摘要:
An iodine polarizing film of the invention includes a polymer film and iodine adsorbed and oriented on the polymer film, wherein a iodine content of the polarizing film is within the range of 1.9 to 3% by weight per 2.85 mm3, a single transmittance of the polarizing film is within the range of 43 to 45%, and a ratio (A2/A1) of a crossed absorbance A2 at a wavelength of 610 nm to a crossed absorbance A1 at a wavelength of 480 nm is 1.16 or less.
摘要:
A pressure-sensitive adhesive and retardation layer-attached polarizing plate (4) comprises a retardation layer-attached polarizing plate (3) comprising a polarizing plate (2) that comprises an iodine-based polarizer (1) and a transparent protective film laminated on both sides of the polarizer and a method for manufacturing the pressure-sensitive adhesive and retardation layer attached polarizing plate (4).
摘要:
A pressure-sensitive adhesive and retardation layer-attached polarizing plate (4) of the invention comprises a retardation layer-attached polarizing plate (3) comprising a polarizing plate (2) that comprises an iodine-based polarizer (1) and a transparent protective film laminated on both sides of the polarizer (1); and a retardation layer provided on at least one of the transparent protective films; and an acrylic pressure-sensitive adhesive layer laminated on the retardation layer side of the retardation layer-attached polarizing plate (3), wherein the iodine-based polarizer (1) has a ratio (K/I), which is the content (% by weight) of potassium (K) to the content (% by weight) of iodine (I) in the polarizer, of 0.200 to 0.235, the polarizing plate (2) comprises the iodine-based polarizer (1) and the transparent protective film laminated with an adhesive layer formed from a water-soluble adhesive containing an acetoacetyl group-containing polyvinyl alcohol resin and a crosslinking agent, the retardation layer-attached polarizing plate (3) has a measured dimensional shrinkage of 0.5% or less in the direction of its absorption axis after it is allowed to stand at 80° C. for 24 hours, the pressure-sensitive adhesive and retardation layer-attached polarizing plate (4) has a single-piece transmittance of 41.0% to 43.2%. The pressure-sensitive adhesive and retardation layer-attached polarizing plate can resist a change in optical properties and keep visibility high, even under heated or humidified conditions.
摘要:
A polarizer that can be used for forming a liquid crystal display or an electroluminescent display with less display irregularities and excellent display characteristics is provided. The polarizer contains a dichroic material in a matrix, and its in-plane retardation at a measurement wavelength providing no absorption is in a range of 950 to 1350 nm. The measurement wavelength is preferably a wavelength that the dichroic material provides no absorption, and it is 1000 nm, for example.
摘要:
An end face of a sheet member is cut while rotating a cutting member having a rotation axis extending along a vertical direction of the end face of the sheet member and a cutting blade projecting to a side of the end face of the sheet member around the rotation axis. The cutting member is moved relatively to the sheet member along a longitudinal direction of the end face to be cut. The part separated from a virtual line parallel to the sheet face and passing the rotation center in a cutting region formed by the rotating cutting blade is made to contact the end face of the sheet member.
摘要:
The combination optical film of the invention comprises a plurality of optical films in which at least one end face of the optical films are butted against one another, wherein the butted end faces substantially match one another in shape, the butted end faces each have a portion non-vertical to the front and back surfaces of the optical films, and the end faces are butted against one another so as not to form a continuous gap in the normal direction of the optical films from the front to back surfaces. The combination optical film can prevent light leakage without degrading appearance.
摘要:
An end face of a sheet member is cut while rotating a cutting member having a rotation axis extending along a vertical direction of the end face of the sheet member and a cutting blade projecting to a side of the end face of the sheet member around the rotation axis. The cutting member is moved relatively to the sheet member along a longitudinal direction of the end face to be cut. The part separated from a virtual line parallel to the sheet face and passing the rotation center in a cutting region formed by the rotating cutting blade is made to contact the end face of the sheet member.
摘要:
The present invention provides a method for manufacturing a polarizing film, by which, even when a wide raw film is used, it is possible to obtain a polarizing film that achieves excellent optical characteristics as well as uniformity in in-plane optical characteristics. The method includes the steps of dyeing a polymer film; stretching the dyed film; and drying the film that has undergone the dyeing and stretching steps while conveying the film with rolls. In the drying step, at least two rolls are used as the rolls and the film is dried under a condition that a ratio (R/W) of a distance (R) between the adjacent rolls to an initial width (W) of the polymer film is not less than 0.5 and not more than 4.0.
摘要:
This invention provides a method for manufacturing a combination-type optical film comprising a plurality of optical films each having at least one end face at which the optical films are opposed to one another, comprising the steps of: (1) opposing the end faces of the optical films to one another with a gap provided therebetween; (2) entirely holding the opposed portions of the optical films with a holding member placed on at least one side; (3) connecting an organic solvent- or adhesive-containing vessel to one side of the gap between the opposed portions of the optical films to charge the organic solvent or the adhesive into the gap with the aid of a negative pressure state; and (4) removing the organic solvent or the adhesive under reduced pressure to bond the opposed end faces to one another.
摘要:
A method for producing a polarizing plate of the invention comprises bonding a transparent protective film (A) and another transparent protective film (B) to one side of a polarizer and to another side of the polarizer, respectively, with an adhesive, wherein the polarizer has a moisture content of 15 to 30% by weight, the transparent protective film (A) is made of the same quality material as the transparent protective film (B), the transparent protective film (A) is thicker than the transparent protective film (B), and the transparent protective film (A) has a moisture content higher than that of the transparent protective film (B). The polarizing plate obtained by the production method can suppress curling.