Abstract: A method of preparing a textured glass ceramic is disclosed which comprises the steps of preparing a precursor glass, preparing a precursor glass body, placing the precursor glass body in a furnace in contact with a brick body having a larger or smaller thermal capacity than formed by the precursor glass body, and ceraming the precursor glass body within the furnace in contact with the brick body thereby effecting a temperature gradient across the precursor glass body for precipitating crystallites having a preferred direction of orientation.
Abstract translation: 公开了一种制备织构化玻璃陶瓷的方法,其包括以下步骤:制备前体玻璃,制备前体玻璃体,将前体玻璃体放置在与砖形体接触的炉体中,所述砖体具有比由 前体玻璃体,并且使炉内的前体玻璃体与砖体接触,从而实现跨越前体玻璃体的温度梯度,以沉淀具有优选取向方向的微晶。
-
公开(公告)号:US20070208509A1
公开(公告)日:2007-09-06
申请号:US11705885
申请日:2007-02-13
Applicant: Mark Davis , Katherine Gudgel , Peter Blaum , Paula Vullo
Inventor: Mark Davis , Katherine Gudgel , Peter Blaum , Paula Vullo
IPC: G06F19/00
CPC classification number: C03C10/0072 , B82Y30/00 , C03C10/0009 , C03C23/00 , C03C23/007 , C03C23/009 , C04B35/16 , C04B35/495 , C04B2235/3201 , C04B2235/3251 , C04B2235/3255 , C04B2235/3418 , C04B2235/3427 , C04B2235/781 , C04B2235/80 , C04B2235/9661 , G02F1/3558 , H01G7/026 , H01G7/06 , H01L41/257
Abstract: A method of selecting poling parameters for poling a glass ceramic body comprising ferroelectric domains, by applying an electric field across the glass ceramic body at a certain poling temperature for a certain poling time comprises the steps of: determining an upper bound of poling temperature given by the maximum poling temperature at which uncontrolled heat-up (thermal runaway) is avoided; and selecting the poling temperature to be smaller than the upper bound, preferably close to the upper bound.
Abstract translation: 通过在特定的极化温度下在一定的极化时间内在玻璃陶瓷体上施加电场来选择用于极化玻璃陶瓷体的极化参数的方法,所述方法包括以下步骤:确定极化温度的上限 避免不受控制的加热(热失控)的最高极化温度; 并选择极化温度小于上限,优选接近上限。
-
公开(公告)号:US20070203011A1
公开(公告)日:2007-08-30
申请号:US11699442
申请日:2007-01-29
Applicant: Katherine Gudgel , Peter Blaum , Mark Davis , Paula Vullo
Inventor: Katherine Gudgel , Peter Blaum , Mark Davis , Paula Vullo
CPC classification number: C03B32/02 , C03C10/0009 , C03C10/0054 , H01L41/183
Abstract: A translucent piezoelectric glass ceramic is disclosed. The glass ceramic is prepared from a precursor glass by a ceraming process, using a temperature gradient to effect the precipitation of non-ferroelectric piezo-active crystallites from the precursor glass with a preferred direction of orientation and having an average crystal size of less than 1 micrometer. Alternatively, a translucent piezoelectric glass ceramic comprising ferroelectric crystallites may be prepared by poling. In this case the crystal size is controlled to be smaller than 90 nanometers but preferably larger than 10 nanometers.
Abstract translation: 公开了一种半透明的压电玻璃陶瓷。 玻璃陶瓷由前体玻璃通过蜡化工艺制备,使用温度梯度来实现具有优选的取向方向并且平均晶体尺寸小于1的前体玻璃的非铁电压电活性微晶的沉淀 千分尺 或者,可以通过极化来制备包含铁电晶体的半透明压电玻璃陶瓷。 在这种情况下,晶体尺寸被控制为小于90纳米但优选大于10纳米。
-
-