公开(公告)号:US20240417275A1
公开(公告)日:2024-12-19
申请号:US18723511
申请日:2022-07-29
Applicant: GEM (WUXI) ENERGY MATERIALS CO., LTD.
Inventor: Kaihua XU , Wei LI , Dechong LIU , Jun XIE , Ningjing LIAO , Yang SHI , Xiaoyan ZHOU , Yujun CHEN , Shiguo XU
Abstract: A method of preparing lithium nickel manganese cobalt oxide high-nickel single-crystal positive electrode material comprises the following steps: mixing and ball milling nickel cobalt manganese hydroxide with a lithium source, zirconium oxide, tungsten oxide, and sodium carbonate, then performing primary sintering, pulverizing, and then obtaining an lithium nickel manganese cobalt oxide high-nickel single-crystal positive electrode material intermediate, the temperature of the primary sintering being 50-150° C. higher than a normal sintering temperature; and evenly mixing the lithium nickel manganese cobalt oxide high-nickel single-crystal positive electrode material intermediate and a coating agent, and then performing secondary sintering to obtain the lithium nickel manganese cobalt oxide high-nickel single-crystal positive electrode material.