公开(公告)号:US20140187680A1
公开(公告)日:2014-07-03
申请号:US14134659
申请日:2013-12-19
申请人: Edward Kripavicius
发明人: Edward Kripavicius
IPC分类号: C04B26/04
CPC分类号: C04B38/00 , C04B26/04 , C04B28/04 , C04B2111/00284 , C04B2111/0075 , Y02W30/92 , C04B14/06 , C04B16/0625 , C04B18/08 , C04B24/18 , C04B24/2623 , C04B16/0633 , C04B2103/0088 , C04B2103/302 , C04B2103/32 , C04B24/06 , C04B24/2647 , C04B14/16 , C04B24/10 , C04B24/2664 , C04B2103/0057
摘要: A fast-curing pervious concrete mix made by combining: water; a cementitious material comprising portland cement and a supplementary cementitious material; aggregate sized to form a pervious concrete; a water reducer; a quantity of fibers; and a polymeric bonding agent, the mix curing to a compressive strength of at least 2,000 psi within 24 hours of placement. Also, a method of forming a pervious concrete structure by forming the fast-curing pervious concrete mix, placing the mix in a desired formation, and curing the placed mix, and a pervious concrete obtained by placing and curing the fast-curing pervious concrete mix.
摘要翻译: 一种快速固化的透水混凝土混合物,结合:水; 包括硅酸盐水泥和补充水泥材料的水泥材料; 骨料尺寸形成透水混凝土; 减水器; 一定数量的纤维; 和聚合物粘合剂,该混合物在放置24小时内固化至至少2000psi的抗压强度。 另外,通过形成快速固化的透水混凝土混合物,将混合物置于所需地层中并固化所配置的混合物,以及通过将快速固化的透水混凝土混合物放置和固化得到的透水混凝土,形成透水混凝土结构的方法 。
-
公开(公告)号:US09328027B2
公开(公告)日:2016-05-03
申请号:US14134659
申请日:2013-12-19
申请人: Edward Kripavicius
发明人: Edward Kripavicius
IPC分类号: C04B38/00 , C04B14/38 , C04B26/04 , C04B28/04 , C04B111/00
CPC分类号: C04B38/00 , C04B26/04 , C04B28/04 , C04B2111/00284 , C04B2111/0075 , Y02W30/92 , C04B14/06 , C04B16/0625 , C04B18/08 , C04B24/18 , C04B24/2623 , C04B16/0633 , C04B2103/0088 , C04B2103/302 , C04B2103/32 , C04B24/06 , C04B24/2647 , C04B14/16 , C04B24/10 , C04B24/2664 , C04B2103/0057
摘要: A fast-curing pervious concrete mix made by combining: water; a cementitious material comprising portland cement and a supplementary cementitious material; aggregate sized to form a pervious concrete; a water reducer; a quantity of fibers; and a polymeric bonding agent, the mix curing to a compressive strength of at least 2,000 psi within 24 hours of placement. Also, a method of forming a pervious concrete structure by forming the fast-curing pervious concrete mix, placing the mix in a desired formation, and curing the placed mix, and a pervious concrete obtained by placing and curing the fast-curing pervious concrete mix.
摘要翻译: 一种快速固化的透水混凝土混合物,结合:水; 包括硅酸盐水泥和补充水泥材料的水泥材料; 骨料尺寸形成透水混凝土; 减水器; 一定数量的纤维; 和聚合物粘合剂,该混合物在放置24小时内固化至至少2000psi的抗压强度。 另外,通过形成快速固化的透水混凝土混合物,将混合物置于所需地层中并固化所配置的混合物,以及通过将快速固化的透水混凝土混合物放置和固化得到的透水混凝土,形成透水混凝土结构的方法 。
-