Method for Manufacturing Grain-Oriented Electrical Steel Sheets Having Excellent Magnetic Properties
    1.
    发明申请
    Method for Manufacturing Grain-Oriented Electrical Steel Sheets Having Excellent Magnetic Properties 有权
    制造具有优异磁性能的面向导电的电工钢板的方法

    公开(公告)号:US20130306202A1

    公开(公告)日:2013-11-21

    申请号:US13979790

    申请日:2011-12-16

    IPC分类号: C21D8/02

    摘要: Provided is a method for manufacturing a grain-oriented electrical steel sheet, the method comprising: heating a grain-oriented electrical steel sheet slab; hot-rolling the heated slab; optionally annealing the hot-rolled steel sheet; subjecting the resulting steel sheet to one cold rolling or two or more cold rollings with intermediate annealing therebetween; subjecting the cold-rolled steel sheet to primary recrystallization annealing; and subjecting the annealed steel sheet to secondary recrystallization annealing, wherein the primary recrystallization annealing sequentially comprises an ultra-rapid heating process of heating the steel sheet at an average heating rate of 300° C./sec or higher, a rapid heating process of heating the steel sheet at a lower average heating rate than the average heating rate of the ultra-rapid heating process, but not lower than 100° C./sec, and a general heating process of heating the steel sheet at a lower average heating rate than the average heating rate of the rapid heating process.

    摘要翻译: 本发明提供一种方向性电磁钢板的制造方法,其特征在于,包括:对取向电工钢板进行加热; 热轧板坯; 任选地退火热轧钢板; 对所得钢板进行一次冷轧或两次以上的冷轧,中间退火; 对冷轧钢板进行一次再结晶退火; 对退火后的钢板进行二次再结晶退火,其中,一次再结晶退火依次包括以300℃/秒以上的平均加热速度对钢板进行加热的超快速加热工序,加热快速加热 该钢板的平均加热速度低于超快速加热工艺的平均加热速率,但不低于100℃/秒,以及以较低的平均加热速率加热钢板的一般加热过程 平均加热速度快速加热。