Abstract:
A process for preparing a drag reducing polymer which is to be added to a liquid hydrocarbon. The liquid hydrocarbon has an asphaltene content of at least about 3 weight percent and an API gravity of less than about 26°. The drag reducing polymer can comprise the residues of a monomer having at least one heteroatom. Treatment of the liquid hydrocarbon with the drag reducing polymer allows a reduction in pressure drop associated with turbulent flow of the liquid hydrocarbon through a conduit.
Abstract:
The process begins by obtaining a first batch of monomers selected from a group of acrylates with a molecular weight equal to or less than butyl acrylate and/or methacrylate with a molecular weight equal to or less than butyl methacrylate. A second batch of monomers is then selected from a group of acrylates with a molecular weight greater than butyl acrylate and/or methacrylate with a molecular weight greater than butyl methacrylate. A mixture is then prepared by mixing the first batch of monomers and the second batch of monomers, wherein the second batch of monomers are greater than 50% by weight of the mixture. Finally, the mixture is polymerized to produce an ultra high molecular weight polymer.
Abstract:
The process begins by obtaining a first batch of monomers selected from a group of acrylates with a molecular weight equal to or less than butyl acrylate and/or methacrylate with a molecular weight equal to or less than butyl methacrylate. A second batch of monomers is then selected from a group of acrylates with a molecular weight greater than butyl acrylate and/or methacrylate with a molecular weight greater than butyl methacrylate. A mixture is then prepared by mixing the first batch of monomers and the second batch of monomers, wherein the second batch of monomers are greater than 50% by weight of the mixture. Finally, the mixture is polymerized to produce an ultra high molecular weight polymer.
Abstract:
The process begins by obtaining a first batch of monomers selected from a group of acrylates with a molecular weight equal to or less than butyl acrylate and/or methacrylate with a molecular weight equal to or less than butyl methacrylate. A second batch of monomers is then selected from a group of acrylates with a molecular weight greater than butyl acrylate and/or methacrylate with a molecular weight greater than butyl methacrylate. A mixture is then prepared by mixing the first batch of monomers and the second batch of monomers, wherein the second batch of monomers are greater than 50% by weight of the mixture. Finally, the mixture is polymerized to produce a drag reducing polymer. The drag reducing polymer is capable of imparting drag reducing properties in liquid hydrocarbons.