摘要:
A method of producing a Group II-VI compound semiconductor. The method involves generating a pulsed electrical discharge plasma between metallic electrodes in sulfur to produce a Group II-VI compound semiconductor. A method of producing a Group II-VI compound semiconductor phosphor using a pulsed electrical discharge plasma. A hexagonal crystal of Group II-VI compound semiconductor composed of a plurality of twin crystals.
摘要:
CdSiP2 crystals with sizes and optical quality suitable for use as nonlinear optical devices are disclosed, as well as NLO devices based thereupon. A method of growing the crystals by directional solidification from a stoichiometric melt is also disclosed. The disclosed NLO crystals have a higher nonlinear coefficient than prior art crystals that can be pumped by solid state lasers, and are particularly useful for frequency shifting 1.06 μm, 1.55 μm, and 2 μm lasers to wavelengths between 2 μm and 10 μm. Due to the high thermal conductivity and low losses of the claimed CdSiP2 crystals, average output power can exceed 10 W without severe thermal lensing. A 6.45 μm laser source for use as a medical laser scalpel is also disclosed, in which a CdSiP2 crystal is configured for non-critical phase matching, pumped by a 1064 nm Nd:YAG laser, and temperature-tuned to produce output at 6.45 μm.
摘要:
A phosphor represented by Formula 1: (A1−(a+b)EuaLnb)1−x(B1−cMnc)2Al(6+b−2x)Si(9−b+2x)O30 Formula 1 wherein A includes at least one element selected from the group consisting of Ca, Sr and Ba, Ln includes at least one metal selected from the group consisting of a trivalent rare earth metal, B includes at least one element selected from the group consisting of Mg, Zn, Ge and Co, a is greater than 0 and equal to or less than about 0.5, b is greater than 0 and equal to or less than about 0.25, c is greater than 0 and less than about 0.8, and x is 0 to about 0.2. Also a white light emitting device including the phosphor.
摘要:
A low-pressure discharge lamp includes, in an exemplary embodiment, a light-transmissive envelope, a fill-gas composition capable of sustaining a discharge sealed inside the light-transmissive envelope, and a phosphor composition at least partially disposed on an interior surface of said light-transmissive envelope forming at least one phosphor layer. The phosphor composition includes at least one phosphor, and at least one amalgam-forming material.
摘要:
According to the present invention, a fluorescent powder composed mainly of an acicular or fibrous zinc oxide single crystal with an aspect ratio of 5 or higher is produced by the following steps: a step of producing a raw material solution selected from the group consisting of a raw material solution (A) that is an alkali solution containing zing ions, a raw material solution (B) that is a solution containing zinc ions and ions of dopant element, and a mixed solution of the raw material solution (A) and the raw material solution (B); and a hydrothermal reaction step wherein a hydrothermal reaction of the mixed solution is carried out in a hermetically sealed vessel at a subcritical or supercritical temperature and at a subcritical or supercritical pressure. A zinc oxide single crystal powder can be produced at low cost without the need for a pulverization step or a similar step and high-density orientation can be realized by such crystal powder. Such crystal powder is most suitable for light emitting devices, display devices, fluorescent lamps, and the like.
摘要:
The present invention provides a phosphor having high luminance, a property of low luminance degradation during driving of a light-emitting device, and chromaticity y comparable to that of BAM:Eu. The present invention is a phosphor represented by the general formula aAO.bEuO.DO.cSiO2, where A is at least one selected from Ca, Sr and Ba, D is at least one selected from Mg and Zn, and 2.970≦a≦3.500, 0.001≦b≦0.030, and 1.900≦c≦2.100 are satisfied. In this phosphor, a peak intensity at 1490 cm−1 is 0.02 to 0.8 when a peak intensity at 565 cm−1 is set to 1 in a spectrum obtained by measurement using photoacoustic spectroscopy.
摘要:
A phosphor material is presented that includes a blend of a first phosphor, a second phosphor and a third phosphor. The first phosphor includes a composition having a general formula of ((Sr1−zMz)1−(x+w)AwCex)3(Al1−ySiy)O4+y+3(x−w)F1−y−3(x−w), wherein 0
摘要翻译:提供了包括第一荧光体,第二荧光体和第三荧光体的共混物的荧光体材料。 第一种荧光体包括具有通式((Sr1-zMz)1-(x + w)AwCex)3(Al1-ySiy)O4 + y + 3(x-w)F1-y-3(x- w),其中0
摘要:
A plasma display device having a panel main body in which a pair of transparent substrates is arranged in opposition so as to form a discharge space between the substrates on at least a front side, barrier ribs are arranged on at least one of the substrates to divide the discharge space into a plurality of spaces, a group of electrodes is arranged on the substrates so as to generate discharge in the discharge space divided with the barrier ribs, and phosphor layers that emit by discharge are provided, in which the phosphor layers are equipped with a green phosphor layer including at least Zn2SiO4:Mn, a surface of Zn2SiO4:Mn is coated with magnesium oxide, and a ratio of an Mg element to a Si element on the surface measured with an XPS apparatus is 0.7 to 4.0.
摘要:
A population of nanoparticles is disclosed. The population is comprised of a plurality of core/shell nanocrystals, each including: a semiconductor core, an intermediate semiconductor shell layer disposed over the semiconductor core, an external semiconductor shell layer disposed over the intermediate semiconductor shell layer, and a hydrophilic organic layer in direct contact with the external semi-conductor shell layer. The population of nanoparticles has a αon value of less than about 1.4.