公开(公告)号:US4232136A
公开(公告)日:1980-11-04
申请号:US15736
申请日:1979-02-27
申请人: Istvan Kovacsay , Maria Szajko nee Lorinczi , Istvan Dubovszky , Laszlo Magdanyi , Ferenc Szailer , Ede Szatmari
发明人: Istvan Kovacsay , Maria Szajko nee Lorinczi , Istvan Dubovszky , Laszlo Magdanyi , Ferenc Szailer , Ede Szatmari
IPC分类号: C08F299/04 , C08F2/44 , C08K5/29 , G01N22/00 , C08F18/00 , C08F118/14
CPC分类号: C08K5/29
摘要: The invention relates to a process for the controlled hardening of unsaturated polyester resins at temperatures of -5.degree. C. to +150.degree. C. using an organic peroxide initiator. According to the process of the invention an organic dyestuff of the general formula (I), ##STR1## wherein R.sup.1 stands for a group of the general formula (II), ##STR2## and in this formula R.sup.5 is a C.sub.1-4 alkyl group and n is an integer from 1 to 3,R.sup.2 and R.sup.3 each represent a C.sub.1-4 alkyl group,R.sup.4 stands for hydrogen, orR.sup.1 and R.sup.4 form together a group of the general formula (III), ##STR3## and in this formula R.sup.6, R.sup.7 and R.sup.8 each represent hydrogen or a C.sub.1-4 alkyl group and Z stands for oxygen or sulfur atom or a -NH- group, andX stands for chlorine or bromine, is admixed with the polyester resin and/or the organic peroxide in an amount of 0.001 to 0.05% by weight, calculated for the weight of the polyester resin.Using the method of the invention the composition and homogeneity of the polyester resin/additive mixtures can be observed easily and the progress of cross-linking can be monitored visually through characteristic colors and color changes, respectively.
摘要翻译: 本发明涉及使用有机过氧化物引发剂在-5℃至+ 150℃的温度下控制硬化不饱和聚酯树脂的方法。 根据本发明的方法,通式(I)的有机染料,其中R1代表通式(Ⅱ)的基团,其中R1和R2分别是 C 1-4烷基,n为1至3的整数,R 2和R 3各自表示C 1-4烷基,R 4表示氢,或R 1和R 4一起形成通式(III)的基团, (III)中,在该式R6中,R7和R8各自表示氢或C1-4烷基,Z表示氧或硫原子或-NH-基团,X表示氯或溴,与 聚酯树脂和/或有机过氧化物,其量为聚酯树脂重量的0.001至0.05重量%。 使用本发明的方法,可以容易地观察到聚酯树脂/添加剂混合物的组成和均匀性,并且可以通过特征颜色和颜色变化来分别监视交联的进展。