Abstract:
A magnetic head and a manufacturing method of the magnetic head and a magnetic recording and reproducing apparatus used this head, in which the following problem is solved, are provided. A plated film realizing large saturation magnetization Bs about 2T can not realize a high resistivity at the same time, therefore, when this plated film is applied to a magnetic head, the high frequency characteristic is deteriorated. This problem is solved at the present invention. Further, the present invention provides a magnetic head that is low cost and has large saturation magnetization Bs, and has a excellent high frequency characteristic suitable for a high density recording. A magnetic head, in which a coil insulated by insulation layers is disposed between a first magnetic core for recording and a second magnetic core for recording that is disposed to face the first magnetic core for recording via a recording gap, and which executes recording by that a magnetic flux of the first and second magnetic cores for recording excited by the coil is generated from the recording gap, is provided. And at least one of the first and second magnetic cores for recording is composed of a first plated magnetic layer and a second plated magnetic layer in a state that the first plated magnetic layer is disposed at the near side of the recording gap, and saturation magnetization of the first plated magnetic layer is 1.7 T (tesla) or more. And when resistivity of the first plated magnetic layer is defined as &rgr;1 and the thickness of the first plated magnetic layer is defined as &dgr;1, and resistivity of the second plated magnetic layer is defined as &rgr;2, and the thickness of the second plated magnetic layer is defined as &dgr;2, &rgr;1
Abstract:
By inserting a first antistripping layer comprising a first non-magnetic layer 22 and a first conductive layer 23 between a first magnetic layer 16 and a magnetic separation layer 13, adhesion between the first conductive layer 23 and the magnetic separation layer 13 is improved to prevent the first magnetic layer 16 from stripping. In addition, by inserting a second antistripping layer comprising a second non-magnetic layer 24 and a second conductive layer 25 between a second magnetic layer 21 and a magnetic gap layer 17, adhesion between the second conductive layer 24 and the magnetic gap layer 17 is improved to prevent the second magnetic layer 25 from stripping.
Abstract:
A magnetic material includes a main component expressed by a general formula CoNiFeX, wherein X is at least one element selected from the group consisting of Cr, Ti, V, Ru, Rh, Pd, Os, Ir and Pt, and wherein weight percentages a, b, c and d of Co, Ni, Fe and X contents, respectively, in the main component are such that 40%≦a≦10%, 5%≦b≦20%, 10%≦c≦30%, and 0%
Abstract translation:磁性材料包括由通式CoNiFeX表示的主要成分,其中X是选自Cr,Ti,V,Ru,Rh,Pd,Os,Ir和Pt中的至少一种元素,其中重量百分数a 主成分中Co,Ni,Fe,X含量的b,c,d分别为40%<= a <= 10%,5%<= b <= 20%,10%<= c <= 30%,0%
Abstract:
A ferromagnetic film according to the present invention includes ferromagnetic element and nonmagnetic element and has a first portion and a second portion. Concentration of the nonmagnetic element in the first portion is lower than an average concentration of the nonmagnetic element in the ferromagnetic film. On the other hand, concentration of the nonmagnetic element in the second portion is higher than the average concentration of the nonmagnetic element in the ferromagnetic film. The nonmagnetic element includes at least one element selected from the group consisting of Zr, Ti, Nb, Ta, Hf, Mo and W. The ferromagnetic film is applied to a magnetic free layer of a magneto-resistance element in an MRAM.
Abstract:
A magnetic random access memory includes a substrate; a first ferromagnetic layer; a magnetic tunnel junction (MTJ) device provided on a same side of the substrate as the first ferromagnetic layer; and a wiring layer provided between the first ferromagnetic layer and the MTJ device. The MTJ device includes a second ferromagnetic layer opposing to the wiring layer. A first perpendicular projection of the first ferromagnetic layer on the substrate and a second perpendicular projection of the second ferromagnetic layer on the substrate are different in area, and one of the first and second perpendicular projections contains the other.
Abstract:
A recording head is a magnetic head in which ends on one side of opposed first and second magnetic cores form a recording gap, said other ends form a magnetic joint, coils insulated by an insulating material are provided between said first and second magnetic cores, magnetic fluxes of said first and second magnetic cores excited by said coils leak from said recording gap so that recording onto a recording medium is carried out. In said recording head, a distance from said end of said recording gap close to said magnetic medium to a contact point of said magnetic joint (hereinafter, yoke length) is not more than 20 μm. A magnetic recording/reproduction apparatus has this head.
Abstract:
A recording head is a magnetic head in which ends on one side of opposed first and second magnetic cores form a recording gap, said other ends form a magnetic joint, coils insulated by an insulating material are provided between said first and second magnetic cores, magnetic fluxes of said first and second magnetic cores excited by said coils leak from said recording gap so that recording onto a recording medium is carried out. In said recording head, a distance from said end of said recording gap close to said magnetic medium to a contact point of said magnetic joint (hereinafter, yoke length) is not more than 20 &mgr;m. A magnetic recording/reproduction apparatus has this head.
Abstract:
A magnetoresistance element includes a lower electrode layer, a magnetoresistance effect layer, an upper electrode layer and a lower electrode anti-erosion/flaking layer. The lower electrode anti-erosion/flaking layer, which is formed before a photoresist layer remaining on the patterned lower electrode layer is removed, is formed around the lower electrode layer so that its edge facing the lower electrode layer will be in contact with the edge of the lower electrode layer. By use of the lower electrode anti-erosion/flaking layer, the edge of the lower electrode layer is protected from being exposed to a release agent containing a dissolved photoresist in a photoresist layer removal step (when the photoresist layer remaining on the patterned lower electrode layer is removed), thereby the increase of roughness of the edge of the lower electrode layer due to erosion/flaking of the edge in the photoresist removal step can be avoided, and thereby electrical shorts between the upper electrode layer and the lower electrode layer can be eliminated, and thereby a magnetoresistance element of high sensitivity and high performance can be obtained and manufacturing yield of the magnetoresistance elements can be improved.
Abstract:
Disclosed is a magnetic heads suitable for high density recording which comprises an ID head where a CoNiFe film or a CoNiFeX film is formed by a physical vapor deposition method and further a plated film of CoNiFe etc. is formed while avoiding vanishment of a seed layer. The ID head shows high reliability and high production efficiency. The upper magnetic pole of the ID head is composed of a laminated layers of a first magnetic layer 13 of a CoNiFe film or a CoNiFeX film which is formed by a physical vapor deposition method, a second magnetic layer 14 of NiFe layer composing a seed layer laminated thereon, and a third magnetic layer 11 of CoNiFe plated film etc. further laminated on the second layer.
Abstract:
A recording head is a magnetic head in which ends on one side of opposed first and second magnetic cores form a recording gap, said other ends form a magnetic joint, coils insulated by an insulating material are provided between said first and second magnetic cores, magnetic fluxes of said first and second magnetic cores excited by said coils leak from said recording gap so that recording onto a recording medium is carried out. In said recording head, a distance from said end of said recording gap close to said magnetic medium to a contact point of said magnetic joint (hereinafter, yoke length) is not more than 20 μm. A magnetic recording/reproduction apparatus has this head.