Abstract: A thin-walled honeycombed structure is made by extruding a plastically deformable batch, including ceramic materials mixed with water and a methyl cellulose extrusion aid, through a die apparatus comprising an extrusion barrel, an extrusion die extending transversely across the barrel and a mask located around the periphery of the outlet face of the die for inwardly moving peripheral portions of the extruded structure to form an integral skin of material. The temperature of the batch as it is placed into the barrel is 2*-25*F. (preferably 5*-15*F.) above the gel point of such batch. The extrusion barrel is maintained at a temperature 0*-15*F. (preferably 5*-12*F.) less than the temperature of the ceramic batch placed in the barrel (and preferably not less than 5*F. below the gel point of the batch) to form a uniform skin of desired thickness on the honeycombed structure.
Abstract translation: 薄壁蜂窝结构通过挤出可塑性变形的批料,包括与水和甲基纤维素挤出助剂混合的陶瓷材料,通过包括挤出筒,挤压模横向延伸穿过筒体的模具装置和围绕 模具的出口面的周边,用于向内移动挤出结构的周边部分,以形成整体的材料表皮。 批料放入管内时的温度应在该批次的凝胶点以上2°-25°F(优选5°-15°F)。 挤出筒保持在低于置于桶中的陶瓷批料的温度(优选不小于凝胶下面5°F)的0°-15°F(优选5°-12°F)的温度 点)以在蜂窝结构上形成所需厚度的均匀皮肤。