公开(公告)号:US4118860A
公开(公告)日:1978-10-10
申请号:US763058
申请日:1977-01-27
CPC分类号: H01M6/48 , H01M6/12 , Y10T29/49115
摘要: The method of making a thin flat laminar battery comprising the steps of coating a substrate with a dispersion of zinc powder and water to produce an anode slurry, and thereafter diffusing electrolytes into said anode slurry; and electrical cells and batteries made by this process.
摘要翻译: 制造薄平板状电池的方法包括以下步骤:用锌粉和水的分散体涂覆基材以产生阳极浆料,然后将电解质扩散到所述阳极浆料中; 以及通过该过程制造的电池和电池。
-
公开(公告)号:US4363407A
公开(公告)日:1982-12-14
申请号:US227477
申请日:1981-01-22
申请人: Sheldon A. Buckler , Jeffrey B. Burns , Alfredo G. Kniazzeh , Paul A. Plasse , David J. Sullivan
发明人: Sheldon A. Buckler , Jeffrey B. Burns , Alfredo G. Kniazzeh , Paul A. Plasse , David J. Sullivan
CPC分类号: B07C5/344 , G01R31/3627 , G01R31/3641 , G01R31/362
摘要: A method and system for testing and sorting a production run of sheet-like batteries includes: testing each battery to obtain a first value of electrical energy; placing machine readable indicia on each battery corresponding to the first value; retesting each battery after passage of a period of time to obtain a second value of electrical energy; machine reading the indicia and computing the rate of decay of electrical energy for each battery as a function of the difference between said first and second values per unit time; and sorting the batteries in accordance with the computed rate of decay to separate those batteries having an acceptable rate of decay from those batteries having too great a rate of decay.
摘要翻译: 用于测试和分类片状电池的生产运行的方法和系统包括:测试每个电池以获得电能的第一值; 在每个电池上放置对应于第一值的机器可读标记; 在经过一段时间后重新测试每个电池以获得第二电能值; 读取标记并计算每个电池的电能衰减速率作为每单位时间的所述第一和第二值之间的差的函数; 并根据计算的衰减速率对电池进行分类,以将具有可接受的衰减速率的电池与具有太大衰减速率的电池分离。
-
公开(公告)号:US4242424A
公开(公告)日:1980-12-30
申请号:US894369
申请日:1978-04-07
摘要: The method of making a thin flat laminar battery comprising the steps of coating a substrate with a dispersion of zinc powder and water to produce an anode slurry, and thereafter diffusing electrolytes into said anode slurry; and electrical cells and batteries made by this process.
摘要翻译: 制造薄平板状电池的方法包括以下步骤:用锌粉和水的分散体涂覆基材以产生阳极浆料,然后将电解质扩散到所述阳极浆料中; 以及通过该过程制造的电池和电池。
-
公开(公告)号:US4080728A
公开(公告)日:1978-03-28
申请号:US744872
申请日:1976-11-24
申请人: Sheldon A. Buckler
发明人: Sheldon A. Buckler
CPC分类号: H01M6/48 , H01M4/50 , H01M6/06 , Y10T29/49114 , Y10T29/49115
摘要: A method of making thin flat laminar batteries in which subassemblies are made by sealing conductive intercell connectors to the inner peripheries of frames of nonconducting material and wet electrodes are applied on either side of the intercell connectors. A separator is placed over one of the wet electrodes. A series array of these subassemblies are sealed together about the outer peripheries of the frames, with electrodes of opposite polarity in adjacent subassemblies in contact with the separator. End cells are completed by frames sealed on one side to terminal collector sheets and on the other side to external surfaces of the series array.
摘要翻译: 制造薄平板状电池的方法,其中通过将导电细胞间连接器密封到不导电材料和湿电极的框架的内周而制成子组件,其被施加在电池单元连接器的任一侧上。 在一个湿电极上放置隔板。 这些子组件的串联阵列围绕框架的外周密封在一起,相邻子组件中与隔板接触的相反极性的电极。 端单元由在一侧封闭到端子集电体片的框架和另一侧到串联阵列的外表面的框架完成。
-
公开(公告)号:US4105815A
公开(公告)日:1978-08-08
申请号:US744871
申请日:1976-11-24
申请人: Sheldon A. Buckler
发明人: Sheldon A. Buckler
CPC分类号: H01M6/48 , H01M4/50 , H01M6/06 , Y10T29/49114 , Y10T29/49115
摘要: Thin flat Leclanche cells and batteries comprising cathodes in the form of slurries of manganese dioxide and carbon in an electrolyte solution containing from 23 to 30 percent of water based on the weight of the slurry. The anodes may be of conventional dry patch construction, or may take the form of slurries of zinc powder in an electrolyte solution containing from 25 to 40 percent of water based on the weight of the anode slurry.
摘要翻译: 薄的扁平Leclanche电池和电池包含基于浆料重量的含有23至30%水的电解液中的二氧化锰和碳浆形式的阴极。 阳极可以是常规的干式贴片结构,或者可以基于阳极浆料的重量,以含有25%至40%的水的电解质溶液的形式获得锌粉的形式。
-
-
-
-