摘要:
The invention relates to a carbon black having an aggregate size distribution which has a (d90−d10)/d50 ratio of less than or equal to 1.1. The carbon blacks are produced by admixing hot air if desired to a gas mixture comprising a carrier gas and a carbon black feedstock, passing the gas mixture into a burner pipe, burning the gas mixture at the burner pipe openings, and drawing the flames under suction, together with the ambient air drawn in freely under suction from the outside, through a cooled, narrowing gap, and carrying out cooling, the cooled, narrowing gap having a height (h) to width (b) ratio of 1-100, the width (b) being 0.5 to 10 mm, and the flow rate at the narrowest point of the gap being 10-200 m/s. The carbon blacks can be used as non-reinforcing filler, reinforcing filler, UV stabilizer, conductive black, pigment or reducing agent.
摘要:
The invention relates to carbon black having a C-14 content greater than 0.05 Bq/g and a ratio ΔD50/Dmode of the aggregate size distribution of less than 0.7. The carbon black is produced by thermal oxidative pyrolysis or thermal cleavage of the carbon black raw material in that the carbon black raw material contains renewable carbon black raw materials and an oxygen deficiency is present in the pyrolysis/cleavage reaction. The carbon blacks can be used in rubber and rubber mixtures, plastic, printing inks, inks, inkjet inks, toners, lacquers, paints, paper, adhesives, batteries, pastes, bitumens, concrete, and other building materials and as reducing agents in metallurgy.
摘要:
The invention relates to a carbon black having an aggregate size distribution which has a (d90-d10)/d50 ratio of less than or equal to 1.1. The carbon blacks are produced by admixing hot air if desired to a gas mixture comprising a carrier gas and a carbon black feedstock, passing the gas mixture into a burner pipe, burning the gas mixture at the burner pipe openings, and drawing the flames under suction, together with the ambient air drawn in freely under suction from the outside, through a cooled, narrowing gap, and carrying out cooling, the cooled, narrowing gap having a height (h) to width (b) ratio of 1-100, the width (b) being 0.5 to 10 mm, and the flow rate at the narrowest point of the gap being 10-200 m/s. The carbon blacks of the invention can be used as non-reinforcing filler, reinforcing filler, UV stabilizer, conductive black, pigment or reducing agent.
摘要:
The invention relates to a carbon black with a CTAB surface area of from 20 to 49 m2/g, with a COAN greater than 90 ml/(100 g), and with a sum of OAN and COAN greater than 235 ml/(100 g). The carbon black is produced in a furnace reactor, where from 20 to 55% by weight of the feedstock used for the carbon black are introduced radially through a nozzle within the first third of the reaction zone, and the remaining amount of the feedstock used for the carbon black is introduced through a nozzle upstream at least one further point into the reactor. The carbon black can be used in rubber mixtures.
摘要:
The invention relates to carbon black having a C-14 content greater than 0.05 Bq/g and a ratio ΔD50/Dmode of the aggregate size distribution of less than 0.7. The carbon black is produced by thermal oxidative pyrolysis or thermal cleavage of the carbon black raw material in that the carbon black raw material contains renewable carbon black raw materials and an oxygen deficiency is present in the pyrolysis/cleavage reaction. The carbon blacks can be used in rubber and rubber mixtures, plastic, printing inks, inks, inkjet inks, toners, lacquers, paints, paper, adhesives, batteries, pastes, bitumens, concrete, and other building materials and as reducing agents in metallurgy.
摘要翻译:本发明涉及C-14含量大于0.05Bq / g的碳黑,并且聚集体尺寸分布的比D&D D D D / 炭黑是通过炭黑原料的热氧化热解或热裂解产生的,因为炭黑原料含有可再生炭黑原料,热解/裂解反应存在缺氧。 炭黑可用于橡胶和橡胶混合物,塑料,印刷油墨,油墨,喷墨油墨,调色剂,油漆,油漆,纸张,粘合剂,电池,糊料,沥青,混凝土和其他建筑材料,以及冶金中的还原剂 。
摘要:
The invention relates to a carbon black with a CTAB surface area of from 20 to 49 m2/g, with a COAN greater than 90 ml/(100 g), and with a sum of OAN and COAN greater than 235 ml/(100 g). The carbon black is produced in a furnace reactor, where from 20 to 55% by weight of the feedstock used for the carbon black are introduced radially through a nozzle within the first third of the reaction zone, and the remaining amount of the feedstock used for the carbon black is introduced through a nozzle upstream at least one further point into the reactor. The carbon black can be used in rubber mixtures.