DESIGN METHOD OF WELDING METHOD, WELDING METHOD AND WELDED JOINT BODY
    1.
    发明申请
    DESIGN METHOD OF WELDING METHOD, WELDING METHOD AND WELDED JOINT BODY 有权
    焊接方法,焊接方法和焊接接头体的设计方法

    公开(公告)号:US20120094141A1

    公开(公告)日:2012-04-19

    申请号:US13257712

    申请日:2010-03-18

    摘要: A welding method is provided which makes it possible to obtain a joint body having a sufficient strength by selecting a metal glass and a crystalline metal having given conditions. According to the present invention, there is provided a welding method of applying energy to an interface where a metal glass and a crystalline metal make contact with each other or to the metal glass near the interface, of forming a molten layer by heating and melting the metal glass and of performing welding, in which the molten layer after the metal glass and the crystalline metal have been joined together has a glass formation ability, the metal glass has a glass formation ability in which a nose time of a TTT curve when a solid of the metal glass is reheated is 0.2 seconds or more, and the metal glass and the crystalline metal are formed with a material that satisfies a temperature range of a temperature of the metal glass at which a spread factor of the crystalline metal that has not been melted and the molten metal glass is 25% or more and a melting point of the crystalline metal to be 100k or more.

    摘要翻译: 提供一种焊接方法,其可以通过选择具有给定条件的金属玻璃和结晶金属来获得具有足够强度的接头体。 根据本发明,提供了一种焊接方法,其将金属玻璃和结晶金属彼此接触的界面或界面附近的金属玻璃施加能量,通过加热熔融形成熔融层, 金属玻璃和金属玻璃之间的熔融层和结晶金属已经接合在一起的焊接,具有玻璃形成能力,金属玻璃具有玻璃形成能力,其中固体TTT曲线的鼻时间 的金属玻璃的再加热温度为0.2秒以上,并且金属玻璃和结晶金属形成为满足未结晶金属的扩散系数的金属玻璃的温度的温度范围的材料 熔融,熔融金属玻璃为25%以上,结晶性金属的熔点为100k以上。

    Method of welding method, welding method and welded joint body
    2.
    发明授权
    Method of welding method, welding method and welded joint body 有权
    焊接方法,焊接方法和焊接接头体

    公开(公告)号:US08944307B2

    公开(公告)日:2015-02-03

    申请号:US13257712

    申请日:2010-03-18

    IPC分类号: B23K31/02 B23K15/00 B23K26/32

    摘要: A welding method of applying energy to an interface where a metal glass and a crystalline metal make contact with each other or to the metal glass near the interface, heating and melting the metal glass to form a molten layer, and joining the metal glass and the crystalline metal. The metal glass has a glass formation ability in which a nose time of a TTT curve when a solid of the metal glass is reheated is 0.2 seconds or more. The metal glass and the crystalline metal are formed with a material that satisfies a temperature range of a temperature of the metal glass at which a spread factor of the crystalline metal that has not been melted and the molten metal glass is 25% or more and a melting point of the crystalline metal to be 100 K or more.

    摘要翻译: 一种对金属玻璃和结晶金属彼此接触的界面或界面附近的金属玻璃施加能量的焊接方法,加热熔融金属玻璃以形成熔融层,并将金属玻璃和 结晶金属。 金属玻璃具有玻璃形成能力,其中当金属玻璃的固体被再加热时TTT曲线的鼻时间为0.2秒以上。 金属玻璃和结晶金属由满足金属玻璃的温度范围的材料形成,金属玻璃的未融化的结晶性金属的扩散系数和熔融金属玻璃的扩散系数为25%以上, 结晶性金属的熔点为100K以上。

    INJECTION NOZZLE
    3.
    发明申请
    INJECTION NOZZLE 审中-公开
    注射喷嘴

    公开(公告)号:US20130284829A1

    公开(公告)日:2013-10-31

    申请号:US13883594

    申请日:2011-11-02

    IPC分类号: F02M61/16

    摘要: Provided is an injection nozzle which is capable of maintain high response performance over a long period of time, in a manner compatible with an increase in fuel injection pressure of a high-pressure common rail system which is one type of fuel injection system for internal combustion engines such as diesel engines. The injection nozzle comprises a valve body 1, and a needle valve 2 disposed in an inner bore of the valve body 1 and adapted to intermittently seal an injection port 11 of the nozzle body 1, wherein at least a distal end 22 of the needle valve 2 is made of a metallic glass.

    摘要翻译: 本发明提供一种注射喷嘴,能够长时间保持较高的响应性能,能够与作为一种内燃用燃料喷射系统的高压共轨系统的燃料喷射压力的增加相适应 发动机如柴油发动机。 注射喷嘴包括阀体1和设置在阀体1的内孔中并适于间歇地密封喷嘴体1的喷射口11的针阀2,其中针阀的至少远端22 2由金属玻璃制成。