摘要:
A polymer blend foam having smooth skin and/or an open-cell content of at least 20 volume percent, a crosslinked gel content of no greater than 10 percent, a minimum cross-sectional area of at least 1000 mm.sup.2, and a density of no greater than 250 kg/m.sup.3. The blend includes (A) a substantially random interpolymer having polymerized therein (1) a vinyl or vinylidene aromatic monomer and/or a sterically hindered aliphatic or cycloaliphatic vinyl or vinylidene monomer, and (2) one or more of ethylene and a C.sub.3-20 aliphatic .alpha.-olefin; and (B) an olefin polymer based on one or more of ethylene, C.sub.3-20 aliphatic .alpha.-olefins, and C.sub.3-20 aliphatic .alpha.-olefins containing polar groups. The olefin polymer (B) lacks any of the vinyl or vinylidene aromatic monomers found in (A).
摘要:
This invention pertains to a composition and a process for preparing a closed cell alkenyl aromatic polymer foam having enlarged cell size, comprising one or more alkenyl aromatic polymers, one or more substantially random interpolymers, one or more blowing agents having zero ozone depletion potential and optionally one or more co-blowing agents, and optionally, one or more nucleating agents and optionally, one or more other additives.This combination allows the manufacture of closed cell, low density alkenyl aromatic polymer foams of enlarged cell size, when blowing agents of relatively high nucleation potential are employed. When such blowing agents are used with alkenyl aromatic polymers in the absence of the substantially random interpolymers, small cell foams result.
摘要:
A blend of polymeric materials comprising (A) of from about 1 to about 99.99 weight percent based on the combined weights of Components A, B and C of at least one substantially random interpolymer; and wherein said interpolymer; (1) contains of from about 0.5 to about 65 mole percent of polymer units derived from; (a) at least one vinyl or vinylidene aromatic monomer, or (b) at least one hindered aliphatic or cycloaliphatic vinyl or vinylidene monomer, or (c) a combination of at least one vinyl or vinylidene aromatic monomer and at least one hindered aliphatic or cycloaliphatic vinyl or vinylidene monomer; (2) contains of from about 35 to about 99.5 mole percent of polymer units derived from at least one aliphatic &agr;-olefin having from 2 to 20 carbon atoms; (3) has a molecular weight (Mn) greater than about 1,000; (4) has a melt index (I2) of from about 0.01 to about 1,000; (5) has a molecular weight distribution (Mw/Mn) of from about 1.5 to about 20; and (B) of from about 99 to about 0.01 weight percent based on the combined weights of Components A, B, and C of one or more conductive additives and/or one or more additives with high magnetic permeability ; and (C) of from 0 to about 98.99 weight percent based on the combined weights of Components A, B, and C of one or more polymers other than A.
摘要:
A soft foam having an Asker C hardness of less than about 65, comprising; (A) from about 30 to about 70 percent by weight (based on the combined weight of Components A and B) of one or more alkenyl aromatic polymers and wherein at least one of said alkenyl aromatic polymers has a molecular weight (Mw) of from about 100,000 to about 500,000; and (B) from about 30 to about 70 percent by weight (based on the combined weight of Components A and B) of one or more substantially random interpolymers having an I2 of about 0.1 to about 50 g/10 min, an Mw/Mn of about 1.5 to about 20; comprising (1) from about 8 to about 45 mol % of polymer units derived from; (a) at least one vinyl or vinylidene aromatic monomer, or (b) at least one hindered aliphatic or cycloaliphatic vinyl or vinylidene monomer, or (c) a combination of at least one aromatic vinyl or vinylidene monomer and at least one hindered aliphatic or cycloaliphatic vinyl or vinylidene monomer, and (2) from about 55 to about 92 mol % of polymer units derived from at least one of ethylene and/or a C3-20 &agr;-olefin; and (3) from 0 to about 20 mol % of polymer units derived from one or more of ethylenically unsaturated polymerizable monomers other than those derived from (1) and (2); and (C) optionally, one or more nucleating agents; and (D) optionally, one or more other additives; and (E) one or more blowing agents present in a total amount of from about 0.4 to about 5.0 gram-moles per kilogram (based on the combined weight of Components A and B).
摘要:
A soft foam having an Asker C hardness of less than about 65, comprising;(A) from about 30 to about 70 percent by weight (based on the combined weight of Components A and B) of one or more alkenyl aromatic polymers and wherein at least one of said alkenyl aromatic polymers has a molecular weight (M.sub.w) of from about 100,000 to about 500,000; and(B) from about 30 to about 70 percent by weight (based on the combined weight of Components A and B) of one or more substantially random interpolymers; and(C) optionally, one or more nucleating agents; and(D) optionally, one or more other additives; and(E) one or more blowing agents present in a total amount of from about 0.4 to about 5.0 gram-moles per kilogram (based on the combined weight of Components A and B).
摘要:
The present invention pertains to improved alkenyl aromatic polymer foams (and processes for their preparation) having increased heat distortion temperature and improved dimensional stability while maintaining good tensile/tear, creep and environmental dimensional change properties.The closed cell low density alkenyl aromatic polymer foams exhibit increased heat distortion temperature, when substantially random interpolymers of about 21 to about 65 mol % styrene are blended in. When these same alkenyl aromatic polymer foams are made without these interpolymers, the heat distortion temperature is not improved.
摘要:
This invention pertains to a composition and a process for preparing a closed cell alkenyl aromatic polymer foam having enlarged cell size, comprising one or more alkenyl aromatic polymers, one or more substantially random interpolymers, one or more blowing agents having zero ozone depletion potential and optionally one or more co-blowing agents, and optionally, one or more nucleating agents and optionally, one or more other additives. This combination allows the manufacture of closed cell, low density alkenyl aromatic polymer foams of enlarged cell size, when blowing agents of relatively high nucleation potential are employed. When such blowing agents are used with alkenyl aromatic polymers in the absence of the substantially random interpolymers, small cell foams result.
摘要:
An acoustical insulation foam having, either with or without elastification, an Asker C hardness of less than about 65, a density of about 5 to about 150 kg/m3, a cell size of about 0.05 to about 15 mm, an open cell content of 0 to about 100 volume percent, a thickness of about 1 to about 200 mm, and a width of about 100 to about 3000 mm; comprising; (A) one or more alkenyl aromatic polymers, (B) one or more substantially random interpolymers and (C) optionally, one or more nucleating agents and (D) optionally, one or more other additives; and (E) one or more blowing agents.
摘要翻译:一种绝缘泡沫,具有或不具有弹性,具有小于约65的Asker C硬度,约5至约150kg / m 3的密度,约0.05至约15mm的孔尺寸,开孔含量 0至约100体积%,厚度为约1至约200mm,宽度为约100至约3000mm; (A)一种或多种链烯基芳族聚合物,(B)一种或多种基本上无规共聚体和(C)任选的一种或多种成核剂和(D)任选的一种或多种其它添加剂; 和(E)一种或多种发泡剂。
摘要:
An acoustical insulation foam having, either with or without elastification, an Asker C hardness of less than about 65, a density of about 5 to about 150 kg/m3, a cell size of about 0.05 to about 15 mm, an open cell content of 0 to about 100 volume percent, a thickness of about 1 to about 200 mm, and a width of about 100 to about 3000 mm; comprising; (A) one or more alkenyl aromatic polymers, (B) one or more substantially random interpolymers and (C) optionally, one or more nucleating agents and (D) optionally, one or more other additives; and (E) one or more blowing agents.
摘要翻译:一种绝缘泡沫,具有或不具有弹性,具有小于约65的Asker C硬度,约5至约150kg / m 3的密度,约0.05至约15mm的孔尺寸,开孔含量 0至约100体积%,厚度为约1至约200mm,宽度为约100至约3000mm; (A)一种或多种链烯基芳族聚合物,(B)一种或多种基本上无规共聚体和(C)任选的一种或多种成核剂和(D)任选的一种或多种其它添加剂; 和(E)一种或多种发泡剂。
摘要:
The present disclosure is directed to a plasticizer, polymeric compositions containing the plasticizer, and conductors coated with the polymeric composition. The plasticizer includes (i) an epoxidized fatty acid methyl ester, (ii) an epoxidized natural oil, and (iii) an epoxidized tallate ester. Polymeric compositions containing a polymeric resin and the plasticizer exhibit a weight loss less than 50 mg/cm2 after exposure to 100° C. for seven days. Conductors coated with the polymeric composition (containing the plasticizer) pass the low temperature unwind test of UL719 and exhibit a weight loss less than 50 mg/cm2 after exposure to 100° C. for seven days.
摘要翻译:本公开涉及含增塑剂的增塑剂,聚合物组合物和涂覆有聚合物组合物的导体。 增塑剂包括(i)环氧化脂肪酸甲酯,(ii)环氧化天然油,和(iii)环氧化的酯酸酯。 含有聚合物树脂和增塑剂的聚合物组合物在暴露于100℃下显示重量损失小于50mg / cm 2,持续7天。 用聚合物组合物(含增塑剂)涂覆的导体通过UL719的低温退火试验,并且在暴露于100℃下显示出低于50mg / cm 2的重量减少7天。