Coating composition and method of forming
    2.
    发明授权
    Coating composition and method of forming 失效
    涂料组合物和成型方法

    公开(公告)号:US5279649A

    公开(公告)日:1994-01-18

    申请号:US63797

    申请日:1993-05-20

    CPC classification number: C04B28/342 C09D5/103 C23C22/74 C04B2111/00482

    Abstract: A coating composition comprises a slurry consisting essentially of an aluminum neutralized phosphate bonding solution and aluminum powder. The bonding solution advantageously contains a relatively small but essential amount of vanadium pentoxide and, preferably, magnesium. A process for forming the bonding solution component of the coating slurry includes equilibrating an aqueous phosphate solution with a small but controlled and necessary amount of solute aluminum prior to adding aluminum powder to form the slurry. The present invention overcomes the problem of bonding solutions which require environmentally disadvantageous chromates or molybdates.

    Abstract translation: 涂料组合物包含基本上由铝中和磷酸盐粘合溶液和铝粉末组成的浆料。 粘合溶液有利地包含相对小但必要量的五氧化二钒,优选含有镁。 用于形成涂布浆料的粘合溶液成分的方法包括在加入铝粉以形成浆料之前,用少量但受控并且必需量的溶质铝平衡磷酸盐水溶液。 本发明克服了需要环境不利的铬酸盐或钼酸盐的粘结溶液的问题。

    Slip composition
    3.
    发明授权

    公开(公告)号:US10336648B1

    公开(公告)日:2019-07-02

    申请号:US07233708

    申请日:1988-08-19

    Inventor: Alvin R. Stetson

    Abstract: A slip composition includes an electromagnetic-absorbing, magnetic powder having a mean particle size of not more than about 6 microns, a glass or vitreous frit having a mean particle size of not more than about 6 microns, and a methyl alcohol vehicle.A method of making a slip composition void of clay and aluminum oxide, includes mixing a wet milled vitreous frit, a powdered magnetic material, and a methyl alcohol vehicle.The disclosed embodiment is particularly useful in making an electromagnetic wave absorption coating suitable for application to stainless steel and many nickel base alloys.

    Coating composition and method of forming
    4.
    发明授权
    Coating composition and method of forming 失效
    涂料组合物和成型方法

    公开(公告)号:US5242488A

    公开(公告)日:1993-09-07

    申请号:US891098

    申请日:1992-06-01

    CPC classification number: C09D5/103 C04B28/342 C23C22/74 C04B2111/00525

    Abstract: A coating composition for ferrous metal alloy surfaces comprises a slurry consisting essentially of an aluminum neutralized phosphate bonding solution and aluminum powder. A process for forming the bonding solution component of the coating slurry includes equilibrating an aqueous phosphate solution with a small but controlled and necessary amount of solute aluminum prior to adding aluminum powder to form the slurry. The bonding solution preferably also contains magnesium. The present invention overcomes the problem of bonding solutions which require environmentally disadvantageous chromates or molybdates to neutralize the bonding solution prior to formation of the slurry.

    Abstract translation: 用于黑色金属合金表面的涂料组合物包括基本上由铝中和磷酸盐粘合溶液和铝粉末组成的浆料。 用于形成涂布浆料的粘合溶液成分的方法包括在加入铝粉以形成浆料之前,用少量但受控并且必需量的溶质铝平衡磷酸盐水溶液。 粘合溶液优选还含有镁。 本发明克服了在形成浆料之前需要环境不利的铬酸盐或钼酸盐中和粘合溶液的粘合溶液的问题。

    Corrosion resistant seal coat composition and method of forming
    5.
    发明授权
    Corrosion resistant seal coat composition and method of forming 失效
    耐腐蚀密封涂料组合物及其成型方法

    公开(公告)号:US5279650A

    公开(公告)日:1994-01-18

    申请号:US063798

    申请日:1993-05-20

    Abstract: A seal coat composition comprises a slurry consisting essentially of an aluminum neutralized phosphate bonding solution and iron oxide (Fe.sub.2 O.sub.3) powder. The bonding solution advantageously contains a relatively small but essential amount of vanadium pentoxide and, preferably, magnesium. A process for forming the bonding solution component of the coating slurry includes equilibrating an aqueous phosphate solution with a small but controlled and necessary amount of solute aluminum prior to adding iron oxide powder to form the slurry. The present invention overcomes the problem of bonding solutions which require environmentally disadvantageous chromates or molybdates to neutralize the bonding solution prior to formation of the slurry.

    Abstract translation: 密封涂料组合物包含基本上由铝中和磷酸盐粘合溶液和氧化铁(Fe 2 O 3)粉末组成的浆料。 粘合溶液有利地包含相对小但必要量的五氧化二钒,优选含有镁。 用于形成涂布浆料的粘合溶液成分的方法包括在添加氧化铁粉末之前,用少量但受控并且必需量的溶质铝平衡磷酸盐水溶液以形成浆料。 本发明克服了在形成浆料之前需要环境不利的铬酸盐或钼酸盐中和粘合溶液的粘合溶液的问题。

    Glass frit composition
    6.
    发明授权
    Glass frit composition 失效
    玻璃料组成

    公开(公告)号:US4731347A

    公开(公告)日:1988-03-15

    申请号:US855211

    申请日:1986-03-21

    Inventor: Alvin R. Stetson

    CPC classification number: C03C8/02

    Abstract: A glass frit comprising about 60% by weight of glass formers, 30% by weight of monovalent fluxes and 10% by weight of divalent fluxes; the glass formers consisting essentially of SiO.sub.2 and B.sub.2 O.sub.3 ; the monovalent fluxes consisting essentially of Li.sub.2 O, Na.sub.2 O and K.sub.2 O; the divalent fluxes being selected from the group consisting of CaO, SrO, BaO and PbO; and trace elements not exceeding 10% by weight. Preferably the glass frit has the following composition, in terms of oxides:______________________________________ SiO.sub.2 49% B.sub.2 O.sub.3 12% Li.sub.2 O 3.6% Na.sub.2 O 14.4% K.sub.2 O 11.4% CaO 5% SrO 1.85% BaO 2.75% ______________________________________ The glass frit has a coefficient of thermal expansion of 7.2.times.10.sup.-6 /.degree. F. (13.times.10.sup.-6 /.degree. C.) over the range from room temperature to 600.degree. F. (316.degree. C.). It is useable to make a slip where it can be fired at temperatures around 950.degree. F. (510.degree. C.) and applied to a suitable substrate in accordance with existing practices to provide a high quality coating or a viscous damper. Suitable substrates include many nickel-base alloys and stainless steels.

    Abstract translation: 玻璃料包含约60重量%的玻璃形成物,30重量%的单价助熔剂和10重量%的二价助熔剂; 基本上由SiO 2和B 2 O 3组成的玻璃形成剂; 基本上由Li2O,Na2O和K2O组成的单价通量; 所述二价流量选自CaO,SrO,BaO和PbO; 微量元素不超过10重量%。 优选地,玻璃料具有以下氧化物的组成:-SiO 2 49%-B 2 O 3 12%-Li 2 O 3.6%-Na 2 O 14.4%-K 2 O 11.4%-CaO 5%-SrO 1.85%-BaO 2.75% - 玻璃料 在室温至600°F(316℃)的范围内具有7.2×10 -6 /°F(13×10 -6 /℃)的热膨胀系数。 可以在一个可以在950°F(510°C)附近的温度下进行粉碎,并根据现有的实践应用到合适的基材上,以提供高品质的涂层或粘性阻尼器。 合适的基材包括许多镍基合金和不锈钢。

Patent Agency Ranking