppm的炭黑,以及作为催化活性组分的铂或双金属或多金属掺杂或合金化的铂。 通过在炭黑表面上沉积贵金属制备电催化剂。 它们可用于生产燃料电池。
-
公开(公告)号:US06231624B1
公开(公告)日:2001-05-15
申请号:US08866245
申请日:1997-06-05
申请人: Conny Vogler , Karl Vogel , Jan Kopietz
发明人: Conny Vogler , Karl Vogel , Jan Kopietz
IPC分类号: C01B3114
CPC分类号: C09C1/60 , C01P2004/51 , C01P2006/10 , C01P2006/11 , C01P2006/12 , C01P2006/19
摘要: A process for continuous dry granulation of powdered carbon black. Granulation is performed with the assistance of a granulator. As a result, for comparable sized equipment, the carbon black throughput can be increased several times as compared with pelletizing drums used in the conventional manner.
摘要翻译: 一种粉末状炭黑连续干法造粒的方法。 在造粒机的帮助下进行造粒。 结果,对于相当尺寸的设备,与以常规方式使用的造粒鼓相比,炭黑产量可以增加几倍。
-
公开(公告)号:US6132876A
公开(公告)日:2000-10-17
申请号:US212272
申请日:1998-12-16
申请人: Conny Vogler , Karl Vogel , Udo Wieschnowsky , Jan Kopietz
发明人: Conny Vogler , Karl Vogel , Udo Wieschnowsky , Jan Kopietz
CPC分类号: C09C1/58 , C01P2006/12 , C01P2006/19 , Y10T428/30
摘要: Carbon black pellets which can be produced by the addition of wax during dry granulation of carbon black powder. The carbon black pellets are distinguished by a pellet hardness of at least 0.15 N with a wax content of less than 10 wt. %, based on the total weight of the carbon black pellets.
摘要翻译: 炭黑颗粒,其可以通过在炭黑粉末的干法制粒过程中加入蜡来生产。 炭黑颗粒的特征在于蜡含量低于10重量%的至少0.15N的颗粒硬度。 %,基于炭黑颗粒的总重量。
-
公开(公告)号:US08852739B2
公开(公告)日:2014-10-07
申请号:US13031694
申请日:2011-02-22
申请人: Arndt-Peter Schinkel , Michael Stanyschöfsky , Conny Vogler , Joachim Fröhlich , Bernhard Schwaiger , Thomas Pelster
发明人: Arndt-Peter Schinkel , Michael Stanyschöfsky , Conny Vogler , Joachim Fröhlich , Bernhard Schwaiger , Thomas Pelster
CPC分类号: C09C1/50 , B29K2007/00 , B29K2009/00 , B60C1/00 , B82Y30/00 , C01P2004/64 , C01P2006/12 , C01P2006/19 , C09C1/48 , Y10T428/2982
摘要: The invention relates to a carbon black with a CTAB surface area of from 20 to 49 m2/g, with a COAN greater than 90 ml/(100 g), and with a sum of OAN and COAN greater than 235 ml/(100 g). The carbon black is produced in a furnace reactor, where from 20 to 55% by weight of the feedstock used for the carbon black are introduced radially through a nozzle within the first third of the reaction zone, and the remaining amount of the feedstock used for the carbon black is introduced through a nozzle upstream at least one further point into the reactor. The carbon black can be used in rubber mixtures.
摘要翻译: 本发明涉及CTAB表面积为20至49m 2 / g,碳当量大于90ml /(100g),且COAN大于235ml /(100g )。 炭黑在炉式反应器中生产,其中20至55重量%的用于炭黑的原料通过喷嘴在径向上被引入反应区的第一个三分之一内,而用于 炭黑通过喷嘴上游至少一个进一步的喷嘴引入反应器。 炭黑可用于橡胶混合物。
-
公开(公告)号:US20110207872A1
公开(公告)日:2011-08-25
申请号:US13031694
申请日:2011-02-22
申请人: Arndt-Peter Schinkel , Michael Stanyschöfsky , Conny Vogler , Joachim Fröhlich , Bernhard Schwaiger , Thomas Pelster
发明人: Arndt-Peter Schinkel , Michael Stanyschöfsky , Conny Vogler , Joachim Fröhlich , Bernhard Schwaiger , Thomas Pelster
CPC分类号: C09C1/50 , B29K2007/00 , B29K2009/00 , B60C1/00 , B82Y30/00 , C01P2004/64 , C01P2006/12 , C01P2006/19 , C09C1/48 , Y10T428/2982
摘要: The invention relates to a carbon black with a CTAB surface area of from 20 to 49 m2/g, with a COAN greater than 90 ml/(100 g), and with a sum of OAN and COAN greater than 235 ml/(100 g). The carbon black is produced in a furnace reactor, where from 20 to 55% by weight of the feedstock used for the carbon black are introduced radially through a nozzle within the first third of the reaction zone, and the remaining amount of the feedstock used for the carbon black is introduced through a nozzle upstream at least one further point into the reactor. The carbon black can be used in rubber mixtures.
摘要翻译: 本发明涉及CTAB表面积为20至49m 2 / g,碳当量大于90ml /(100g),且COAN大于235ml /(100g )。 炭黑在炉式反应器中生产,其中20至55重量%的用于炭黑的原料通过喷嘴在径向上被引入反应区的第一个三分之一内,而用于 炭黑通过喷嘴上游至少一个进一步的喷嘴引入反应器。 炭黑可用于橡胶混合物。
-
-
-
-
-
-
-
-
-