公开(公告)号:US20050252579A1
公开(公告)日:2005-11-17
申请号:US11168324
申请日:2005-06-29
申请人: Yasushi Morikage , Takahiro Kubo , Koich Yasuda , Keniti Amano , Kazuo Hiraoka , Akihiko Ohta , Chiaki Shiga
发明人: Yasushi Morikage , Takahiro Kubo , Koich Yasuda , Keniti Amano , Kazuo Hiraoka , Akihiko Ohta , Chiaki Shiga
CPC分类号: C22C38/02 , B23K35/3086 , C22C38/04 , C22C38/44 , Y10T428/12493
摘要: In the present invention, an iron based alloy which contains by mass %: 0.20% or less of C; 6.0 to 16.0% of Cr; 6.0 to 16.0% of Ni and whose martensitic transformation starting temperature (Ms point temperature) is in the range of 0-170° C., inclusive of 0°C and exclusive of 170° C., is used as a welding material. With respect to a weld metal, the weld metal has a iron alloy composition which contains by mass %: 0.20% or less of C; 3.0 to 13.0% of Cr; 3.0 to 13.0% of Ni and whose martensitic transformation starting temperature (Ms point temperature) is in the range of 50-360° C., inclusive of both 50° C. and 360° C.
摘要翻译: 在本发明中,以质量%计含有C:0.20%以下的铁基合金, 6.0〜16.0%的Cr; 6.0〜16.0%的Ni,其马氏体相变开始温度(Ms点温度)在0〜170℃的范围内(包括0℃,不含170℃)用作焊接材料。 对于焊接金属,焊接金属具有质量%:0.20%以下的C的铁合金组成, 3.0〜13.0%的Cr; 3.0〜13.0%的Ni,其马氏体相变开始温度(Ms点温度)在50〜360℃的范围内,包括50℃和360℃。
-
公开(公告)号:US6059177A
公开(公告)日:2000-05-09
申请号:US997667
申请日:1997-12-23
申请人: Osamu Watanabe , Akihiko Ohta , Chiaki Shiga , Satoshi Nishijima
发明人: Osamu Watanabe , Akihiko Ohta , Chiaki Shiga , Satoshi Nishijima
CPC分类号: C21D9/50 , B23K35/3086 , C21D2211/008
摘要: A welding method for two members adapted to be welded and formed of a low-alloy steel for structural purposes causing the weld metal to develop martensite transformation during cooling after welding, so that the weld metal becomes expanded to a greater degree at room temperature than at a temperature at which the martensite transformation initiates. The welding material comprises a ferrous alloy containing C, Cr, Ni, Si, Mn, Mo and Nb, all of which meet substantially with the contents of the following equation (1): ##EQU1##
摘要翻译: 一种焊接方法,用于焊接并由用于结构目的的低合金钢形成的两个构件,其使焊接金属在焊接后的冷却期间发生马氏体相变,使得焊接金属在室温下比在 马氏体转变开始的温度。 该焊接材料包括含有C,Cr,Ni,Si,Mn,Mo和Nb的铁合金,所有这些都基本符合以下等式(1)的含量:
-
公开(公告)号:US07325717B2
公开(公告)日:2008-02-05
申请号:US11168324
申请日:2005-06-29
申请人: Yasushi Morikage , Takahiro Kubo , Koich Yasuda , Keniti Amano , Kazuo Hiraoka , Akihiko Ohta , Chiaki Shiga
发明人: Yasushi Morikage , Takahiro Kubo , Koich Yasuda , Keniti Amano , Kazuo Hiraoka , Akihiko Ohta , Chiaki Shiga
CPC分类号: C22C38/02 , B23K35/3086 , C22C38/04 , C22C38/44 , Y10T428/12493
摘要: In the present invention, an iron based alloy which contains by mass %: 0.20% or less of C; 6.0 to 16.0% of Cr; 6.0 to 16.0% of Ni and whose martensitic transformation starting temperature (Ms point temperature) is in the range of 0-170° C., inclusive of 0° C. and exclusive of 170° C., is used as a welding material. With respect to a weld metal, the weld metal has a iron alloy composition which contains by mass %: 0.20% or less of C; 3.0 to 13.0% of Cr; 3.0 to 13.0% of Ni and whose martensitic transformation starting temperature (Ms point temperature) is in the range of 50-360° C., inclusive of both 50° C. and 360° C.
摘要翻译: 在本发明中,以质量%计含有C:0.20%以下的铁基合金, 6.0〜16.0%的Cr; 6.0〜16.0%的Ni,其马氏体相变开始温度(Ms点温度)在0〜170℃的范围内,包括0℃,不包括170℃作为焊接材料。 对于焊接金属,焊接金属具有质量%:0.20%以下的C的铁合金组成, 3.0〜13.0%的Cr; 3.0〜13.0%的Ni,其马氏体相变开始温度(Ms点温度)在50〜360℃的范围内,包括50℃和360℃。
-
4.
公开(公告)号:US06653594B2
公开(公告)日:2003-11-25
申请号:US09793991
申请日:2001-02-28
IPC分类号: B23K9173
CPC分类号: B23K9/295
摘要: A gas having an arc current-voltage property that is different from a shielding gas is intermittently added to the shielding gas, an arc current is intermittently changed in proportion to an intermittent chemical composition change of the shielding gas at an arc generation region, and an arc generation point situated at a tip of a welding wire is displaced upwardly or downwardly along a groove of a base metal.
摘要翻译: 与保护气体不同的具有电弧电流特性的气体被间歇地添加到保护气体中,电弧电流与电弧产生区域的保护气体的间歇化学组成变化成比例地间歇地变化, 位于焊丝前端的电弧产生点沿着母材的沟槽向上或向下移位。
-
公开(公告)号:US06290905B1
公开(公告)日:2001-09-18
申请号:US09504707
申请日:2000-02-16
申请人: Osamu Watanabe , Akihiko Ohta , Chiaki Shiga , Satoshi Nishijima
发明人: Osamu Watanabe , Akihiko Ohta , Chiaki Shiga , Satoshi Nishijima
IPC分类号: C22C3840
CPC分类号: C21D9/50 , B23K35/3086 , C21D2211/008
摘要: A welding method for two members adapted to be welded and formed of a low-alloy steel for structural purposes causing the weld metal to develop martensite transformation during cooling after welding, so that the weld metal becomes expanded to a greater degree at room temperature than at a temperature at which the martensite transformation initiates. The welding material comprises a ferrous alloy containing C, Cr, Ni, Si, Mn, Mo and Nb, all of which meet substantially with the contents of the following equation (1): 170≦719−(795×C wt %)−(23.7×Cr wt %)−(26.5×Ni wt %)−(35.55×Si wt %)−(13.25×Mn wt %)−(23.7×Mo wt %)−(11.85×Nb wt %)
摘要翻译: 一种焊接方法,用于焊接并由用于结构目的的低合金钢形成的两个构件,其使焊接金属在焊接后的冷却期间发生马氏体相变,使得焊接金属在室温下比在 马氏体转变开始的温度。 该焊接材料包括含有C,Cr,Ni,Si,Mn,Mo和Nb的铁合金,所有这些都基本符合以下等式(1)的含量:
-
公开(公告)号:US5266417A
公开(公告)日:1993-11-30
申请号:US946805
申请日:1992-09-17
申请人: Takahiro Kubo , Yoshifumi Nakano , Chiaki Shiga , Osamu Tanigawa
发明人: Takahiro Kubo , Yoshifumi Nakano , Chiaki Shiga , Osamu Tanigawa
CPC分类号: C21D6/001 , C22C38/08 , Y10T428/12965
摘要: There is provided a low-temperature service nickel steel plate with excellent weld toughness. This steel plate consists essentially of not less than 0.03% of C, 0.02 to 0.22% of Si, 0.05 to 0.47% of Mn, not more than 0.005% of P, not more than 0.005% of S, 7.5 to 12.0% of Ni, 0.01 to 0.10% of Al, and the remaining of Fe, where the following relations stand 3.5%.ltoreq.(8Si+9Mn).ltoreq.5.1% and 123C+(8Si+9Mn).ltoreq.10.9%.
摘要翻译: 提供了具有优异焊接韧性的低温维修镍钢板。 该钢板基本上由C:0.03%以上,Si:0.02〜0.22%,Mn:0.05〜0.47%,P:0.005以下,S:0.005%以下,Ni:7.5〜12.0% ,0.01〜0.10%的Al,余下的Fe,其中以下关系为3.5%(8Si + 9Mn)= 5.1%和123C +(8Si + 9Mn)= 10.9%。
-
-
-
-
-