1.
公开(公告)号:US08268927B2
公开(公告)日:2012-09-18
申请号:US13166964
申请日:2011-06-23
申请人: Robert Baumann , Juergen Dombrowski , Hartmut Kuehn , Etienne Lazarus , Gerold A Lohmuller , Margarita Perello , Yafei Zhu
发明人: Robert Baumann , Juergen Dombrowski , Hartmut Kuehn , Etienne Lazarus , Gerold A Lohmuller , Margarita Perello , Yafei Zhu
IPC分类号: C08F8/00 , C08F16/06 , C08F116/06 , C08L9/00 , C08L25/02
CPC分类号: C08L25/08 , C04B28/02 , C04B40/0042 , C04B2111/00284 , C08J3/12 , C08J2309/06 , C08J2313/00 , C08J2325/08 , C08L13/00 , C08L25/10 , C08L2205/02 , C08L2666/08 , C08L2666/04 , C04B24/085 , C04B24/2641 , C04B24/2676
摘要: A water redispersible polymer powder is produced by drying an aqueous mixture of a high Tg carboxylated styrene butadiene polymer and a low Tg carboxylated styrene butadiene polymer, where the ratio of the mean or average particle size of the high Tg polymer to the particle size of the low Tg polymer is from 1:1 to 5:1, preferably from 1:1 to 3:1, and the amount of the high Tg polymer is from 20 wt. % to 35 wt. %, preferably from 25 wt. % to 30 wt. %, based upon the total weight of the high Tg polymer and the low Tg polymer. Cement compositions such as mortars, which contain the redispersible polymer powder exhibit unexpectedly superior high bond strength and high impact resistance.
摘要翻译: 通过干燥高Tg羧化苯乙烯丁二烯聚合物和低Tg羧化苯乙烯丁二烯聚合物的水性混合物制备水可再分散聚合物粉末,其中高Tg聚合物的平均或平均粒度与 低Tg聚合物的量为1:1至5:1,优选1:1至3:1,高Tg聚合物的量为20重量%。 %〜35重量% %,优选25wt。 %〜30重量% %,基于高Tg聚合物和低Tg聚合物的总重量。 包含可再分散聚合物粉末的诸如砂浆的水泥组合物显示出出人意料的优异的高粘合强度和高耐冲击性。
-
2.
公开(公告)号:US20120029119A1
公开(公告)日:2012-02-02
申请号:US13166964
申请日:2011-06-23
申请人: Juergen DOMBROWSKI , Hartmut KUEHN , Margarita PERELLO , Gerold A. LOHMULLER , Etienne LAZARUS , Robert BAUMANN , Yafei ZHU
发明人: Juergen DOMBROWSKI , Hartmut KUEHN , Margarita PERELLO , Gerold A. LOHMULLER , Etienne LAZARUS , Robert BAUMANN , Yafei ZHU
CPC分类号: C08L25/08 , C04B28/02 , C04B40/0042 , C04B2111/00284 , C08J3/12 , C08J2309/06 , C08J2313/00 , C08J2325/08 , C08L13/00 , C08L25/10 , C08L2205/02 , C08L2666/08 , C08L2666/04 , C04B24/085 , C04B24/2641 , C04B24/2676
摘要: A water redispersible polymer powder is produced by drying an aqueous mixture of a high Tg carboxylated styrene butadiene polymer and a low Tg carboxylated styrene butadiene polymer, where the ratio of the mean or average particle size of the high Tg polymer to the particle size of the low Tg polymer is from 1:1 to 5:1, preferably from 1:1 to 3:1, and the amount of the high Tg polymer is from 20 wt. % to 35 wt. %, preferably from 25 wt. % to 30 wt. %, based upon the total weight of the high Tg polymer and the low Tg polymer. Cement compositions such as mortars, which contain the redispersible polymer powder exhibit unexpectedly superior high bond strength and high impact resistance.
摘要翻译: 通过干燥高Tg羧化苯乙烯丁二烯聚合物和低Tg羧化苯乙烯丁二烯聚合物的水性混合物制备水可再分散聚合物粉末,其中高Tg聚合物的平均或平均粒度与 低Tg聚合物的量为1:1至5:1,优选1:1至3:1,高Tg聚合物的量为20重量%。 %〜35重量% %,优选25wt。 %〜30重量% %,基于高Tg聚合物和低Tg聚合物的总重量。 包含可再分散聚合物粉末的诸如砂浆的水泥组合物显示出出人意料的优异的高粘合强度和高耐冲击性。
-