Abstract:
A process comprising powder moulding a polymer composition having a Shore D hardness value less than 40 points; said polymer composition comprising: 1) a polyolefin composition consisting of: i) 5 to less than 100 parts by weight of a crystalline or partially crystalline isotactic polymer of 1-butene; and ii) more than 0 to 95 parts by weight of a thermoplastic elastomeric polyolefin composition having a melt flow rate of 20-100 g/10 min; or 2) a polyolefin composition consisting of: iii) 100 parts by weight of a crystalline or partially crystalline isotactic polymer of 1-butene or composition (1); and iv) more than 0 to 100 parts by weight of an elastomeric polymer; provided that when the polymer of 1-butene is a homopolymer or a copolymer with less than 2 wt % of comonomer, polymer compositions (1) and (2) contain at least 5 parts by weight of an elastomeric polymer.